- Open aperture with inner wrap turn-ins: Best when the window must stay open for tactile access or plastic-free packaging, provided the cutout has straight edges or generous radiused corners that allow notched wrap flaps to fold smoothly into the wall.
- Laminated clear plastic window with interior liner: Required when contents must stay sealed inside the shell, when small or complex cutouts cannot accommodate neat turn-ins, or when raw greyboard edges must be hidden behind a smooth interior face.
In both structures, the window sits inside a wrapped rigid greyboard box frame whose remaining border width and board thickness govern whether the wall stays flat under wrapping tension.
Specifications and Tolerances
| Parameter | Specification | Production Condition |
|---|---|---|
| Core greyboard thickness | 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in) | Thicker board increases frame stiffness around large cutouts but consumes more wrap length on inner turn-ins |
| Outer wrap margin | 15–20 mm (0.591–0.787 in) | Standard perimeter turn-in; inner-aperture flaps require enough depth to wrap the board thickness and bond flat inside |
| Interior box clearance | 1.5–2.5 mm (0.059–0.098 in) width/height; 1.5–3 mm (0.059–0.118 in) stack height | Prevents cards, trays, or inserts from catching on the interior liner or window film edge |
| Aperture corner radius | R3–R3.5 mm (0.118–0.138 in) minimum recommended | Reduces fiber cracking on wrap turn-ins and prevents stress tears in the greyboard frame |
| Wrap and liner stock | Specified in gsm; interior stocks typically 80–120 gsm (about 0.08–0.13 mm / 0.003–0.005 in per sheet) | Distinguish US Text LB (25 × 38 in basis sheet) from US Cover LB (20 × 26 in basis sheet) when matching US paper grades |
| Prepress and artwork | AI, PDF, or PSD (PDF/X-1a or PDF/X-4); CMYK + separate spot layers; ≥300 DPI | 3 mm (0.118 in) bleed per side into the cutout; ≥3 mm (0.118 in) safety from the cut edge |
| Black ink and surface finish | Outlined or embedded fonts; 100% K fine text; rich black C40–60 M30–40 Y30–40 K100; TAC ≤280%–300% | Anti-scuff matte lamination suits dark artwork around high-handling window borders |
Production Steps
- Die-cut the greyboard core and V-grooves: Cut the viewing aperture out of the 1.5–3 mm (0.059–0.118 in) greyboard blank and score or V-groove the wall folds before wrapping so the window opening is registered to the finished box face.
- Print, laminate, and slit the outer wrap: Print the wrap with 3 mm (0.118 in) bleed extending into the aperture, apply surface film (such as anti-scuff matte), and die-cut or star-slit the wrap inside the window area to form turn-in flaps or a flush opening.
- Mount the wrap and turn in the aperture: Adhere the outer wrap to the greyboard face, then fold and press the notched inner-aperture flaps through the board thickness onto the back face of the greyboard.
- Bond the clear plastic window sheet (if sealed): Apply a controlled perimeter bead of adhesive on the back face of the greyboard around the cutout and lay the clear plastic sheet flat over the opening, leaving enough overlap margin to prevent edge lift.
- Laminate the interior liner and form the shell: Adhere the interior paper liner across the inside of the greyboard, trapping the perimeter of the clear plastic sheet between the core board and the liner. Fold the walls and seal the exterior corners while preserving 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) stack clearance.
Sign-Off Criteria
- Cutout registration: Printed artwork around the window remains within the ≥3 mm (0.118 in) safety margin, with no unprinted white paper edge or exposed greyboard visible along the aperture wall.
- Turn-in adhesion: Inner-aperture wrap flaps lie completely flat against the interior greyboard face with no bubbling, lifting corners, or split fibers at the cutout corners.
- Window clarity and trapping: The clear plastic sheet is free of waves, scuffs, and adhesive squeeze-out, and its edges are fully trapped between the greyboard core and the interior liner.
- Frame flatness and fit: The greyboard border around the window remains flat without bowing, and the assembled shell clears the internal contents by 1.5–2.5 mm (0.059–0.098 in) on width/height and 1.5–3 mm (0.059–0.118 in) on stack height.
- Regulatory records (conditional): Combining a clear plastic window with a paperboard shell can affect material-separation and packaging-reporting obligations in target markets, such as Germany's VerpackG registration or France's Triman sorting instructions. Products intended for children also require EN 71 assessment and testing records before release.
Failure Modes
- Cracked wrap at inner window corners: Sharp 90-degree cutouts combined with thicker greyboard (2.5–3 mm / 0.098–0.118 in) or stiff lamination film over-stretch the outer wrap during turn-in. Increasing the corner radius to R3–R3.5 mm (0.118–0.138 in) and adjusting flap notching prevents tearing.
- Exposed raw greyboard on the window wall: Insufficient bleed (below 3 mm / 0.118 in) or registration drift between the die-cut wrap and the greyboard aperture leaves an uncolored grey edge visible from the front.
- Adhesive squeeze-out into the viewing area: Applying glue too close to the aperture perimeter causes adhesive to bleed onto the clear plastic window when the interior liner is pressed down.
- Window film buckling or tenting: Laminating the clear plastic sheet before wrap and board adhesives have stabilized causes moisture-driven board movement that pulls the plastic film into ripples.
- Warped or collapsed frame border: Placing an oversized window too close to a V-groove or box corner leaves a narrow greyboard bridge that bows under wrap tension or crushes during handling.
Parent guide Wrapped Rigid Shell Construction