When a boxed deck or tabletop game combines high-caliper card stock, double-sided film lamination, a bound booklet, and wrapped rigid greyboard, target the upper end of standard box clearance—1.5–2.5 mm (0.059–0.098 in) across width and height, and 1.5–3 mm (0.059–0.118 in) for stack height—rather than a tight nominal fit. For related manufacturing definitions, see the Manufacturing Glossary.
How Tolerances Accumulate Along One Axis
Along any single assembly axis—width (X), height (Y), or stack depth (Z)—individual part variations add together directly against the enclosing cavity:
Total Stack Tolerance = Sum of Individual Part Tolerances
Minimum Clearance = Minimum Cavity Dimension - Maximum Total Component Stack
Recording nominal dimension (the target measurement) separately from allowable variation (the plus/minus band) prevents two common specification errors:
- Averaging out repeating layers: A single card's caliper spread looks negligible, but multiplying that spread across 50 to 100+ cards creates several millimetres of stack height uncertainty.
- Double-counting or hiding wall thickness: Listing only an outer box size without separating greyboard thickness, wrap build-up, and inner cavity tolerance obscures how much room remains for the contents.
For example, 300 gsm art or blue-core card stock measures 0.28–0.31 mm (0.0110–0.0122 in) per card. Across a 100-card deck, that 0.03 mm (0.0012 in) per-card range produces a 3.0 mm (0.118 in) height difference between the thinnest and thickest possible stacks. Adding double-sided film (0.03–0.05 mm / 0.0012–0.0020 in per card) adds another 3.0–5.0 mm (0.118–0.197 in) to the deck height.
Contact Surfaces and Specifications
Only contact surfaces that constrain movement or close a lid contribute to stack-up along that axis:
- X/Y Cavity Walls: Card trim edges or insert outer walls pressing against the inner box walls (
1.5–2.5 mm/0.059–0.098 intotal clearance). - Z-Axis Stack Interfaces: Card faces, film lamination, booklet sheets, folded game boards, and punchboards stacked between the box floor and the underside of the lid (
1.5–3 mm/0.059–0.118 intotal clearance). - Rigid Box Lid-to-Base Walls: Greyboard walls (
1.5,2,2.5, or3 mm/0.059,0.079,0.098, or0.118 in) plus wrap paper and15–20 mm(0.591–0.787 in) turn-in wrap margins folded over the top rim and corners.
| Component / Interface | Metric Spec | Imperial Equivalent | Stack-Up Impact |
|---|---|---|---|
| Box clearance (width / height) | 1.5–2.5 mm |
0.059–0.098 in |
Absorbs trim, insert, and wrap variation |
| Box clearance (stack height) | 1.5–3 mm |
0.059–0.118 in |
Absorbs cumulative Z-axis caliper spread |
300 gsm art / blue-core card |
0.28–0.31 mm |
0.0110–0.0122 in |
Compounds by total card count |
310 gsm black-core linen card |
0.30–0.32 mm |
0.0118–0.0126 in |
Compounds by total card count |
330 gsm black-core card |
0.32–0.34 mm |
0.0126–0.0134 in |
Compounds by total card count |
350 gsm art stock card |
0.34–0.38 mm |
0.0134–0.0150 in |
Compounds by total card count |
400 gsm card stock |
0.40–0.44 mm |
0.0157–0.0173 in |
High Z-axis sensitivity per deck |
| PVC card stock | 0.30 mm |
0.0118 in |
Rigid, non-compressible stack height |
| Double-sided film lamination | +0.03–0.05 mm / card |
+0.0012–0.0020 in / card |
Multiplies across every laminated card |
Booklet interior (80–120 gsm) |
0.08–0.13 mm / sheet |
0.0031–0.0051 in / sheet |
Scales by signature count (multiples of 4) |
| Greyboard wall thickness | 1.5 / 2 / 2.5 / 3 mm |
0.059 / 0.079 / 0.098 / 0.118 in |
Subtracts 2x wall thickness from outer X/Y |
| Rigid box wrap margin | 15–20 mm |
0.591–0.787 in |
Adds wrap layer build-up at rims and corners |
| Punchboard die gap | 3–4 mm |
0.118–0.157 in |
Defines minimum spacing between die-cut parts |
When specifying booklet or box-wrap papers in US weights alongside gsm, distinguish US Text LB (basis sheet size 25 × 38 in / 635 × 965 mm) for 80–120 gsm interior pages from US Cover LB (basis sheet size 20 × 26 in / 508 × 660 mm) for 200–300 gsm covers.
Production Steps and Sign-Off Criteria
- Separate nominal and tolerance per part: Record the target dimension and allowable variation independently for every component on the bill of materials, including core stock, double-sided film, booklet signatures (saddle stitch
12–40pages, perfect binding28+, or sewn binding80–100+), and greyboard caliper. - Calculate worst-case axis sums: Multiply maximum single-sheet calipers by component counts along the Z-axis, and add maximum X/Y trim and insert tolerances.
- Derive inner cavity dimensions first: Set the inner box or tray cavity to accommodate the worst-case stack plus
1.5–2.5 mm(0.059–0.098 in) in width/height and1.5–3 mm(0.059–0.118 in) in depth, then add two greyboard walls and wrap allowance to establish outer box dimensions. - Verify on a physical white sample: Assemble a dummy sample using the actual production card stock, lamination, booklet, and wrapped greyboard before cutting final box or insert tooling.
Sign-Off Criteria
- The lid seats flush against the base shoulder without bowing, lifting, or requiring forced compression.
- Decks and booklets slide into and out of their cavities without catching on
15–20 mm(0.591–0.787 in) turn-in wrap seams. - Components sit below the base rim with
1.5–3 mm(0.059–0.118 in) Z-axis clearance remaining when using maximum-caliper stock.
Failure Modes
- Lid lift or bowed box sides: Calculating Z-axis depth from nominal card caliper (
0.34 mminstead of0.38 mmon350 gsmstock, or omitting+0.05 mmper card for double-sided film) consumes the1.5–3 mm(0.059–0.118 in) clearance and forces the lid upward. - Tight or binding tray fit: Defining outer rigid box dimensions without subtracting two
2.5–3 mm(0.098–0.118 in) greyboard walls and corner wrap turn-ins shrinks the inner cavity below the1.5–2.5 mm(0.059–0.098 in) X/Y allowance, causing edge friction and scuffed cards. - Component rattle and edge wear: Adding arbitrary clearance beyond the worst-case sum leaves excess void space, allowing decks, punchboards, or booklets to shift and abrade during shipping.
Parent guide Printing and Tabletop Manufacturing Glossary