Deep multi-level 3D relief, bright mirror finishes, and reeded rims require tighter die-fill and deburring checks than flat 2D coins with matte antique plating. When a game includes multiple coin denominations, inspect all sizes together to confirm that plating tone and finish sheen stay consistent across different die cavities.
Sample Specifications and Acceptance Criteria
Evaluate every pre-production coin sample across four physical and visual benchmarks:
| Check Area | What to Verify | Conditions That Change Acceptance |
|---|---|---|
| 3D relief sharpness | Clean edges on raised elements, legible micro-text, and full metal fill at the highest points | High-relief sculpts and sharp 90-degree walls are prone to under-fill unless draft angles are sloped |
| Electroplating and antique wash | Uniform base plating on faces and rims, even dark wash in recesses, and clean highlights on raised areas | Matte antique finishes hide minor micro-scratches; bright nickel or gold plating exposes any surface pitting |
| Rim finishing and deburring | Smooth outer circumference, clean parting-line removal, and intact reeding or edge lettering | Aggressive barrel tumbling removes burrs faster but rounds off sharp 3D face details |
| Unit weight and dimensions | Consistent gram weight (g / oz) across samples and matching diameter/thickness (mm / in) per the 3D CAD | Multi-coin sets packaged by bulk weight (kg / lb) require tighter single-coin weight stability |
If the finished tabletop game is marketed for children, EU Toy Safety (EN 71) assessment and testing apply to production-representative metal coin samples, covering mechanical sharp-edge checks, small-parts sizing, and chemical migration limits on the zinc alloy and surface coatings.
Pre-Production Sample Review Steps
- Inspect under neutral lighting. Place the physical coin samples beside the approved 3D render and plating swatch under diffused daylight-balanced lighting so glare does not mask uneven plating or wash buildup.
- Check obverse and reverse relief alignment. Confirm that raised borders, fine typography, and recessed textures are fully formed without soft corners, sink marks, or trapped air pockets.
- Compare finish consistency across multiple pieces. Line up at least three to five samples from the same pre-production run to verify that hand-wiped or tumbled antique wash leaves uniform shading in the recesses.
- Test rim and edge feel. Run a finger around the circumference and across any reeded or chamfered edges to confirm that die flash and parting-line burrs are fully removed without scratching or snagging.
- Verify unit weight and caliper measurements. Weigh each sample individually in grams (g / oz) and measure diameter and total thickness in millimetres and inches (mm / in) to confirm consistent cavity fill and rim trim.
- Log markups before golden-sample sign-off. Record any required changes to strike pressure, wash dwell time, or deburring duration on annotated photos for the manufacturing partner before authorizing full production.
Common Failure Modes and Corrective Actions
- Under-filled high points or soft lettering: Occurs when zinc alloy does not reach the deepest parts of the die cavity or when steep vertical walls trap air. Corrective action: increase strike tonnage, add die venting, or soften steep draft angles in the 3D tooling.
- Blotchy antique wash or exposed base metal: Caused by uneven hand-wiping, insufficient wash dwell time, or over-polishing that strips thin electroplating off raised edges. Corrective action: standardize tumbling media and wipe duration, increase plating thickness, and apply a uniform protective clear coat.
- Sharp rim burrs or rounded face detail: Happens when trim dies leave flash along the parting line or when heavy barrel deburring wears down crisp 3D artwork. Corrective action: refine the trim die clearance for the rim and shorten face-tumbling cycles.
- Unit weight drift across samples: Results from inconsistent blank sizing, partial cavity fill, or uneven rim grinding. Corrective action: tighten blank weight sorting and re-check cavity fill consistency before locking the approved golden sample.
Parent guide Approving Partner-Sourced Non-Paper Piece Samples
Related guides
- Approving Pre-Production Samples for Acrylic Pieces and Standees
- Approving Pre-Production Samples for Card Sleeves
- Approving Pre-Production Samples for Resin and Acrylic Dice
- Approving Pre-Production Samples for EVA Foam and Formed Trays
- Approving Pre-Production Samples for Neoprene Mats and Pouches