This approval gate changes based on tooling status, resin versus acrylic formulation, and edge finish:

  • Custom mold T1 samples vs. standard stock dice: Custom-engraved faces or non-standard geometries require a T1 tooling sample to verify cavity depth, draft angles, and parting-line placement before texturing or final polish. Standard stock dice skip mold validation and focus on batch consistency, paint fill, and surface finish.
  • Translucent and clear vs. opaque mixes: Clear, translucent, or suspended-inclusion dice expose internal air voids, flow lines, and cure seams under direct light. Opaque mixes conceal interior artifacts, shifting inspection weight toward surface pinholes, sink marks, and balanced mass.
  • Tumbled vs. sharp-edge profiles: Standard rounded-corner dice rely on media tumbling, where over-tumbling softens face cavities and distorts flat planes. Sharp-edge resin dice bypass aggressive tumbling and require clean mold-seam removal without rounding the vertices.

Pre-Production Inspection Criteria

Evaluate physical samples from the non-paper pre-production sample workflow against the approved 3D CAD file or artwork proof across five core checks:

Inspection Area What to Verify Condition That Changes the Check
Mold-cavity definition Crisp cavity walls, uniform engraving depth, and clean icon or numeral strokes Custom T1 molds require checking fine serifs and narrow bridges for incomplete fill or metal flash
Pip and icon paint fill Even pigment coverage sitting flush or cleanly recessed within the cavity, with zero haloing on the surrounding face High-contrast ink on textured or matte faces requires closer inspection for capillary bleed
Corner tumbling Uniform edge radius and consistent corner rounding across every face of the die Sharp-edge dice must show crisp vertices and flat faces with no tumbling wear
Surface polish Smooth, even sheen matching the approved gloss or matte specification, free of swirl marks or haze Clear and dark-pigmented dice show micro-scratches and polishing compound residue most clearly
Internal air voids Zero visible bubbles, cloudy pockets, or surface pinholes Translucent and clear resin or acrylic requires backlighting each face to inspect the core

Resin vs. Acrylic Sample Conditions

Resin and acrylic behave differently during molding and finishing, which changes where defects appear on pre-production samples:

  • Cast resin dice: Resin cures in silicone or custom molds and is prone to trapped micro-bubbles, surface pinholes along upper mold faces, and slight meniscus distortion. Inspect the sprue or gate face closely for sanding marks and uneven polish.
  • Injection-molded or machined acrylic dice: Acrylic offers tighter dimensional repeatability across large runs, measured face-to-face in millimetres and inches (mm / in) against the spec, but can exhibit weld lines, sink marks near thick sections, or gate blush if mold temperature and packing pressure drift.

Sample Review and Sign-Off Steps

  1. Verify dimensions and mass: Measure opposing face-to-face dimensions with calipers (mm / in) and weigh a sample set (kg / lb) to confirm consistency with the approved tooling drawing or stock catalog specification.
  2. Inspect mold cavities and edges under raking light: Angle each die under directional light to check cavity wall sharpness, parting-line witness marks, and uniform corner tumbling across all faces.
  3. Backlight translucent and clear samples: Hold clear or translucent dice over a bright white light source to check for internal air voids, suspended debris, or resin cure layers.
  4. Audit paint fill and wipe quality: Check every pip, numeral, and custom icon for complete pigment coverage, consistent color tone, and clean face wiping without smearing into surface micro-scratches.
  5. Log corrections or lock the golden sample: Document any cavity flash, underfilled ink, or polish haze with face-specific photos for a T2 correction or re-inking run. Once every check passes, retain signed physical samples as the golden reference for mass production and final AQL inspection.

Sign-Off Criteria

Approve the pre-production sample for mass production only when all of the following conditions hold:

  • Custom T1 tooling: All engraved faces match the approved artwork geometry, cavity walls are sharp with no short shots or flash, and parting lines sit cleanly without distorting edge symmetry.
  • Pip and icon fill: Paint sits evenly inside every recess with no missing fill, bubbles in the dried ink, or pigment staining on the face surface.
  • Tumbling and polish: Corner radii match across all dice in the sample set, faces sit flat without rocker distortion, and the polish matches the target sheen without cloudiness.
  • Internal clarity: Clear and translucent dice show zero visible internal air voids, and opaque dice show zero surface pinholes or sink depressions.

Common Failure Modes

  • Soft cavity edges or flashing: Caused by worn mold seams, insufficient clamping pressure, or over-tumbling after molding. Flashing leaves thin plastic fins around pips or edges; over-tumbling rounds off the top rim of engraved icons.
  • Paint haloing, bleed, or underfill: Caused by wiping excess ink before the paint sets, uneven face polish that traps pigment in micro-scratches, or air pockets in narrow icon strokes that leave recessed gaps after drying.
  • Uneven corner tumbling: Caused by inconsistent media mix, overloaded tumbling barrels, or short cycle times, resulting in one face or corner looking sharper than the rest of the die.
  • Polishing haze and swirl marks: Caused by skipping grit stages during wet sanding or leaving dried polishing compound inside recessed pips and icons.
  • Internal air voids and sink marks: Caused by inadequate vacuum degassing in cast resin or insufficient holding pressure in injection-molded acrylic, creating visible bubbles in clear dice or balance and surface defects in opaque dice.

Compliance and Assessment Records

When resin or acrylic dice are packaged in games or kits intended for children or subject to toy safety rules, applicable assessment and testing procedures—such as EN 71 mechanical, physical, and chemical requirements—depend on the target market and age grading. Maintain material declarations and test records aligned with the official European Commission Toy Safety framework before releasing finished goods for distribution.