Specifications and Inspection Targets
Dual-layer boards combine a die-cut upper layer laminated onto a printed base layer. Verify incoming lot samples against these dimensional and finishing targets:
| Checkpoint | Target Specification | Condition That Changes It |
|---|---|---|
| Greyboard layer thickness | 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in) per layer | Deeper token cavities require a thicker upper greyboard layer; verify total stack height against box clearance. |
| Wrap margin | 15–20 mm (0.591–0.787 in) | Full-wrap edges require consistent turn-in tension to prevent corner lifting and directional bowing. |
| Die-cut divider & bleed clearance | 3–4 mm (0.118–0.157 in) minimum divider/die gap; 3 mm (0.118 in) bleed and >=3 mm (0.118 in) safety | Dividers narrower than 3–4 mm (0.118–0.157 in) lose structural stiffness and delaminate easily during die-cutting or handling. |
| Box stack clearance | 1.5–2.5 mm (0.059–0.098 in) width/height; 1.5–3 mm (0.059–0.118 in) stack height | Warped boards or adhesive build-up can exceed stack-height clearance and bow the game box lid. |
| Surface finish | Anti-scuff matte film on dark artwork | High-coverage dark wraps show rub marks during transit and collation without anti-scuff matte lamination. |
Job-Specific Lot Inspection Steps
Pull samples across the start, middle, and end of the production run according to the agreed AQL sampling plan, then run four physical checks:
- Check window-to-base print registration. Lay each sampled board flat under even light and inspect every recessed window against the printed base-layer tracks, numbers, and cell borders. Confirm that die-cut edges do not clip safety-margin text (>=3 mm / 0.118 in from cut lines) or expose unprinted greyboard.
- Test adhesive bonding around narrow dividers and edges. Gently flex the board along both axes and apply light thumb pressure to narrow internal bridges, window corners, and wrapped edges. Listen for crackling (dry glue spots) and look for lifted wrap paper, bubbles, or dried adhesive squeeze-out inside the cavities.
- Measure recess depth and test token cavity fit. Verify recess depth matches the specified upper greyboard caliper across all four corners and the center of the board. Drop actual production tokens (wood, acrylic, or punchboard) into multiple cavities across the sample set to confirm they sit flat, seat cleanly without binding on burred die edges, and lift out easily.
- Verify flatness, warp resistance, and box fit. Place single boards and full player-count stacks on a flat reference surface to check for cupping or corner lift. Confirm the full stack drops into the production box interior within the 1.5–2.5 mm (0.059–0.098 in) lateral and 1.5–3 mm (0.059–0.118 in) stack-height clearances.
Sign-Off Criteria
- Reject or sort the lot for any delamination on narrow dividers, exposed raw greyboard inside printed windows, clipped base-layer text, adhesive squeeze-out that blocks token seating, or warping that prevents the board stack from fitting inside the box clearance.
- Accept within tolerance when window-to-base registration stays inside the 3 mm (0.118 in) bleed/safety envelope with no clipped graphics, all tokens seat flush in their cavities, and single-board bow does not interfere with token placement on a flat table.
Concrete Failure Modes
| Failure Mode | Physical Cause | Inspection Action |
|---|---|---|
| Window-to-base misregistration | Sheet-to-die alignment drift during upper-to-base lamination | Check outer and center windows across the run; reject boards with clipped cell labels or visible unprinted margins. |
| Narrow-divider delamination | Insufficient adhesive coverage or excessive die pressure on dividers under 3–4 mm (0.118–0.157 in) | Flex narrow bridges gently; flag any lifting corners or dry spots for re-gluing or lot rejection. |
| Token binding in cavities | Adhesive squeeze-out into the recess, swollen board edges, or crushed/burred die-cut walls | Fit-test actual production tokens in tightest and smallest cavities across multiple boards. |
| Board cupping or bowing | Moisture imbalance between upper and base wraps, uneven lamination pressure, or asymmetric film tension | Stack-check on a flat surface after conditioning; verify the stack fits within the 1.5–3 mm (0.059–0.118 in) box stack-height clearance. |
| Scuffing on dark wraps | Friction during die-cutting, stacking, or transit on unlaminated or standard matte dark artwork | Inspect high-ink dark areas under angled light; confirm anti-scuff matte finish holds without rub marks. |