Structural sign-off should happen on unprinted CAD-cut white samples before steel-rule dies are ordered, alongside broader component checks covered in structural sample proofing. The exact clearance target changes based on three conditions:
- Card stock and film thickness: Moving from 300 gsm art or blue-core stock to 350–400 gsm stock, or adding double-sided film lamination, expands total deck thickness by several millimetres across a full deck.
- Closure mechanism: Tuck boxes use dust flaps and a friction or slit-lock tongue to retain the deck, whereas slipcases and belly bands rely entirely on sidewall friction and require tighter dimensional control so cards do not slide out under their own mass.
- Intended storage state: Decks meant to be stored in third-party card sleeves after opening must be tested with sleeved cards rather than bare cards, as sleeves add bulk to both stack height and lateral width.
Clearance and Material Specifications
Use the following tolerances and reference calipers when specifying and measuring unprinted tuck-box, belly-band, and slipcase samples:
| Parameter | Target Specification | Notes |
|---|---|---|
| Width & height clearance | 1.5–2.5 mm (0.059–0.098 in) | Measured between card edges and inner box walls |
| Stack-height (depth) clearance | 1.5–3.0 mm (0.059–0.118 in) | Measured from top card face to closed inner lid |
| Double-sided film allowance | 0.03–0.05 mm (0.001–0.002 in) per card | Add to base card caliper before calculating depth |
| Bleed & safety margin | 3 mm (0.118 in) bleed; ≥3 mm (0.118 in) safety | Keep critical elements clear of score and cut lines |
Calculate the target internal depth using plain-text stack math before cutting the sample:
Target internal depth = (Card caliper + Film thickness) x Card count + 1.5 to 3.0 mm (0.059 to 0.118 in)
Reference calipers for common card stocks used in live test stacks:
- 300 gsm art / blue core: 0.28–0.31 mm (0.011–0.012 in) per card
- 310 gsm black-core linen: 0.30–0.32 mm (0.012–0.013 in) per card
- 330 gsm black core: 0.32–0.34 mm (0.013–0.013 in) per card
- 350 gsm art stock: 0.34–0.38 mm (0.013–0.015 in) per card
- 400 gsm stock: 0.40–0.44 mm (0.016–0.017 in) per card
- PVC: 0.30 mm (0.012 in) per card
When specifying paperboard for tuck boxes or paper for belly bands, state weights in gsm alongside US pound ratings and distinguish the basis sheet size: US Cover LB is measured on a 20 x 26 in (508 x 660 mm) basis sheet, while US Text LB is measured on a 25 x 38 in (635 x 965 mm) basis sheet. Lighter 80–120 gsm interior-grade paper (0.08–0.13 mm / 0.003–0.005 in per sheet) is suitable for thin belly bands, whereas tuck boxes and slipcases require rigid folding carton board matched to the deck's mass in kg and lb.
Testing Steps for Live Card Stacks
- Assemble the live target stack: Count out the exact production card quantity using the target card stock and finish. If the white sample arrives before laminated card sheets are ready, add 0.03–0.05 mm (0.001–0.002 in) per card to simulate double-sided film, and weigh the full stack in kg (lb) to verify the load the closure must support.
- Verify lateral and depth clearance: Slide the full stack into the unprinted tuck box or slipcase. Confirm 1.5–2.5 mm (0.059–0.098 in) clearance across width and height and 1.5–3.0 mm (0.059–0.118 in) in stack depth so the deck seats fully without bowing the front or back panels.
- Test tuck-flap engagement and lock: Fold the side dust flaps inward and seat the top tuck tongue. Invert the loaded box and tap it lightly to confirm the friction lock or slit-lock tab holds the full deck mass without popping open.
- Check thumb-notch and extraction clearance: Grasp the loaded stack through the thumb notch on the tuck box or slipcase. Pull the deck out in one smooth motion and re-insert it, checking that card corners do not catch on the dust-flap edges or scrape the notch corners.
- Test belly-band tension: Wrap the unprinted belly band around the bare card stack or inner tuck box. Hold the assembly vertically to confirm the band does not slip off under the stack's weight, then slide it off with two fingers to confirm it releases without denting card edges.
- Inspect score lines and board grain: Fold every crease 180 degrees and inspect the outer surface under raking light. Confirm the paperboard grain runs parallel to the vertical sidewalls so the box resists bowing and score lines do not crack—especially when anti-scuff matte or thick film lamination will be applied in production.
Sign-Off Criteria
Approve the structural sample and release the dieline for production tooling only when all of the following conditions are met:
- Measured clearance: Width and height play sit within 1.5–2.5 mm (0.059–0.098 in), and stack-height play sits within 1.5–3.0 mm (0.059–0.118 in) with the full laminated stack inserted.
- Closure retention: The tuck flap stays locked when the loaded box is held upside down; slipcases and belly bands retain the deck vertically without sliding loose.
- Clean extraction: The thumb notch exposes enough card edge for a firm pinch without tearing the board or catching on dust flaps during insertion.
- Intact creases: All score lines fold cleanly without fiber cracking or delamination along the hinges.
Concrete Failure Modes
- Bulging panels and popping tuck flaps: Testing with unlaminated cards or lower-caliper stock underestimates stack height. Once 0.03–0.05 mm (0.001–0.002 in) of double-sided film per card is added, the deck forces the front panel outward and pops the tuck tongue open. Fix by recalculating depth with the laminated caliper and expanding the side-gusset depth before cutting dies.
- Crushed card corners on insertion: Width clearance below 1.5 mm (0.059 in) or square-cut dust flaps snag the leading corners of the deck as players push cards back into the box. Fix by widening the dieline to 1.5–2.5 mm (0.059–0.098 in) clearance and adding angled bevels to the dust-flap leading edges.
- Belly-band slip or edge tearing: Bands sized on uncoated dummy stacks bind tightly once matte or high-friction film is added, or slide off glossy uncoated decks. Fix by sizing the band circumference on the final surface finish and aligning paper grain parallel to the wrap creases.
- Cracked score lines on dark artwork: Folding heavy carton board perpendicular to the grain—or pairing thick board with heavy film lamination—fractures the outer fibers along the lid hinge. Fix by orienting board grain parallel to the primary vertical scores and confirming score-channel width on the production board stock.
Parent guide Unprinted Structural Sample Approval