Order a physical structural sample whenever a project uses a custom box size, a multi-component insert, a folding game board, or a custom punchboard die. A CAD dieline alone is sufficient only when reusing a partner's existing, unmodified stock tuck-box or standard card-box tooling with a known card count and stock caliper. Even then, changing card stock weight, adding double-sided lamination, or switching from a 1.5 mm (0.059 in) to a 2.5 mm (0.098 in) greyboard changes internal tolerances and requires a fresh white sample. This stage sits within pre-production proofing and locks the mechanical dieline before color proofs or plates are made.
Structural Specifications and Tolerance Baselines
Request white samples in the exact production greyboard, paperboard, and core stocks rather than generic mockup board. Basis weights must be specified in gsm alongside US basis weights where applicable—distinguishing US Text LB (based on a 25 × 38 in sheet) from Cover LB (based on a 20 × 26 in sheet)—because stiffness and caliper vary by fiber density and coating.
| Component | Target Specification (Metric / Imperial) | Structural Function & Sample Check |
|---|---|---|
| Box Clearance (Width & Height) | 1.5–2.5 mm (0.059–0.098 in) | Prevents binding against deck edges or insert walls while avoiding rattle |
| Box Clearance (Stack Height) | 1.5–3 mm (0.059–0.118 in) | Absorbs caliper variation across cards, booklets, and air gaps |
| Rigid Box & Board Greyboard | 1.5 / 2 / 2.5 / 3 mm (0.059 / 0.079 / 0.098 / 0.118 in) | Sets wall rigidity, lid weight, and required wrap allowance |
| Greyboard Wrap Margin | 15–20 mm (0.591–0.787 in) | Ensures outer wrap folds cleanly around board edges without lifting |
| Punchboard Die Gap | 3–4 mm (0.118–0.157 in) | Maintains frame strength between adjacent tokens during cutting and transit |
| Booklet Interior Sheet Caliper | 80–120 gsm; ~0.08–0.13 mm (0.0031–0.0051 in) per sheet | Determines total booklet thickness inside box cavities and insert wells |
Card stack height drives box and insert depth. Calculate expected deck height before reviewing a sample using the stock caliper plus any film finish:
Deck stack height = (Card count * Base card caliper) + (Card count * Film thickness)
Approximate per-card base calipers to use when verifying cavity depth:
- 300 gsm art / blue core: 0.28–0.31 mm (0.0110–0.0122 in)
- 310 gsm black-core linen: 0.30–0.32 mm (0.0118–0.0126 in)
- 330 gsm black core: 0.32–0.34 mm (0.0126–0.0134 in)
- 350 gsm art stock: 0.34–0.38 mm (0.0134–0.0150 in)
- 400 gsm stock: 0.40–0.44 mm (0.0157–0.0173 in)
- PVC: 0.30 mm (0.0118 in)
- Double-sided film lamination: adds 0.03–0.05 mm (0.0012–0.0020 in) per card
For a 100-card deck, double-sided film alone adds 3.0–5.0 mm (0.118–0.197 in) to the stack, which exceeds standard stack clearance if omitted from the structural brief.
Production and Testing Workflow
- Lock component counts and stack math. Send finalized component dimensions, card counts, stock gsm, lamination choices, and booklet page counts (multiples of 4: saddle stitch 12–40 pages, perfect binding 28+ pages, sewn binding 80–100+ pages) to the manufacturing partner in vector format (AI or PDF/X-4) so they can generate the CAD dieline.
- Produce the unprinted white sample. The partner cuts the box, insert, board, and punchboards on a CAD plotter (or production die if hard tooling is already authorized) using the actual production greyboard thickness and paperboard stock. Note that CAD-plotter samples may lack the compression of a steel-rule production die on score lines, so evaluate fold resistance with that difference in mind.
- Load with dummy production-weight contents. Never test an empty box or insert. Fill the sample with a full card stack of the target caliper, any folded 4/6/8-panel leaflets or bound booklets (200–300 gsm covers), and representative tokens or boards.
- Run component-specific physical checks:
- Boxes (tuck and rigid two-piece): Close the box fully, invert it, and observe lid friction. A rigid telescoping lid should hold its own weight briefly before sliding smoothly off the base without prying. Tuck flaps should seat flush without bowing the front panel.
- Inserts: Invert and gently shake the closed box. Decks, tiles, and booklets must stay in their wells without sliding over dividers. Check finger-notch cutouts to confirm a deck can be lifted out cleanly without bending cards.
- Folding boards: Open and close the board across its hinge seams repeatedly, then lay it flat on a table. Inspect the 15–20 mm (0.591–0.787 in) wrap margins along the outer edges and inner hinge channels for bubbling, tension creases, or exposed greyboard.
- Punchboards: Press out a cross-section of small, large, and complex-shape tokens. Confirm the nicks (tiny uncut bridges holding tokens in the sheet) keep pieces secure when the sheet is flexed or shaken, yet release cleanly under thumb pressure without tearing the top or bottom paper liner.
- Issue redlines or written sign-off. Mark exact millimetre/inch adjustments directly on the sample photos and CAD PDF (e.g., "+1.5 mm (+0.059 in) cavity depth" or "deepen thumb notch by 2 mm (0.079 in)") before approving pre-production proofing to proceed to print.
Sign-Off Criteria
Approve the unprinted structural sample only when all of the following conditions hold:
- Box fit: Loaded components sit within the 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) stack clearances without bulging walls or crushing card corners.
- Lid & flap action: Rigid lids release smoothly under gravity or light pull without sticking or falling open; tuck-box dust flaps and locking tabs close flat without spring-back.
- Insert retention: Dividers support the full weight of loaded decks and greyboard sheets without buckling, and components remain seated when the closed box is inverted.
- Board hinge & wrap: Folding hinges open flat without lifting the wrap paper, cracking the spine liner, or leaving a gap wider than the greyboard specification allows.
- Punchboard release: Tokens stay intact in the 3–4 mm (0.118–0.157 in) die-gapped frame during handling and punch out cleanly with minimal fiber tear.
Concrete Failure Modes
- Cavity under-sizing from omitted film caliper: Calculating box or insert depth using only base card gsm while ignoring double-sided film (0.03–0.05 mm / 0.0012–0.0020 in per card) causes decks to bow rigid box lids or split tuck-box seams.
- Lid lock-up or loose drop on rigid boxes: Wrap paper grain direction or tight inner tolerances cause the lid to bind on two sides, requiring force to open; excessive clearance causes the lid to drop off during handling.
- Wrap delamination on thick greyboard: Using a wrap margin narrower than 15 mm (0.591 in) on 2.5–3 mm (0.098–0.118 in) greyboard leaves too little turn-in area, causing corners and edges to peel before assembly.
- Hinge cracking or tenting on folding boards: Shallow scoring or overly tight wrap tension across the fold prevents the board from lying flat or tears the hinge paper after repeated cycles.
- Punchboard liner tear vs. transit drop-out: Overly wide or thick nicks force buyers to pull tokens hard enough to peel the printed face paper; too few or shallow nicks allow tokens to fall loose inside the box before opening.
- Insert collapse under heavy stacks: Lightweight folding-carton dividers without adequate gussets or double-wall folds buckle under dense card stacks or thick greyboard punchboards, letting components shift in transit.
Guides in this section
Parent guide Production Proofs and Sample Approval