Basis Weights, Caliper Bulk, and US Paper Classifications
Paper weight is measured globally in grams per square meter (gsm), while US mill specifications separate Text and Cover stocks by basis sheet size:
- US Text LB: Based on 500 sheets measuring 635 × 965 mm (25 × 38 in). An 80 to 120 gsm sheet corresponds to roughly 54 to 81 lb Text (24.5 to 36.7 kg per 500-sheet basis ream).
- US Cover LB: Based on 500 sheets measuring 508 × 660 mm (20 × 26 in). A 200 to 300 gsm sheet corresponds to roughly 74 to 111 lb Cover (33.6 to 50.3 kg per 500-sheet basis ream).
Because Text and Cover use different basis sheet areas, an 80 lb Cover stock (about 216 gsm) is nearly twice as heavy and rigid as an 80 lb Text stock (about 118 gsm). Always confirm both the gsm rating and the caliper (thickness) before locking a print specification, as uncoated stocks have higher bulk (greater thickness per gsm) than calendered coated stocks of the same weight.
Component Stock Specifications
| Component | Recommended Weight (gsm) | Approx. US Basis Weight | Approx. Caliper per Sheet | Surface & Sizing | Primary Grain Requirement |
|---|---|---|---|---|---|
| Booklet Interiors | 80–120 gsm | 54–81 lb Text | 0.08–0.13 mm (0.0031–0.0051 in) | Coated matte/silk for dense graphics; uncoated offset for text-heavy rules | Parallel to spine |
| Booklet Covers | 200–300 gsm | 74–111 lb Cover | 0.18–0.30 mm (0.0071–0.0118 in) | Coated matte/gloss; add anti-scuff matte film for dark artwork | Parallel to spine |
| Leaflets (4/6/8 Panels) | 100–150 gsm | 68–101 lb Text | 0.09–0.16 mm (0.0035–0.0063 in) | Coated matte/silk or smooth uncoated; scored at 130+ gsm | Parallel to primary fold |
| Scorepads | 70–100 gsm | 47–68 lb Text | 0.08–0.12 mm (0.0031–0.0047 in) | Uncoated, surface-sized offset paper for pen and pencil | Parallel to glued head |
| Reference Sheets | 250–350 gsm | 92–130 lb Cover | 0.24–0.38 mm (0.0094–0.0150 in) | Coated art stock with matte varnish or double-sided film | Parallel to longest edge (or fold) |
| Clue Envelopes | 120–170 gsm | 81–115 lb Text / 44–63 lb Cover | 0.13–0.20 mm (0.0051–0.0079 in) | Uncoated kraft, dyed, or tear-resistant offset stock | Parallel to longest fold |
Note: Adding double-sided lamination film to covers or reference sheets increases caliper by 0.03–0.05 mm (0.0012–0.0020 in) per sheet.
Substrate Performance and Fit Factors
Opacity and Show-Through
High-coverage illustrations, dark tables, or two-sided diagrams require sufficient opacity to prevent text and ink on the reverse side from showing through. Uncoated 80 gsm (~54 lb Text) sheets are prone to show-through under heavy ink; stepping up to 100–120 gsm (~68–81 lb Text) or switching to a coated matte stock increases opacity and keeps double-sided spreads legible.
Surface Coating and Writeability
- Coated Matte / Silk: Holds sharp halftone detail and deep color saturation for rulebooks, leaflets, and reference cards. Uncoated ballpoint pens and pencils skip or smear on coated or laminated surfaces.
- Uncoated Offset: Absorbs ink into the fibers, producing softer contrast than coated stock while accepting pencil, ballpoint, and gel ink cleanly. Scorepads and write-on reference sheets must remain uncoated and unvarnished.
- Anti-Scuff Matte Lamination: Recommended for 200–300 gsm dark-ink booklet covers and heavily handled standalone reference sheets to prevent finger-oil marking and edge rub inside the box.
Stack Height and Box Clearance
Paper caliper accumulates rapidly across multi-signature booklets and thick scorepads. Calculate the finished component thickness early so it fits within the box's 1.5–3 mm (0.059–0.118 in) stack-height clearance and 1.5–2.5 mm (0.059–0.098 in) width/height clearance:
Booklet Stack Height (mm) = (Interior Pages / 2) * Interior Caliper (mm) + Cover Caliper (mm) + Film Caliper (mm)
Scorepad Stack Height (mm) = Sheet Count * Sheet Caliper (mm) + Backing Board Caliper (mm)
Stack Height (in) = Stack Height (mm) / 25.4
For example, a 48-page booklet on 100 gsm uncoated stock at 0.11 mm (0.0043 in) per sheet plus a 250 gsm laminated cover (0.25 mm / 0.0098 in + 0.04 mm / 0.0016 in film) measures roughly 2.93 mm (0.115 in) before spine swell.
Regulatory and Material Documentation
Where paper components ship as part of children's games or enter regulated retail markets, inks, coatings, and packaging weights may require documented compliance. Record material data sheets and test evidence against applicable frameworks such as the EU Toy Safety Directive (EN 71) for chemical migration, Germany's VerpackG for packaging registration, and France's Triman Info-tri for sorting marks on paper and packaging components.
Production Steps and Prepress Setup
- Prepress File Preparation: Supply print-ready AI, PDF, or PSD files exported to PDF/X-1a or PDF/X-4 with all fonts outlined or embedded, images at ≥300 DPI in CMYK (with separate spot layers for special inks or varnishes), 3 mm (0.118 in) bleed on all trim edges, and ≥3 mm (0.118 in) safety margin inside the trim.
- Ink Density Control: Set fine body text to 100% K (black only) to prevent registration halos. Use rich black (
C40–60 M30–40 Y30–40 K100) only for large solid areas, keeping Total Area Coverage (TAC) at or below 280%–300% to avoid ink set-off on uncoated and matte stocks. - Grain and Imposition Planning: Align paper grain parallel to the spine for saddle-stitched (12–40 pages), perfect-bound (28+ pages), and sewn (80–100+ pages) booklets, and parallel to the main fold on 4-, 6-, or 8-panel leaflets and clue envelopes.
- Scoring, Folding, and Binding: Pre-score covers and leaflets at 130 gsm and above before folding. Pad scorepads with a rigid chipboard or greyboard backing sheet and PVA padding compound along the grain-aligned edge.
- Die-Cutting Envelopes: Die-cut clue envelopes from flat sheets, apply fold-flap scores, and glue seams with Remoistenable or peel-and-seal adhesive matched to the substrate's porosity.
Sign-Off Criteria
- Opacity: Zero distracting show-through of heavy headlines or dark graphics on the reverse side of interior pages under normal reading light.
- Fold Integrity: Clean, uncracked ink along scored spines and leaflet folds when folded 180 degrees.
- Flatness: Booklets and reference sheets lie flat without spine spring-back or moisture curl.
- Writeability: Scorepad sheets accept standard #2 pencil and ballpoint ink without skipping or smearing.
- Fit: Finished booklet or pad stack height falls within the assigned box interior clearance.
Concrete Failure Modes
- Cross-Grain Cracking and Spring-Back: Running paper grain perpendicular to a booklet spine, leaflet fold, or envelope crease causes fibers to fracture along the fold line, cracking dark ink and forcing pages to spring open. Always lock grain direction parallel to the primary fold or spine.
- Show-Through on Thin Interiors: Printing dense ink maps or dark tables on 80 gsm uncoated paper lets reverse-side artwork bleed visually through the sheet. Increase stock weight to 100–120 gsm or specify coated matte paper.
- Scuffing and Rub-Off on Dark Covers: Unprotected dark CMYK or rich black solids on 200–300 gsm matte-coated covers show white abrasion marks during collation and shipping. Apply anti-scuff matte lamination or a protective matte aqueous coating.
- Smearing on Coated Scorepads: Using coated silk or matte art paper for scorepads prevents pencil graphite and ballpoint ink from biting into the sheet. Specify uncoated, surface-sized offset paper for any write-on component.
- Box Fit Failure from Caliper Swell: Calculating box depth using nominal paper weight instead of actual caliper—or omitting the 0.03–0.05 mm (0.0012–0.0020 in) thickness of double-sided cover film and saddle-stitch spine swell—pushes the total stack height past the 1.5–3 mm (0.059–0.118 in) box clearance, bowing the lid or crushing component corners.
Guides in this section
- Coated Booklet Cover Stock
- Clue and Dossier Envelope Paper Stock
- Gloss Coated Interior Paper Stock
- Matte and Silk Coated Interior Paper Stock
- Paper Grain Direction for Booklets and Foldouts
- Standalone Quick-Reference Sheet Stock
- Tear-Off Scorepad Paper Stock
- Self-Cover Booklet Stock
- Uncoated and Textured Cover Stock
- Uncoated Offset Interior Paper Stock
Parent guide Rulebook, Booklet, and Printed Reference Specifications