The exact packing build shifts based on four job conditions:
- Board construction: Asymmetric dual-layer recessed boards warp faster than balanced folding boards because the die-cut top layer and solid base layer expand at different rates.
- Film lamination: Single-sided film pulls a board toward the unlaminated back during humidity swings, whereas balanced double-sided film (
0.03–0.05 mm/0.0012–0.0020 intotal added caliper) slows moisture exchange. - Transit route: Ocean freight and unconditioned warehouses expose cartons to multi-week humidity cycles that require sealed barrier bags and desiccants, while short regional ground transit relies primarily on flat orientation and edge bracing.
- Pack format: Boards packed inside finished game boxes depend on tight tray clearance, while bulk component shipments require rigid master-carton corner boards and flat palletization.
Material and Packing Specifications
Specify board thickness, wrap tolerances, and box clearances in millimetres and inches together, and specify paper wraps in gsm (noting that US Text LB uses a 25 × 38 in basis sheet while US Cover LB uses a 20 × 26 in basis sheet).
| Component Type | Core & Wrap Specs | Clearance & Stack Allowance | Primary Packing Controls |
|---|---|---|---|
| Folding Game Boards | 1.5 / 2 / 2.5 / 3 mm (0.059 / 0.079 / 0.098 / 0.118 in) greyboard; 15–20 mm (0.59–0.79 in) wrap margin |
1.5–2.5 mm (0.059–0.098 in) width/height box clearance; 1.5–3 mm (0.059–0.118 in) stack clearance |
Flat orientation, balanced lining or double-sided film, moisture-barrier outer wrap, corner bracing |
| Multi-Panel GM Screens | 2–3 mm (0.079–0.118 in) greyboard; 15–20 mm (0.59–0.79 in) wrap margin across hinge panels |
1.5–2.5 mm (0.059–0.098 in) lateral clearance; 1.5–3 mm (0.059–0.118 in) folded stack clearance |
Folded flat under even compression, desiccant inside sealed polybag, rigid top/bottom buffer pads |
| Dual-Layer Recessed Boards | Two bonded 1.5–2.5 mm (0.059–0.098 in) greyboard plies; 15–20 mm (0.59–0.79 in) outer wrap margin |
1.5–2.5 mm (0.059–0.098 in) tray clearance; 1.5–3 mm (0.059–0.118 in) stack height allowance |
Extended flat curing under weight, individual or small-stack barrier sealing, desiccant, full-perimeter edge guards |
Use the following plain-text formula to verify inner box or master-carton height before locking dielines:
Stack height allowance = (Board caliper * stack count) + (0.03 to 0.05 mm per double-sided film wrap) + 1.5 to 3 mm stack clearance
In inches (25.4 mm/in):
Stack height allowance (in) = (Board caliper in inches * stack count) + (0.0012 to 0.0020 in per double-sided film wrap) + 0.059 to 0.118 in stack clearance
Job-Specific Packing and Freight Steps
- Equilibrate and cure flat after lamination: Keep freshly wrapped folding boards, GM screens, and glued dual-layer boards stacked flat under even top weight until adhesive moisture dissipates. Sealing warm or uncured greyboard traps water vapor inside the wrap.
- Enforce flat horizontal orientation: Pack all boards horizontally in inner boxes and master cartons—never standing on edge. Keep lateral box or insert clearance within
1.5–2.5 mm(0.059–0.098 in) and vertical stack clearance within1.5–3 mm(0.059–0.118 in); fill any remaining headspace with rigid corrugated pads so boards cannot slide and hammer their corners. - Seal inside moisture-barrier wraps with desiccant: Enclose individual boards, game boxes, or inner master bundles in heat-sealed or tightly taped moisture-barrier film. Place desiccant packets inside the sealed barrier (not loose in the outer corrugated carton) and separate packets from direct contact with uncoated paper surfaces.
- Apply rigid edge bracing and palletize flush: Line master-carton walls with corrugated edge protectors or full-height corner boards, and place rigid top and bottom cap sheets inside the carton to distribute strapping pressure. Stack cartons flat on pallets with zero overhang so outer edges carry vertical load without crushing board corners.
- Document destination packaging compliance where applicable: When shipping poly-wrapped or barrier-sealed cartons into regulated markets, maintain the required packaging material records and sorting marks—such as VerpackG registration and reporting for Germany and Triman sorting guidance for France—according to the importer's channel obligations.
Sign-Off Criteria
Verify these physical checks during pre-shipment AQL inspection before releasing freight:
- Flatness on a reference surface: Unwrapped sample boards from the top, middle, and bottom of curing stacks lie flat on a level table with no edge lift or twist.
- Hinge and wrap integrity: Folding boards and GM screens open and close cleanly along score lines without cracking the printed wrap or pulling at the
15–20 mm(0.59–0.79 in) turn-in margins. - Dual-layer bond stability: Recessed top layers sit flush against the base greyboard around every cutout window with no corner peeling or asymmetric bow.
- Barrier seal and carton bracing: Moisture-barrier bags show intact seals with desiccant present, lateral and vertical clearances hold boards immobile, and master-carton corner braces show no compression creasing after strapping.
Failure Modes and Root Causes
| Failure Mode | Physical Cause | Corrective Action |
|---|---|---|
| Cupping or potato-chip warp | Unbalanced moisture absorption between front and back plies, especially on single-side laminated dual-layer boards | Balance front and back liners, cure flat under weight, and seal inside a moisture-barrier wrap with desiccant |
| Corner crushing and mushrooming | Vertical edge-loading in transit, pallet overhang, or excess box clearance (> 2.5 mm / 0.098 in) allowing impact |
Enforce flat horizontal packing, tighten clearance to 1.5–2.5 mm (0.059–0.098 in), and add rigid corner boards |
| Condensation spotting or mold | Sealing boards in barrier film before adhesive moisture evaporates, or omitting desiccant on ocean routes | Extend flat post-lamination curing before bagging and size desiccants to the sealed barrier volume |
| Hinge split or edge delamination | Rapid dry-out shrinkage across 15–20 mm (0.59–0.79 in) turn-ins or flexing cold, overly dry paper wraps |
Maintain balanced wrap-margin adhesion, equilibrate boards flat before folding, and protect stacks from sudden humidity drops |
Parent guide Moisture and Crush Protection for Export Packing