- Select 100 to 120 gsm (68 to 81 lb Text) opaque-lined or dark-dyed kraft for flat single-sheet clues or thin card packets where low stack height inside the box cavity matters most.
- Select 130 to 160 gsm (88 to 108 lb Text / 48 to 59 lb Cover) heavy uncoated or reinforced kraft for bulky multi-card dossiers, sharp-cornered punchboard tokens, or legacy envelopes subjected to repeated opening and resealing.
- Avoid standard 80 to 90 gsm (54 to 61 lb Text) white office envelope paper when enclosing high-contrast card backs, secret numbers, or dark graphics, because bright light reveals internal print through unlined white sheets.
- Avoid stocks heavier than 160 gsm (59 lb Cover) for standard folded-seam envelopes unless the design uses deep-scored gussets and wide glue flaps; heavier cover boards resist sharp folding, crack along cross-grain creases, and add unnecessary stack height.
For general sheet and booklet stock pairings that go inside these envelopes, refer to the parent booklet and paper stocks guide.
Envelope Stock Specifications and Basis Weight Equivalents
Paper weight is specified in grams per square meter (gsm), while US commercial mills separate Text LB (basis sheet 25 × 38 in / 635 × 965 mm) from Cover LB (basis sheet 20 × 26 in / 508 × 660 mm). Because the basis sheets differ in area, the same pound rating represents a much heavier sheet in Cover weight than in Text weight:
gsm = Text LB × 1.48(500-sheet basis ream of 68 lb Text weighs 30.8 kg / 68 lb; 100 lb Text weighs 45.4 kg / 100 lb)gsm = Cover LB × 2.71(500-sheet basis ream of 60 lb Cover weighs 27.2 kg / 60 lb)
| Stock Family | Weight Range (gsm) | US Text LB (25 × 38 in / 635 × 965 mm) | US Cover LB (20 × 26 in / 508 × 660 mm) | Opacity & Strength Profile | Best-Fit Use Case |
|---|---|---|---|---|---|
| Unbleached or Dyed Kraft | 100–160 gsm | 68–108 lb Text | 37–59 lb Cover | High tear and burst strength from long unbleached fibers; natural or dark dye blocks light-through peeking | Legacy clue packets, heavy card bundles, rough handling, vintage dossier aesthetics |
| Heavy Uncoated Offset | 120–160 gsm | 81–108 lb Text | 44–59 lb Cover | Crisp CMYK and spot ink reproduction; moderate tear strength; requires dense fiber or dark interior flood for opacity | Full-color illustrated dossiers, narrative envelopes, custom-printed mystery files |
| Opaque-Lined / Security Paper | 100–140 gsm | 68–95 lb Text | 37–52 lb Cover | Interior security tint or dark/metallic barrier layer stops backlighting even on light-colored exteriors | Bright white or cream secret envelopes enclosing dark-inked cards or spoiler sheets |
Note on interior inserts: Standard booklet interior sheets run 80–120 gsm (about 0.08–0.13 mm / 0.003–0.005 in per sheet). A single-fold 140 gsm envelope adds roughly 0.28–0.32 mm (0.011–0.013 in) to stack height before accounting for side-seam overlap.
Core Performance Requirements
Opacity Against Backlighting
Light-through peeking occurs when high-contrast text, barcodes, or dark card backs sit directly against an unlined white envelope under overhead room lighting or a flashlight. Weight alone does not guarantee opacity: a 120 gsm (81 lb Text) bright white uncoated sheet transmits more light than a 100 gsm (68 lb Text) dark-dyed kraft sheet. To prevent peeking on light-colored exteriors, specify either an opaque-lined security stock or an interior flood coat (such as a dense dark pattern or solid interior tint) printed before folding.
Tear and Burst Strength
Envelopes packed inside a boxed game experience lateral compression during shipping and point pressure from sharp card corners or die-cut tokens. Kraft paper retains longer wood fibers that resist edge tearing and corner punch-through better than short-fiber woodfree uncoated sheets. When heavy uncoated offset stock is required for crisp four-color artwork, step up to 140–160 gsm (95–108 lb Text / 52–59 lb Cover) to compensate for lower intrinsic tear resistance.
Fold Endurance and Grain Direction
Every envelope requires multiple 180-degree folds (side seams, bottom flap, and top closure flap). Align the paper grain parallel to the primary long fold (or the direction of the most-used opening crease) so fibers bend rather than snap. Cross-grain folds on 130–160 gsm stocks show visible cracking along dark printed solids and weaken the hinge on legacy envelopes opened multiple times.
Seam Adhesive Bonding
Side and bottom seams rely on cold PVA or hot-melt adhesive penetrating the paper fibers. Uncoated and kraft surfaces bond reliably once cured. If the exterior uses heavy ink coverage, varnish, or anti-scuff matte lamination to protect dark artwork, leave the glue-flap bonding zones unvarnished and unlaminated (with ink knocked out where possible) so adhesive contacts bare paper fibers directly.
Prepress, Sizing, and Production Steps
Card Deck Press coordinates custom envelope production through specialist offset and tabletop manufacturing partners. Boxed game tooling and custom die-cut envelopes follow project and component minimums rather than standard offset card-deck minimums (which start at 200 decks across usual tiers of 200 / 300 / 500 / 1,000+).
Sizing and Box Cavity Fit
Derive flat dieline and folded envelope dimensions from the enclosed component stack plus insertion clearance, rather than forcing contents into an arbitrary stock size:
- Account for the thickness of folded seams (four layers of stock at corner overlaps) when calculating stack height.
- Keep the finished envelope footprint within the game box's 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) stack-height allowance.
Prepress Specifications
- File Format & Color: Submit print-ready PDF/X-1a or PDF/X-4 exported from AI/PDF/PSD, using CMYK with separate spot layers where required (such as metallic ink or interior security tint).
- Resolution & Bleed: Supply raster artwork at ≥300 DPI, with 3 mm (0.118 in) bleed past the outer cut line on all sides and ≥3 mm (≥0.118 in) safety margin from all score lines and die-cut edges.
- Type & Black Ink: Outline or embed all fonts. Set fine text and thin rules to 100% K. Use rich black (C40–60 M30–40 Y30–40 K100) for large dark solids while keeping total area coverage (TAC) at ≤280%–300%.
- Surface Protection: Specify anti-scuff matte coating or varnish on dark full-bleed exterior artwork, with clean knockouts on all internal glue flaps.
Manufacturing Sequence
- Sheet Conditioning & Printing: Print exterior artwork and any interior opacity tint on grain-aligned sheets; allow ink and varnish to cure before die cutting.
- Die Cutting & Creasing: Cut the flat dieline and impress deep channel scores along all fold lines, verifying grain orientation on the press sheet.
- Folding & Seam Gluing: Fold side and bottom flaps and apply adhesive to bare, unvarnished glue zones; stack under controlled pressure until the seam bond cures.
- Closure Application & Packing: Apply peel-and-seal adhesive strips, remoistenable gum, or leave tuck-flap die cuts clean; pack envelopes flat in moisture-resistant bundles to prevent warping before box assembly.
Sign-Off Criteria and Regulatory Notes
Physical Sign-Off Checks
- Backlighting Opacity Check: Insert the highest-contrast card or printed clue sheet into a folded production sample and inspect under bright direct light; no text, numbers, or card-back borders may show through.
- Seam Peel Check: Pull folded side and bottom seams apart after full adhesive cure; paper fibers should tear before the glue line releases cleanly.
- Fold-Crack Inspection: Fold and open the closure flap repeatedly on dark-inked samples; score lines must remain intact without white fiber exposure or splitting.
- Box Fit Check: Place the loaded envelope stack into the final game box tray or cavity to confirm it sits flat within the 1.5–2.5 mm (0.059–0.098 in) lateral and 1.5–3 mm (0.059–0.118 in) vertical tolerances.
Regulatory Assessment Notes
- Toy Safety (EN 71): When clue envelopes are packaged inside games intended for children in the EU, physical, mechanical, and chemical properties fall under EN 71 assessment and testing procedures as outlined in the EU Toy Safety framework.
- Packaging & Recycling Marks: If envelopes function as disposable retail or outer packaging in regulated EU markets, verify producer registration, material coding, and sorting-label requirements against VerpackG (LUCID) and France's Triman / Info-Tri guidance before finalizing dieline artwork.
Concrete Failure Modes
| Failure Mode | Root Cause | Physical Outcome | Prevention |
|---|---|---|---|
| Light-Through Peeking | Unlined white 80–100 gsm (54–68 lb Text) stock used over high-contrast inserts | Players read secret numbers or card backs through the sealed envelope | Switch to dark-dyed kraft, opaque-lined security stock, or add a dense interior tint |
| Seam Splitting in Transit | Short-fiber lightweight stock or narrow glue flaps under tight box compression | Side or bottom seams pop open when sharp card corners press outward | Use 120–160 gsm kraft or heavy uncoated stock with wide glue flaps and full adhesive cure |
| Glue-Flap Pop-Open | Ink, aqueous varnish, or matte lamination extending onto the bonding surface | Adhesive sits on smooth coating rather than paper fiber and releases under tension | Knock out all ink, varnish, and film from glue-flap zones in the prepress dieline |
| Cracking Along Folds | Cross-grain sheet layout or stock heavier than 160 gsm (59 lb Cover) without deep creasing | White paper fibers split and flake along dark printed fold lines | Align primary folds parallel to paper grain and stay within 100–160 gsm |
| Ink Scuffing on Dark Solids | Unprotected heavy rich-black or dark spot ink rubbing during box packing | Matte surface burnishes or transfers ink onto adjacent components | Keep TAC ≤280%–300% and add anti-scuff matte varnish over dark exterior artwork |
Parent guide Booklet, Leaflet, and Reference Paper Stocks