Unprinted white-dummy samples isolate board geometry, score behavior, and mechanical fit from print graphics. Approval criteria shift based on greyboard caliper—1.5, 2.0, 2.5, or 3.0 mm (0.059, 0.079, 0.098, or 0.118 in)—wrap turn-in allowance of 15 to 20 mm (0.591 to 0.787 in), and whether the sample is tested bare or with its final inner tray and card or component stack installed. For the broader sample workflow across packaging and components, see the structural sample approval guide.

Structural Specifications and Clearances

Boxed games and rigid packaging follow project-specific component minimums and tooling tolerances rather than flat deck minimums. Every structural sample must hold these base tolerances before wrap printing begins:

Parameter Metric Specification Inch Equivalent Structural Role
Greyboard caliper 1.5 / 2.0 / 2.5 / 3.0 mm 0.059 / 0.079 / 0.098 / 0.118 in Sets wall rigidity, V-groove depth, and outer footprint
Wrap turn-in margin 15–20 mm 0.591–0.787 in Covers board edges and lines interior lip or sleeve mouth
Width and height clearance 1.5–2.5 mm 0.059–0.098 in Prevents binding when loading decks, inserts, or trays
Stack height clearance 1.5–3.0 mm 0.059–0.118 in Absorbs component stack height without lifting the lid

Job-Specific Inspection Steps and Sign-Off Criteria

Test unprinted samples with actual-thickness contents or dummy blocks inside. Empty boxes flex differently and mask height interference.

1. Two-Piece Rigid Boxes (Lid Damping)

  1. Seat the lid squarely over the base with the base resting flat on a level bench.
  2. Lift the lid until only the bottom rim engages the base wall, then release it without downward pressure.
  3. Sign-off criteria: The lid descends smoothly on a controlled cushion of escaping air and seats flush against the base shoulder or bottom edge. A bare greyboard dummy must leave enough gap for the eventual outer wrap and lamination so the wrapped production lid does not bind.

2. Magnetic Closure Boxes (Flap Latch Alignment)

  1. Open the hinged spine and close the front flap across multiple cycles to relax the hinge crease.
  2. Check magnet engagement along the full length of the front lip and inspect the gap between the flap and front wall.
  3. Sign-off criteria: Magnets pull the flap shut cleanly without manual pressing, lateral skew, or corner lift. The hinge on 2.0 to 3.0 mm (0.079 to 0.118 in) greyboard folds flat without cracking the outer wrap or springing the flap back open.

3. Drawer and Slipcase Boxes (Pull Clearance)

  1. Load the inner drawer tray with its target contents and slide it fully into the outer sleeve.
  2. Pull the tray out using the thumb notch or ribbon pull with one hand while holding the sleeve lightly.
  3. Sign-off criteria: The tray slides smoothly across the full stroke without snagging on the 15 to 20 mm (0.591 to 0.787 in) interior wrap turn-in at the sleeve mouth. Sidewalls remain straight without bowing inward under light grip pressure.

4. Corner Squareness and Board Rigidity (All Styles)

  1. Measure diagonal lengths across opposite corners of the base, lid, or sleeve, and check all four corners with a right-angle square.
  2. Apply light vertical hand pressure to the top corners to test wall column strength.
  3. Sign-off criteria: Corners meet at 90 degrees with tight mitered V-grooves or stayed joints, zero daylight through the seam, and no sidewall bowing. Loaded contents sit within the 1.5 to 2.5 mm (0.059 to 0.098 in) width/height clearance and 1.5 to 3.0 mm (0.059 to 0.118 in) stack height clearance.

Concrete Failure Modes

Failure Mode Physical Cause Production Impact
Lid drops instantly or jams Lid-to-base gap too wide for air cushion, or too tight to absorb wrap and film thickness Lid separates during handling or locks onto the base after wrapping
Magnetic flap skews or springs open Misaligned magnet pockets, shallow spine score on 2.5–3.0 mm (0.098–0.118 in) board, or stack height exceeding clearance Flap sits crooked, fails to latch in transit, or stresses the hinge crease
Drawer catches at sleeve mouth Exposed edge of the 15–20 mm (0.591–0.787 in) wrap turn-in lifting, or sleeve height clearance under 1.5 mm (0.059 in) Tray tears the inner lining or requires excessive force to open
Gapped or racked corners Over-cut V-groove depth, loose corner stay tape, or 1.5 mm (0.059 in) greyboard flexing on large footprints Box twists out of square and crushes under carton stacking
Contents bind or rattle Internal clearance outside 1.5–2.5 mm (0.059–0.098 in) width/height or 1.5–3.0 mm (0.059–0.118 in) height Cards and inserts scuff during insertion or shift inside the box