Finished opacity is physically separate from both thickness (caliper) and basis weight (gsm). A thicker or heavier uncoated or art sheet still transmits light through its paper fibers and mineral fillers, whereas a thinner two-ply card stock bonded with a pigmented internal core blocks light transmission at the adhesive barrier. For more production terms, see the manufacturing glossary.

Specifications and Stock Comparison

Card Deck Press produces custom cards with specialist offset and tabletop manufacturing partners, with standard offset card runs starting at 200 decks (usual tiers of 200, 300, 500, and 1,000+ decks). Selecting the right stock depends on balancing light-blocking performance against card stiffness and total deck stack height.

Stock / Construction Basis Weight Approximate Caliper (mm / in) Internal Light Barrier Opacity Behavior
Art / blue core 300 gsm 0.28–0.31 mm (0.0110–0.0122 in) Blue-pigmented adhesive core Blocks normal face-to-back show-through
Black-core linen 310 gsm 0.30–0.32 mm (0.0118–0.0126 in) Carbon-black adhesive core High concealment; linen embossing scatters surface glare
Black core 330 gsm 0.32–0.34 mm (0.0126–0.0134 in) Carbon-black adhesive core Highest paper-card concealment for dark or high-contrast faces
Art stock (no barrier core) 350 gsm 0.34–0.38 mm (0.0134–0.0150 in) None (solid paper ply) Thicker than 300–330 gsm core stocks, but transmits more light
Art stock (no barrier core) 400 gsm 0.40–0.44 mm (0.0157–0.0173 in) None (solid paper ply) Rigid board feel; still relies on fiber bulk rather than an opaque core
PVC — 0.30 mm (0.0118 in) Solid pigmented polymer Naturally opaque when pigmented; resists moisture

Double-sided film lamination adds 0.03–0.05 mm (0.0012–0.0020 in) per card to the finished caliper. For example, a 330 gsm black-core card with double-sided film reaches approximately 0.35–0.39 mm (0.0138–0.0154 in) per card, which directly affects box stack clearance (typically 1.5–3 mm / 0.059–0.118 in).

Basis Weight vs. Caliper vs. Opacity

  • Basis weight (gsm or US LB): Measures mass per unit area, not light blockage. In US paper specifications, US Text LB (based on a 25 × 38 in / 635 × 965 mm basis sheet) and US Cover LB (based on a 20 × 26 in / 508 × 660 mm basis sheet) represent different sheet densities at the same nominal pound number; always anchor specifications in gsm alongside caliper.
  • Booklet and insert stocks: Interior booklet sheets at 80–120 gsm (about 0.08–0.13 mm / 0.0031–0.0051 in per sheet) have lower opacity than card stocks, so heavy ink coverage on one side of a leaflet or manual page can ghost through to the reverse. Covers at 200–300 gsm reduce show-through from the outer wrap.
  • Ink density and surface finish: High-contrast face graphics—especially rich black areas (C40–60 M30–40 Y30–40 K100, with total area coverage kept at TAC ≤280%–300%)—create sharper silhouettes if light passes through the sheet. Anti-scuff matte lamination suits dark artwork by reducing surface reflection without changing core opacity.

Production Steps

  1. Lock the core specification before layout: Confirm whether the deck requires blue core (300 gsm) or black core (310–330 gsm) based on face-to-back contrast and whether cards must remain concealed when held near a light source.
  2. Prepare print files for offset: Supply artwork in CMYK with separate spot layers at ≥300 DPI in AI, PDF, or PSD (PDF/X-1a or PDF/X-4), with outlined or embedded fonts, 100% K for fine text, and TAC ≤280%–300%. Include 3 mm (0.118 in) bleed per side, ≥3 mm (0.118 in) safety margin (≥4–5 mm / 0.157–0.197 in for bordered backs), and R3–R3.5 mm (0.118–0.138 in) corners.
  3. Laminate, cure, and die-cut: Apply double-sided protective film (+0.03–0.05 mm / 0.0012–0.0020 in per card) or varnish over the printed sheets, then die-cut and round corners after ink and adhesive cure.
  4. Calculate finished stack height: Multiply the finished per-card caliper (base stock + film) by deck count and add box stack clearance of 1.5–3 mm (0.059–0.118 in) before finalizing packaging dimensions.

Sign-Off Criteria

  • Backlight inspection: Hold a finished card between the eye and an overhead or window light source; on blue-core and black-core stocks, high-contrast face elements (dark borders, rich black panels, or bold icons) must not be identifiable from the back.
  • Caliper verification: Measure finished card thickness with a micrometer to confirm the sheet plus double-sided film falls within the expected tolerance (for example, 0.32–0.34 mm / 0.0126–0.0134 in base plus 0.03–0.05 mm / 0.0012–0.0020 in film for 330 gsm black core).
  • Color and edge check: Confirm dark ink areas show even coverage without scuffing and that cut edges expose a clean, uniform core line without delamination.

Concrete Failure Modes

  • Selecting high-gsm art stock for concealed cards: Choosing 350 gsm (0.34–0.38 mm / 0.0134–0.0150 in) or 400 gsm (0.40–0.44 mm / 0.0157–0.0173 in) art stock instead of a blue- or black-core stock increases stiffness and thickness but still allows high-contrast face shapes to show through under bright light.
  • Equating basis weight with opacity: Specifying a heavier gsm or higher US Cover/Text LB sheet without checking core construction results in unnecessary deck bulk without solving light transmission.
  • High-contrast face artwork on thin or unpigmented sheets: Large rich-black blocks or dark artwork on the card face paired with light-colored backs amplify ghosting when a barrier core is omitted.
  • Omitting film thickness from box sizing: Adding double-sided film (+0.03–0.05 mm / 0.0012–0.0020 in per card) to achieve durability or matte scuff protection without updating stack height calculations can exceed the 1.5–3 mm (0.059–0.118 in) box clearance and cause tight or bowed tuck boxes.