Conditions that change the choice:

  • Sharp 90-degree edge geometry: When display presentation or tight geometric alignment requires crisp, square outer corners instead of a slight fold radius, V-grooving replaces crush scoring.
  • Heavy board calipers: At 2.5 mm (0.098 in) and 3 mm (0.118 in) greyboard thicknesses, bending along a crush score places high tensile stress on the outer fibers and creates a wider corner radius; thicker boards often shift the build toward V-grooving to prevent outer-liner cracking or corner flare.

Structural Specifications

Parameter Specification Notes
Greyboard caliper 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), 3 mm (0.118 in) Thinner calipers (1.5–2 mm / 0.059–0.079 in) fold with tighter radii and lower outer-fiber stress
Wrap margin (turn-in) 15–20 mm (0.591–0.787 in) Folded over the top rim onto the interior wall to lock the wrap and cover raw board edges
Width and height clearance 1.5–2.5 mm (0.059–0.098 in) Internal cavity allowance around decks, inserts, or inner trays
Stack height clearance 1.5–3 mm (0.059–0.118 in) Vertical allowance above stacked contents
Wrap bleed (if printed) 3 mm (0.118 in) per side CMYK with separate spot layers, ≥300 DPI, PDF/X-1a or PDF/X-4, TAC ≤280%–300%

Unit conversion: in = mm / 25.4.

Production Steps

  1. Die-cutting and crush-scoring: A steel-rule die cuts the outer cruciform blank (base panel plus four side flaps) while blunt creasing rules compress the fold lines from the interior face. Unlike V-grooving, no board material is removed along the hinge.
  2. Flap folding: The four side flaps bend 90 degrees upward along the compressed score channels. Because the exterior greyboard fibers stretch around the uncompressed outer arc rather than meeting at a mitered cut, the finished corners carry a slight natural radius.
  3. Heat-activated corner-stay taping: A corner-staying machine applies heat-activated adhesive tape across each of the four vertical corner seams. Controlled platen heat and pressure melt the adhesive into the raw greyboard edges, locking the shell square before wrapping.
  4. Wrapping and turn-in: The glued wrap sheet is mounted onto the exterior of the taped shell. The 15–20 mm (0.591–0.787 in) wrap margin turns over the top rim and presses flat against the inner walls, concealing the corner-stay tape and raw board.

Sign-Off Criteria

  • Seam integrity: All four corner-stay tape strips adhere flat across the vertical joints with no edge lifting, bubbling, or seam separation under lateral finger pressure.
  • Outer corner uniformity: Folded edges show consistent, slightly rounded profiles without split greyboard fibers, ridging, or wrap tenting.
  • Cavity fit: Internal dimensions maintain 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) stack height clearance so decks, inserts, and lids seat smoothly without binding.
  • Turn-in adhesion: The 15–20 mm (0.591–0.787 in) wrap margin bonds flush to the interior wall with clean corner pleats and no exposed greyboard along the rim.

Concrete Failure Modes

  • Outer-liner cracking or fiber burst: Excessive score compression or folding 2.5–3 mm (0.098–0.118 in) greyboard over too narrow a crease channel over-stresses the outer surface, producing visible splits or rough ridges beneath the wrap.
  • Corner-stay tape pop: Insufficient heat, dwell time, or clamping pressure during taping leaves the adhesive partially unbonded. Residual spring-back in the folded flaps pushes the vertical seams apart, creating soft or gapped corners.
  • Wrap tenting at corners: Unevenly applied stay tape or inconsistent fold radii prevent the glued wrap from conforming to the corner arc, leaving hollow air bridges that crease or puncture during handling.
  • Inward score bulge reducing cavity clearance: Crush scoring displaces compressed greyboard fibers inward along the base perimeter. When die layouts omit compensation for inward bead displacement and board thickness, internal clearance drops below 1.5–2.5 mm (0.059–0.098 in) and traps inserts or card stacks.