Move to a lighter weight (80 to 90 gsm) when binding 80–100+ page sewn books, 28+ page perfect-bound books, or 6- and 8-panel leaflets that need tight stack height and flat folds. Step up to 105–128 gsm for 12–40 page saddle-stitched rulebooks and 4-panel leaflets that require firmer page turn and lower show-through behind dense diagrams. For text-only interiors without fine graphics, or for layouts requiring maximum gloss saturation, compare options in the booklet paper stocks overview.
Specifications and Basis Weight Reference
Interior paper stocks run 80–120 gsm (extending to 128 gsm for heavier matte/silk rulebook sheets), while booklet covers run 200–300 gsm.
| Property | Matte & Silk Coated Interior Baseline | Notes & Boundaries |
|---|---|---|
| Grammage range | 90–128 gsm (general interior band: 80–120 gsm) | 80–90 gsm for high page counts; 105–128 gsm for lower page counts |
| US basis weight equivalent | ~54–86 lb Text | Measured on a 25 x 38 in (635 x 965 mm) Text basis sheet; distinct from Cover LB, which uses a 20 x 26 in (508 x 660 mm) basis sheet for 200–300 gsm covers |
| Sheet caliper | ~0.08–0.13 mm (0.0031–0.0051 in) per sheet | Less aggressively calendered than gloss coated, preserving slightly higher bulk |
| Bleed & safety | 3 mm (0.118 in) bleed per side; >=3 mm (0.118 in) safety | Bound signatures require multiples of 4 pages |
| Binding compatibility | Leaflets: 4/6/8 panels; Saddle stitch: 12–40 pages; Perfect: 28+ pages; Sewn: 80–100+ pages | Higher caliper pushes 36–40 page saddle-stitched books toward perfect or sewn binding |
| Prepress & ink limits | CMYK + separate spot layers; >=300 DPI; PDF/X-1a or PDF/X-4 | 100% K fine text; rich black C40–60 M30–40 Y30–40 K100; TAC <=280%–300% |
Estimate finished booklet thickness before locking box cavity depth:
Booklet Stack Height (mm) = (Interior Page Count / 2) * Interior Sheet Caliper (mm) + 2 * Cover Caliper (mm)
Keep finished booklet dimensions inside the box with 1.5–2.5 mm (0.059–0.098 in) clearance across width and height, and 1.5–3 mm (0.059–0.118 in) clearance across total stack height.
Coating Behavior and Mechanical Limits
- Ink holdout: The mineral-coated surface keeps ink pigment on top of the paper fibers rather than letting it wick into the sheet. Fine 100% K diagram lines, small callout labels, and screen-tint gradients stay sharp without feathering.
- Low-glare reading performance: Matte and silk surfaces diffuse overhead room lighting instead of producing specular reflections across the page. Silk carries a subtle sheen that raises dark-ink contrast slightly above dead-matte while keeping rules text legible from angled seating positions.
- Scuff sensitivity: Because the coating is micro-textured rather than mirror-smooth, unsealed matte and silk ink layers are vulnerable to rub-off, burnishing, and edge scuffing when pages slide across each other or rub against cards in a box. Dead-matte scuffs more readily than silk; dark full-bleed spreads require an inline aqueous coating or matte varnish to seal the ink.
- Folding limits: Grain direction must run parallel to the spine or primary fold. Unscored sheets above 105–115 gsm crack along the coated surface when folded across heavy ink coverage. Multi-panel leaflets (6 or 8 panels) and thick sewn signatures fold flatter and resist spring-back when kept at 80–105 gsm.
Production Steps and Sign-Off Criteria
- Prepress preparation: Export AI, PDF, or PSD artwork as PDF/X-1a or PDF/X-4 with outlined or embedded fonts, >=300 DPI images, 3 mm (0.118 in) bleed per side, and >=3 mm (0.118 in) safety margin. Set fine rules text to 100% K, large dark fills to rich black (C40–60 M30–40 Y30–40 K100), and keep Total Area Coverage (TAC) at <=280%–300%.
- Stock and grain matching: Select 90–105 gsm for 6/8-panel leaflets, 28+ page perfect binding, or 80–100+ page sewn binding; select 105–128 gsm for 4-panel leaflets or 12–40 page saddle-stitched booklets. Orient paper grain parallel to the spine or primary fold.
- Printing and surface sealing: Print offset CMYK (plus separate spot layers if specified) with controlled ink density. Allow sufficient drying time in the delivery pile or apply inline aqueous varnish so unabsorbed ink does not transfer onto the back of the next sheet.
- Scoring, folding, and binding: Score fold lines on 115–128 gsm sheets and on any ink-heavy spine before folding. Collate signatures in multiples of four, apply creep compensation on thicker saddle-stitched runs, and trim to final size.
Sign-Off Criteria
- Fine 100% K text and diagram callouts render cleanly with no dot spread or haloing.
- Coated surface reads evenly under overhead light without glossy patches or blotchy drying.
- Spine and leaflet folds show zero white coating crack or fiber splitting.
- Dark ink areas resist rub-off and burnishing under normal page handling.
- Finished booklet width, height, and stack height preserve the planned box clearances.
Concrete Failure Modes
- Coating crack on the fold: Occurs when paper grain runs perpendicular to the fold, or when 115–128 gsm stock is folded across heavy ink without scoring. Prevent by aligning grain parallel to the spine, scoring prior to folding, or stepping down to 90–105 gsm.
- Ink scuffing and burnishing: Occurs on dark, unsealed matte spreads when sheets rub during collating, trimming, or repeated tabletop use. Prevent by keeping TAC <=280%–300%, applying an inline aqueous or matte varnish, or switching from dead-matte to silk.
- Set-off in the press pile: Occurs because coated matte and silk surfaces absorb ink vehicle more slowly than uncoated paper, transferring wet rich black onto adjacent sheets. Prevent by respecting TAC <=280%–300%, sealing inline, and allowing full drying before guillotine trimming.
- Show-through on two-sided diagrams: Occurs when 80–90 gsm stock carries heavy dark graphics on one side and light text or tables on the reverse. Prevent by stepping up to 105–128 gsm or balancing ink density across opposing pages.
- Saddle-stitch spring-back and margin creep: Occurs when pairing upper-end caliper (0.12–0.13 mm / 0.0047–0.0051 in) with 36–40 page saddle-stitched signatures, forcing the booklet open and pushing outer page content toward the trim. Prevent by dropping to 90–105 gsm, applying prepress creep compensation, or switching to 28+ page perfect binding or 80–100+ page sewn binding.
Parent guide Booklet, Leaflet, and Reference Paper Stocks