Specifications & Material Behavior
Gloss coated paper (C2S gloss art) uses a clay-and-polymer surface coating smoothed through steel calendering rollers. Because the rollers compress the sheet and seal the fiber pores, ink sits on top of the coating rather than soaking into the paper fibers.
- Weight range and US basis equivalents: Standard interior booklet stocks run 80–120 gsm (about 54–81 lb Text), with gloss coated options commonly specified from 90 to 128 gsm (about 61–86 lb Text). Always distinguish US Text LB—measured on a 25 × 38 in (635 × 965 mm) basis sheet—from US Cover LB, which uses a smaller 20 × 26 in (508 × 660 mm) basis sheet. A 200–300 gsm booklet cover equals roughly 74–111 lb Cover, whereas a 120 gsm interior sheet is 81 lb Text, not 80 lb Cover.
- Caliper efficiency and box fit: Interior stocks typically measure 0.08–0.13 mm (0.0031–0.0051 in) per sheet. Calendered gloss coated stock delivers the thinnest caliper per gram in that range, keeping booklet bulk low when total box stack height must preserve 1.5–3 mm (0.059–0.118 in) of clearance.
- Mass impact: A higher-density coated sheet weighs more per unit of thickness than an uncoated sheet of equal caliper. When packing bulk print runs, keep individual carton weights manageable—typically under 15–20 kg (33–44 lb) per carton—to avoid crushed booklet corners during transit.
- Binding and signature rules: Bound signatures must be imposed in multiples of 4 pages. Saddle stitching fits 12–40 pages; perfect binding applies at 28+ pages; sewn binding is recommended at 80–100+ pages.
- Prepress and ink limits: Supply print-ready AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 with outlined or embedded fonts. Set images to CMYK (with separate spot layers where needed) at ≥300 DPI, 3 mm (0.118 in) bleed per side, and ≥3 mm (0.118 in) safety margin. Keep fine body text at 100% K, use rich black at C40–60 M30–40 Y30–40 K100, and cap Total Area Coverage (TAC) at ≤280%–300%.
Use this plain-text formula to check whether a booklet's thickness fits inside a game box alongside cards and boards:
Booklet thickness (mm) = (Interior pages / 2) * Interior sheet caliper (mm) + 2 * Cover caliper (mm)
Production Steps
- Prepress and ink-density audit: Verify that rich-black panels and full-bleed illustrations stay at or below 280%–300% TAC. Because gloss coatings do not absorb excess vehicle quickly, over-inked spreads remain wet on press.
- Grain alignment and imposition: Impose signatures in multiples of 4 pages with the paper grain running parallel to the spine. Parallel grain reduces resistance along the fold line and keeps pages from springing open.
- Offset printing and curing: Print sheets via offset lithography with controlled ink-water balance and anti-set-off spray powder or inline IR/UV drying. Allow sufficient stack cure time before moving sheets to the folder so wet ink does not transfer onto the back of the next sheet.
- Folding, binding, and three-knife trim: Fold signatures cleanly, score heavier 115–128 gsm folds if heavy ink crosses the gutter, collate with the 200–300 gsm cover, bind according to page count, and trim the three open edges to remove the 3 mm (0.118 in) bleed.
Sign-Off Criteria
- Surface cleanliness: Zero ink set-off, scuffing, or roller marks on facing white or light-tinted pages after stacking.
- Fold integrity: Clean spine creases with no white fiber cracking along the outer or inner fold, particularly across dark artwork.
- Pagination and squareness: Exact multiple-of-4 page count, consistent gutter alignment, and ≥3 mm (0.118 in) safety clearance from the trimmed edge on all live text and page numbers.
- Box and stack fit: Finished booklet caliper plus deck and component heights maintain 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) stack clearance inside the box.
Failure Modes
- Overhead lighting glare: Specular reflection off the smoothed clay coating creates bright hotspots under tabletop lamps, causing eye fatigue on dense, small-font rule pages.
- Spine-fold cracking: At 115–128 gsm—especially if the paper grain runs perpendicular to the spine or heavy TAC crosses the fold—the brittle surface coating fractures along the crease, exposing white base fibers.
- Ink set-off and smudging: Exceeding 280%–300% TAC or rushing folded signatures into binding before surface ink oxidizes transfers wet ink onto adjacent pages.
- Saddle-stitch spring and creep: Running close to 40 pages at the upper end of the 90–128 gsm range increases spine bulk, causing outer pages to creep inward and the booklet to resist lying flat without heavier clamping or a switch to perfect binding (28+ pages).
Parent guide Booklet, Leaflet, and Reference Paper Stocks