Approval criteria shift based on three job conditions:
- Card caliper and finish: Heavier stocks (such as 350 gsm art stock at 0.34–0.38 mm / 0.013–0.015 in or 400 gsm stock at 0.40–0.44 mm / 0.016–0.017 in) and double-sided film lamination (which adds 0.03–0.05 mm / 0.001–0.002 in per card) require tighter attention to side-weld width and mouth clearance than thinner 300 gsm (0.28–0.31 mm / 0.011–0.012 in) or 0.30 mm (0.012 in) PVC cards. Note that when comparing paper specs, US Cover LB uses a 20 x 26 in basis sheet, whereas US Text LB uses a 25 x 38 in basis sheet.
- Printed vs. unprinted film: Printed sleeve backs add ink and protective coating layers, requiring adhesion, rub-resistance, and color-registration checks on top of standard film inspection.
- Boxed-game integration: If sleeved cards must fit inside a game box or tray, sample approval must also verify the sleeved stack height against box clearance (1.5–2.5 mm / 0.059–0.098 in across width and height, and 1.5–3 mm / 0.059–0.118 in for stack height).
Governing Specifications and Sample Checks
Evaluate pre-production sleeve samples as part of non-paper sample approval across four physical dimensions:
| Check Area | What to Verify | Physical Condition for Approval |
|---|---|---|
| Film clarity and texture | Front window transparency; matte or textured back consistency | Clear fronts show crisp card artwork with no haze, fish-eyes, or die streaks; matte or textured backs show uniform grain across the pack without glossy patches. |
| Ultrasonic weld-seam strength | Left and right side seams; bottom fold transition | Side welds are continuous, flat, and free of pinholes, brittle burn-through, or weak gaps; seams resist splitting when a card is inserted and flexed. |
| Cut tolerance and height | Overall sleeve height; mouth lip alignment | Top edges are cleanly sheared with no film burrs; front and back lips align within the pack so cards do not protrude above the opening. |
| Live-card fit | Insertion resistance; corner clearance; stack behavior | Finished cards slide in cleanly without bowing or catching on the side welds, leaving minimal side play and consistent top coverage. |
Pre-Production Sample Approval Steps
Inspect film optics and surface finish under neutral light. Hold clear-front sleeves over printed card faces to check for cloudiness, extrusion lines, or surface scratches. For matte or anti-glare fronts and textured backs, fan multiple samples side by side to confirm consistent sheen and grain density. If the backs are printed, verify CMYK/spot color match, artwork centering, and scuff resistance.
Measure cut height uniformity across the sample batch. Stack 10 or more sample sleeves flush on the bottom fold on a flat surface. Inspect the top opening for stepped or uneven cut heights, skewed corners, and jagged knife marks left by dull slitting or guillotine blades.
Run live-card insertion and handling tests. Insert finished production cards—or matched-caliper dummies matching the job's exact stock (for example, 310 gsm black-core linen at 0.30–0.32 mm / 0.012–0.013 in or 330 gsm black core at 0.32–0.34 mm / 0.013–0.013 in) and lamination thickness—into at least 10–20 sleeves. Confirm that cards seat fully at the bottom fold without forcing the side seams outward or bowing the card face. Shuffle the sleeved stack to check corner catch and static cling.
Stress-test ultrasonic side welds. Apply firm thumb-and-finger outward pressure at the top mouth corners and along the mid-seam of several sample sleeves. An acceptable ultrasonic weld holds firm without unzipping or delaminating, and the film beside the weld does not tear cleanly along a brittle heat-affected line.
Verify sleeved-stack dimensions and pack weight. Calculate and measure the sleeved stack thickness:
sleeved stack height = card count * (card caliper + 2 * sleeve wall thickness)If the sleeves ship inside a retail box or board game, test-fit the full sleeved deck into the box cavity to confirm the 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) stack-height clearances remain intact. Record sample pack weight in both kg and lb (using 1 kg = 2.205 lb) if master carton or freight weight limits are tight.Document sign-off or revision instructions. Approve the sample only when all four checks pass on the same sample lot. If weld strength, cut height, or fit fails, specify the exact defect and affected dimension in writing and require a corrected pre-production sample before full-run tooling and film slitting begin.
Sign-Off Criteria
- Pass: Cards insert smoothly with zero bowing; top card edges sit fully recessed below the sleeve mouth; clear fronts show no distortion; matte/textured surfaces match across samples; ultrasonic side welds resist manual mouth-spreading stress without splitting.
- Hold / Revise: Any sleeve splits along a side weld during normal insertion or shuffling; card corners catch on internal weld ridges; cut height varies visibly across a stacked sample; film exhibits haze, pinholes, or ink scuffing.
Concrete Failure Modes
- Side-weld splitting at the top mouth: Caused by insufficient ultrasonic energy, contaminated film edges, or overly tight sleeve width forcing cards against the seam during insertion. Results in immediate seam unzipping during shuffling.
- Brittle seam tearing next to the weld: Caused by excessive ultrasonic dwell time or pressure thinning the film immediately adjacent to the weld line. The weld itself stays fused while the surrounding film tears cleanly under light stress.
- Card bowing or "banana" curl: Caused by an undersized inner width tolerance relative to the finished card trim and caliper, or uneven tension between the front and back film layers.
- Inconsistent cut height and exposed card tops: Caused by film web wander during folding or poor registration at the cross-cut knife. Taller cards or uneven cuts leave the top edge of the card exposed to wear.
- Optical haze or uneven matte grain: Caused by resin contamination, inconsistent chill-roll cooling during film extrusion, or mixed film batches. Reduces artwork legibility and creates visible variation across a deck.
- Box cavity overflow after sleeving: Caused by approving sleeve fit in isolation without accounting for doubled wall thickness across the full deck, violating the 1.5–3 mm (0.059–0.118 in) stack-height clearance in paired packaging.
Compliance and Packaging Documentation
When card sleeves are sold as standalone retail accessories or included in boxed games for regulated markets, align sample and packaging records with applicable channel requirements:
- Toy safety: For products intended for children, arrange assessment and testing against EN 71 using final production film and inks.
- Packaging and recycling: Where applicable to the destination market, maintain packaging participation records under VerpackG and apply required sorting markings such as Triman on outer sleeve packs or retail boxes.
Parent guide Approving Partner-Sourced Non-Paper Piece Samples
Related guides
- Approving Pre-Production Samples for Acrylic Pieces and Standees
- Approving Pre-Production Samples for Resin and Acrylic Dice
- Approving Pre-Production Samples for EVA Foam and Formed Trays
- Approving Pre-Production Samples for Metal Coins
- Approving Pre-Production Samples for Neoprene Mats and Pouches
- Approving Pre-Production Samples for Wooden Pieces