Inspection focus shifts with panel count, board caliper, and joint construction. Two-fold and four-fold boards concentrate stress on one or two primary spines, whereas six-fold and eight-fold boards stack multiple hinge thicknesses and require tighter wrap-margin and grain-direction control to lie flat. Interlocking boards replace cloth or paper hinges with die-cut tabs that must seat flush without lifting the face wrap. Standing GM screens add an upright balance requirement: panels must hold an angled arc on the table without twisting or tipping. For broader board and punchboard lot procedures, see board and punchboard inspection.
Specifications and Inspection Reference
| Attribute | Target Specification | Condition That Changes Inspection Focus |
|---|---|---|
| Greyboard core thickness | 1.5 mm (0.059 in), 2.0 mm (0.079 in), 2.5 mm (0.098 in), or 3.0 mm (0.118 in) | Thicker 2.5–3.0 mm (0.098–0.118 in) cores require wider hinge gaps so folded panels close without straining the outer wrap. |
| Wrap margin | 15–20 mm (0.591–0.787 in) turned over edges | Corners and spine ends on multi-fold boards need full adhesive contact to prevent edge lifting. |
| Bleed and safety | 3 mm (0.118 in) bleed per side; >= 3 mm (0.118 in) safety from edges and fold lines | Text or fine borders placed inside the 3 mm (0.118 in) safety zone risk distortion or clipping at the hinge. |
| Print and ink limits | CMYK with separate spot layers; >= 300 DPI; TAC <= 280%–300% | Heavy ink coverage above 300% TAC cracks more readily along folded spines. |
| Surface finish | Anti-scuff matte lamination recommended for dark artwork | Gloss or unlaminated dark solids show rub marks and hinge whitening faster during repeated flexing. |
| Format scope | Two-fold to eight-fold wrapped boards, interlocking boards, standing GM screens | Eight-fold layouts compound minor mounting skew; GM screens require symmetric fold tension to stand upright. |
Lot Inspection Checkpoints
- Hinge flex and wrap integrity Open and close each sampled board or GM screen through its full range of motion multiple times. Inspect both the outer face wrap and inner backing liner along every spine for cracking, ink whitening, bubbling, or adhesive separation. Check the 15–20 mm (0.591–0.787 in) turned-over wrap margins and mitred corners for clean adhesion.
- Table flatness and standing stability Unfold two-fold to eight-fold boards onto a flat inspection surface and check whether all panels settle evenly without tenting at the hinge or cupping upward at the outer corners. Stand sampled GM screens in their intended winged or zig-zag configuration on a level table to confirm each panel contacts the surface cleanly and the screen remains upright without leaning or rocking.
- Cross-crease artwork and interlocking alignment Check grids, tracks, and continuous illustrations crossing each hinge gap for vertical step-offset, stretching, or missing detail. For interlocking boards, assemble the full set of modular panels and inspect each joint for flush seating, consistent gap width, and clean die-cut edges.
- Surface finish and edge condition Examine dark-ink areas and spot-varnish zones near creases under angled light for scuffing, flaking, or film delamination. Run a finger lightly along wrapped edges and interlocking tabs to confirm there are no sharp paper burrs or lifted wrap edges.
Sign-Off Criteria
- Hinges: No splitting, cracking, whitening, or liner separation appears on any spine after repeated opening and closing.
- Flatness and stance: Folding boards lie flat on the table without rocking or persistent spine tenting; GM screens stand stably on a flat surface in their display arc.
- Alignment: Artwork, borders, and grid lines crossing creases align within visual register, and interlocking tabs seat smoothly without forcing or tearing the wrap.
- Edges and finish: All 15–20 mm (0.591–0.787 in) wrap turn-ins remain bonded, and laminated surfaces show no peeling or scuffing from normal handling.
Concrete Failure Modes
- Spine cracking or ink whitening on dark artwork: Caused by total ink coverage exceeding 280%–300% TAC, brittle surface coating, or an undersized hinge gap for 2.5–3.0 mm (0.098–0.118 in) greyboard.
- Panel bowing or tenting: Caused by mismatched grain direction between the face sheet, greyboard core, and backing liner, or uneven moisture uptake after lamination and mounting.
- Cross-crease artwork step-offset: Caused by sheet shift during board mounting or uncompensated hinge-gap spacing across four-fold to eight-fold layouts.
- Interlocking tab binding or wrap tear: Caused by worn die-cutting rules compressing thick greyboard instead of shearing cleanly, or weak glue tack along cut tab edges.
- GM screen tipping or panel twist: Caused by warped greyboard panels or unequal tension across consecutive hinges preventing even table contact.
Parent guide Game Board and Punchboard Lot Inspection