Baseline vs. Specialized Routing
The deck's substrate, edge finish, and die profile determine which checkpoints are added to the standard lot-sampling plan.
| Job Attribute | Baseline Lot Checks | Additional Specialized Checkpoints | Primary Physical Risk |
|---|---|---|---|
| Standard paperboard (300–400 gsm) | Count, collation, border symmetry, edge trim, scuff | Core opacity check; caliper stack height vs. box clearance | Edge nicking, border drift, dark-ink scuffing |
| Gilded or foil-edged decks | Count, collation, border symmetry, edge trim, scuff | Edge-foil adhesion, lamination-edge compatibility, card-to-card blocking | Foil flaking or delamination against thick film |
| PVC decks (0.30 mm / 0.012 in) | Count, collation, border symmetry, edge trim, scuff | Static separation, ink/coating scratch adhesion, thermal curl | Static double-feeds, ink lift, die-cut burrs |
| Shaped or non-standard profiles | Count, collation, border symmetry, edge trim, scuff | Multi-axis die registration, asymmetrical safety margin, tray/box clearance | Clipped art on tight radii, jammed tuck-box insertion |
Specifications and Inspection Tolerances
Lot inspectors verify finished decks against the approved prepress and manufacturing tolerances:
- Substrate Caliper and Stack Height: Verify single-card caliper against the specified stock:
- 300 gsm art or blue-core stock: 0.28–0.31 mm (0.011–0.012 in)
- 310 gsm black-core linen stock: 0.30–0.32 mm (0.012–0.013 in)
- 330 gsm black-core stock: 0.32–0.34 mm (0.013–0.013 in)
- 350 gsm art stock: 0.34–0.38 mm (0.013–0.015 in)
- 400 gsm stock: 0.40–0.44 mm (0.016–0.017 in)
- PVC stock: 0.30 mm (0.012 in)
- Double-sided film lamination: adds 0.03–0.05 mm (0.001–0.002 in) per card.
- Paper weight records must state gsm directly; when cross-referencing US paper equivalents, distinguish Text LB (25 × 38 in / 635 × 965 mm basis sheet) from Cover LB (20 × 26 in / 508 × 660 mm basis sheet).
- Trim, Bleed, Safety, and Corner Radius: Finished trim must leave no white bleed edges (3 mm / 0.118 in bleed per side in prepress). Essential text and graphics require at least 3 mm (0.118 in) safety margin; bordered backs require at least 4–5 mm (0.157–0.197 in) to absorb die-cutting shift without visible asymmetry. Standard rounded corners measure R3–R3.5 mm (0.118–0.138 in).
- Box and Stack Clearance: Deck-to-box fit requires 1.5–2.5 mm (0.059–0.098 in) clearance across width and height and 1.5–3 mm (0.059–0.118 in) clearance for total stack height.
- Color, Ink Coverage, and Surface: Verify CMYK output and separate spot layers against approved proofs, 100% K crispness on fine text, rich black balance (C40–60 M30–40 Y30–40 K100), and total area coverage (TAC) at or below 280%–300%. Dark artwork finished with anti-scuff matte lamination is checked under angled light for burnishing or rub marks.
- Carton Weight Verification: Master cartons in the lot are weighed in both kg and lb against the packing specification before palletization.
Job-Specific Inspection Steps
1. Universal Lot-Sampling Sequence (All Decks)
- Pre-pack and collation audit: Pull sample decks across early, middle, and late press-sheet cuts. Fan each deck to confirm exact card count and uninterrupted collation sequence (no duplicated, missing, or inverted cards).
- Border and trim inspection: Align the deck faces and backs flush on a flat surface. Check all four edges for equal border margins on bordered backs, clean shear lines, and uniform R3–R3.5 mm (0.118–0.138 in) corner rounding without stepped notches.
- Scuff and rub check: Inspect dark solids and high-coverage areas (near the 280%–300% TAC ceiling) for ink transfer, white scuff streaks, or matte-film burnishing caused by automated collating belts.
- Caliper and box-fit check: Measure stack height with calipers and insert the finished deck into its tuck box or rigid box (1.5/2/2.5/3 mm greyboard, 0.059/0.079/0.098/0.118 in) to confirm smooth insertion within the 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) height clearances.
2. Gilded-Edge Routing
- Lamination conflict check: Confirm that thick lamination was not paired with edge gilding in a way that causes film lift along the trimmed edge.
- Flex and fan test: Fan the deck in both directions under raking light. Check for bare paperboard flecks, bridged foil sticking adjacent cards together, or uneven metallic coverage at rounded corners.
3. PVC-Substrate Routing
- Static and separation check: Shuffle and deal a sample deck to verify that static buildup does not bind cards together or cause double-feeds.
- Adhesion and flatness check: Inspect printed and coated surfaces at the cut edge for ink chipping or varnish lift. Lay a full deck on a flat reference plate to check for edge curl or cupping.
4. Custom-Profile and Shaped-Deck Routing
- Die-to-print registration: Check asymmetric curves, notches, or non-rectangular perimeters against the ≥3 mm (0.118 in) safety zone (or ≥4–5 mm / 0.157–0.197 in for bordered backs) so artwork is not clipped by the custom rule die.
- Nesting and packaging clearance: Verify that shaped decks sit inside their box or insert without binding on tight internal radii.
Sign-Off Criteria and Regulatory Records
A lot is cleared for packing when sampled decks meet these conditions:
- Count and collation: Zero missing, duplicated, or out-of-sequence cards in the lot sample.
- Trim and borders: Clean, burr-free edges and visually balanced borders within the ≥4–5 mm (0.157–0.197 in) bordered-back safety allowance.
- Surface and edge finish: No visible scuffing on dark anti-scuff matte surfaces, no foil flaking on gilded edges, and no ink lift on 0.30 mm (0.012 in) PVC.
- Box fit: Free insertion and removal within 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) stack-height tolerances.
Where destination-market rules apply, lot sign-off also verifies that required compliance documentation is on file before release—without inferring automatic pass status from visual inspection alone:
- EN 71 assessment and testing: If the deck falls under EU toy safety scope, confirm that third-party assessment and testing records are linked to the exact lot ink, coating, and substrate bill of materials per the European Commission Toy Safety framework.
- Packaging registration and sorting marks: For lots shipping into Germany or France, verify printed packaging marks and registration records against VerpackG participation and data reporting and French Triman / Info-Tri sorting guidance.
Concrete Failure Modes
| Failure Mode | Physical Cause | Lot Outcome |
|---|---|---|
| Uneven bordered backs | Die-cut shift exceeding safety margin (under 4–5 mm / 0.157–0.197 in) | Hold lot; sort and re-cut or reprint affected sheets |
| Gilded foil flaking or card sticking | Thick lamination edge resistance or excess foil heat/pressure | Reject affected gilded decks; strip or re-run with compatible coating |
| Dark-artwork scuff streaks | High TAC (>280%–300%) or standard gloss/matte film abraded during collation | Hold lot; verify anti-scuff matte film spec and belt tension |
| Deck jams in box | Stack height swollen by double-sided film (+0.03–0.05 mm / 0.001–0.002 in per card) exceeding 1.5–3 mm (0.059–0.118 in) clearance | Re-check box dieline clearance before further packing |
| PVC edge chipping or burr | Dull die rule or incompatible ink/varnish curing on 0.30 mm (0.012 in) PVC | Quarantine lot; inspect die sharpness and curing adhesion |
| Collation sequence skip | Misfeed at automated collator pocket or unflagged splice sheet | 100% deck re-check or automated weight/count re-sorting |
Guides in this section
Parent guide Production Lot Inspection and AQL