Use V-grooved shells when a rigid box requires sharp, architectural 90-degree edges on thicker greyboard—1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in)—where standard scoring would leave rounded corners or excessive wall spring-back. When softer edges are acceptable or board caliper is thinner, alternative constructions within wrapped rigid boxes may be used instead.

Specifications and Cut-Depth Limits

Parameter Specification
Greyboard thickness 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in)
Groove profile 90-degree V-channel milled partway through the interior face
Backing web Continuous, uncut outer layer of greyboard fibers supporting the fold
Wrap turn-in margin 15–20 mm (0.591–0.787 in)
Interior box clearance 1.5–2.5 mm (0.059–0.098 in) width/height; 1.5–3 mm (0.059–0.118 in) stack height
Wrap prepress CMYK with separate spot layers, ≥300 DPI, 3 mm (0.118 in) bleed per side, ≥3 mm (0.118 in) safety
Wrap finish Anti-scuff matte lamination recommended for dark artwork crossing corners

How Cut Depth Controls Corner Quality and Wrap Integrity

V-grooving removes a 90-degree wedge of greyboard along each fold line so the two 45-degree beveled walls meet flush when folded upright. Stopping the cut just short of the outer surface is the critical tolerance:

  • Controlled partial cut (target): Leaving a thin, intact backing web creates a flexible hinge along the outer face. When the walls fold to 90 degrees, the web distributes tension evenly and gives the exterior paper wrap a continuous surface to bridge.
  • Cut too deep (severed web): Milling completely through the greyboard eliminates the backing web. With no board fibers bridging the corner, the walls can shift independently and all folding stress concentrates directly on the wrap paper and adhesive, causing the wrap to crack, split, or show a sharp ridge.
  • Cut too shallow: Leaving too much uncut greyboard at the base of the groove forces the outer fibers to compress and bulge during folding, producing rounded edges, wall spring-back, and uneven miter seams.

Production Steps

  1. Flat blank cutting: Cut the 1.5–3 mm (0.059–0.118 in) greyboard sheets to the flat shell dimensions, accounting for board wall thickness plus the 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) stack-height interior clearances.
  2. 90-degree V-grooving: Mill the 90-degree V-channels along all wall fold lines on the inner face of the greyboard, maintaining uniform depth so the outer backing web remains intact across every fold.
  3. Shell folding and squaring: Fold the grooved walls upward until the beveled edges meet flush at 90 degrees, and secure the corners before wrapping so the shell holds its square geometry.
  4. Wrap printing and finishing: Print the exterior wrap (CMYK with separate spot layers, ≥300 DPI, 3 mm / 0.118 in bleed per side, ≥3 mm / 0.118 in safety), apply surface protection such as anti-scuff matte lamination for dark solids, and trim with a 15–20 mm (0.591–0.787 in) turn-in margin.
  5. Wrapping and turn-in: Apply adhesive and wrap the exterior sheet tightly around the squared shell, pressing the wrap smoothly over each intact corner web and folding the 15–20 mm (0.591–0.787 in) margin neatly onto the interior walls.

Sign-Off Criteria

  • Corner geometry: Walls meet at crisp 90-degree angles with flush interior miter seams and no outward bow or spring-back.
  • Wrap and web continuity: Exterior corners are smooth and unbroken, with no split board fibers, telegraphing ridges, or cracked ink/lamination along the fold.
  • Turn-in adhesion: The 15–20 mm (0.591–0.787 in) wrap margin sits flat against the inside walls with no lifting, bubbling, or exposed greyboard at the corners.
  • Internal fit: Assembled shell maintains the 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) stack-height clearances so contents slide in and out smoothly.

Failure Modes

Failure Mode Physical Cause Prevention / Correction
Wrap cracking along corners Groove milled all the way through the greyboard, severing the backing web and leaving the wrap unsupported; or dark solid ink folding without protective lamination Maintain an intact outer backing web at the base of the 90-degree V-groove; use anti-scuff matte lamination on dark artwork
Rounded corners or wall spring-back Groove milled too shallow, leaving excessive uncut board thickness at the fold Increase V-groove cut depth closer to the outer face while preserving a thin, unbroken backing web
Corner ridge or uneven seam Inconsistent groove depth across the blank or misaligned mitered walls during corner squaring Verify uniform milling depth across the sheet and square the folded shell fully before wrapping
Interior wrap lifting Turn-in margin narrower than 15–20 mm (0.591–0.787 in) or insufficient pressing during wrap application Keep the full 15–20 mm (0.591–0.787 in) wrap margin and press turn-ins firmly into the interior corners
Tight or binding box fit Greyboard wall thickness and wrap buildup encroaching on interior cavity dimensions Size the flat blank so finished internal dimensions retain 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) stack-height clearance