For standard air-freight shipments in climate-controlled cargo holds, individual deck wraps inside snug, double-walled master cartons with zero-slop dividers are typically sufficient without heavy desiccant loading. For ocean freight (FCL or LCL), humid port storage, or any deck with metallic gilded edges, sealed moisture-barrier poly liners and calibrated desiccants become mandatory alongside tight void control. For broader palletization, corner-board, and container-level crush rules, see the parent Export Moisture and Crush Protection guide.
Material and Packing Specifications
Card decks pack far more mass per cubic unit than hollow board-game boxes, which amplifies both vibration energy and stack compression during transit. Paper-core stocks absorb ambient moisture unevenly through their cut or gilded edges, while PVC remains dimensionally stable against humidity but still suffers from surface scuffing and heat deformation.
When specifying card stock weights, Card Deck Press uses grams per square meter (gsm), which corresponds to US Cover LB (based on a 20 x 26 in / 508 x 660 mm basis sheet) rather than US Text LB (based on a 25 x 38 in / 635 x 965 mm basis sheet).
| Deck Construction | Typical Stock & Caliper | Key Transit Vulnerability | Required Export Packing Spec |
|---|---|---|---|
| Standard paper-core deck | 300 gsm art/blue core: 0.28–0.31 mm (0.011–0.012 in); 310 gsm black-core linen: 0.30–0.32 mm (0.012–0.013 in); 330 gsm black core: 0.32–0.34 mm (0.013 in) | Edge moisture swell and face-to-edge warp; scuffing on dark anti-scuff matte surfaces | Sealed unit wrap + zero-slop dividers + sealed carton poly liner + desiccant for ocean transit |
| Heavyweight paper deck | 350 gsm art stock: 0.34–0.38 mm (0.013–0.015 in); 400 gsm: 0.40–0.44 mm (0.016–0.017 in) | High carton density causing bottom-seam blowouts and edge crushing | Strict 15–20 kg (33–44 lb) carton weight cap + reinforced dividers + sealed poly liner + desiccant |
| Gilded or foil-edged deck | Paper cores above (thick lamination can conflict with gilded edges); double-sided film adds 0.03–0.05 mm (0.001–0.002 in) per card | Foil blocking from heat/humidity/pressure; foil flaking from micro-vibration | Post-gilding cure before wrap + soft edge isolation + zero-slop dividers + sealed poly liner + desiccant |
| Plastic deck | PVC: 0.30 mm (0.012 in) | Surface abrasion from dust/grit and heat-induced warping under heavy top loads | Tight unit wrap + zero-slop dividers + carton weight cap; desiccants optional for carton dryness |
Boxed decks also operate within tight internal tolerances. Standard tuck boxes and rigid boxes built with 1.5–3 mm (0.059–0.118 in) greyboard use 1.5–2.5 mm (0.059–0.098 in) clearance across width and height and 1.5–3 mm (0.059–0.118 in) for stack height. External packing must keep outer carton walls from bowing inward onto those clearances.
Export Packing Steps
- Cure and acclimate before wrapping. Allow printed, coated, and gilded decks to cool and reach moisture equilibrium in a conditioned staging area before applying shrink-wrap or cello-wrap. Sealing warm or freshly gilded decks traps residual heat and moisture inside the unit wrap.
- Isolate gilded edges at the unit level. Wrap individual decks cleanly without prolonged heat-gun dwell near foil edges. For unboxed gilded decks or multi-deck sets inside rigid boxes, use smooth paper sleeves or non-abrasive interleaving so metallic edges do not rub directly against rough board or adjacent cards.
- Load into zero-slop inner dividers. Pack wrapped decks into corrugated or heavy chipboard cells sized to eliminate lateral and vertical play. Fill any remaining headspace with flat corrugated pads rather than loose void fill, which settles under ocean vibration.
- Cap master carton gross weight. Keep each master carton at or below 15–20 kg (33–44 lb), especially for 350–400 gsm (0.34–0.44 mm / 0.013–0.017 in) decks. High-density card stacks placed in oversized cartons crush bottom-layer corners and split tape seams during manual transshipment.
- Seal inside a poly liner with desiccants. Line the master carton with a moisture-barrier poly bag before loading the inner dividers. Place desiccant sachets in the upper corner pockets outside the unit wraps—never in direct contact with bare cards or gilded edges—and heat-seal or tightly twist-and-tape the liner neck before sealing the outer flaps.
- Verify destination packaging and compliance records. Keep transit master-carton markings distinct from consumer-facing packaging disclosures. Where consumer packaging enters regulated markets, maintain applicable records such as Germany's VerpackG registration and data reporting or France's Triman info-tri sorting marks, and retain EN 71 assessment and testing documentation if the product falls within toy-safety scope.
Sign-Off Criteria
Before releasing a shipment for export pickup, verify the following conditions on sampled master cartons:
- Liner seal integrity: The poly liner is fully closed with no tears from corrugated staple points or sharp divider corners.
- Desiccant isolation: Desiccant sachets sit outside sealed unit wraps and cannot press directly into 1.5–3 mm (0.059–0.118 in) greyboard lids or exposed card edges.
- Zero-slop shake check: Closed master cartons produce no internal rattle or deck shift when tilted or lightly shaken.
- Carton weight ceiling: Verified scale weight of packed master cartons stays within 15–20 kg (33–44 lb) (gross weight = deck weight + dividers + outer carton).
- Gilded edge inspection: Sampled gilded decks show clean separation between cards, no foil transfer onto inner box walls, and no edge chipping.
Concrete Failure Modes
- Foil blocking and card fusion: High ambient humidity combined with container heat and heavy vertical stacking pressure softens foil adhesives on gilded edges, fusing adjacent cards together or bonding edges to box interiors.
- Edge rub and finish scuffing: Even 3–5 mm (0.118–0.197 in) of unpadded void inside a master carton lets dense card stacks vibrate continuously against dividers during sea transit, wearing metallic foil off edges and burnishing dark anti-scuff matte faces.
- Edge swell and box-lid binding: When moisture penetrates an unlined carton, exposed paper-core edges absorb humidity faster than film-laminated faces (which add 0.03–0.05 mm / 0.001–0.002 in per card). The deck curls and expands beyond the 1.5–3 mm (0.059–0.118 in) stack-height clearance, jamming inside tuck or rigid boxes.
- Carton seam blowout: Packing too many dense decks into a single carton above 20 kg (44 lb) concentrates shear force on bottom-flap tape and corners, bursting cartons when pallets are broken down at destination warehouses.
- Desiccant indentation and staining: Placing loose desiccant packets directly against soft greyboard boxes or unwrapped cards creates permanent dent marks under stack weight and risks localized staining if condensation forms on the sachet surface.
Parent guide Moisture and Crush Protection for Export Packing