Two physical conditions shift where a job sits within these ranges:

  • Grayboard caliper: Thicker cores (2.5 mm / 0.098 in or 3 mm / 0.118 in) consume more of the wrap sheet across the edge wall than 1.5 mm (0.059 in) or 2 mm (0.079 in) boards, so thicker boards require the upper end of the 15 to 20 mm (0.59 to 0.79 in) turn-in to preserve enough glued flap area on the back face.
  • Wrap stiffness and lamination: Film lamination—such as anti-scuff matte film used over dark artwork—increases fold resistance and spring-back along the 90-degree edge wall, requiring full turn-in width and crisp corner miters to stay flat.

For overall board sizing, folding clearances, and core thickness options, see game board tolerances.

Specifications and Allowances

Parameter Specification Physical Purpose
Wrap turn-in width 15–20 mm (0.59–0.79 in) per side Provides enough glued flap on the back face to resist spring-back
Grayboard caliper 1.5 / 2 / 2.5 / 3 mm (0.059 / 0.079 / 0.098 / 0.118 in) Sets edge-wall wrap consumption and corner tab length
Corner miter cut Angled corner trim matched to board caliper Removes excess flap overlap while leaving enough tab to cover the corner core
Back-liner inset 1.5–2.5 mm (0.059–0.098 in) from outer edge Seals over the raw inner edge of the wrap turn-in without overhanging the board perimeter
Artwork safety zone ≥3 mm (0.118 in); ≥4–5 mm (0.16–0.20 in) for bordered layouts Prevents borders or key graphics from wrapping unevenly onto the edge wall

Use the following plain-text formula to calculate the flat wrap sheet size before mitering:

Wrap sheet dimension = Board face dimension + (2 * Grayboard caliper) + (2 * Turn-in width)

Prepress and Material Notes

  • File setup: Supply print-ready PDF/X-1a or PDF/X-4 files (from AI/PDF/PSD) at ≥300 DPI in CMYK (with separate spot layers where applicable), with fonts outlined or embedded. Use 100% K for fine text, rich black (C40–60 M30–40 Y30–40 K100) for solid dark areas, and keep total area coverage (TAC) at ≤280%–300%.
  • Paper weight notation: Specify wrap and back-liner stocks in gsm; when referencing North American basis weights, distinguish US Text LB (25 × 38 in basis sheet) from Cover LB (20 × 26 in basis sheet) so sheet stiffness is unambiguous.

Production Steps

  1. Extend artwork across the wrap zone: Build the wrap sheet to the full calculated dimension (face + 2 * caliper + 2 * turn-in), bleeding background color or artwork through the edge wall and onto the 15–20 mm (0.59–0.79 in) turn-in so no unprinted paper shows along the board edge.
  2. Miter the four corners: Die-cut or trim each corner of the wrap sheet at an angle, leaving a small corner tab sized to the grayboard caliper (1.5–3 mm / 0.059–0.118 in) so the corner core is covered without overlapping two full layers of wrap paper on the back.
  3. Mount the wrap to the board face: Apply adhesive evenly across the wrap sheet, register the grayboard core onto the face, and press from the center outward to expel trapped air.
  4. Fold turn-ins and tuck corners: Fold one pair of opposite turn-ins tight against the edge wall onto the back face, tuck the mitered corner tabs neatly against the board thickness, and then fold the remaining two sides.
  5. Apply the back liner: Center and laminate the back liner onto the back face with a 1.5–2.5 mm (0.059–0.098 in) inset from all four outer edges, bridging and sealing the inner cut edge of the wrap turn-in.

Sign-Off Criteria

  • All four wrap turn-ins measure 15–20 mm (0.59–0.79 in) on the back face and bond flat with no lifting along the edge wall.
  • Corners sit square and flush, with no exposed grayboard core and no double-layer paper ridges under the back liner.
  • The back liner maintains a uniform 1.5–2.5 mm (0.059–0.098 in) inset on all four sides and never protrudes past the board edge.
  • Face artwork stays centered, with borders clear of the edge wall by ≥4–5 mm (0.16–0.20 in) and non-bordered elements clear by ≥3 mm (0.118 in).

Failure Modes

  • Edge peeling and turn-in lift: Turn-in widths below 15 mm (0.59 in)—especially on 2.5 mm (0.098 in) or 3 mm (0.118 in) grayboard or stiff laminated wraps—lack sufficient glue contact area and peel away from the back face.
  • Bulky or dog-eared corners: Shallow or omitted corner miters trap two overlapping wrap flaps on the back face, creating raised corner bumps that telegraph through the back liner.
  • Exposed grayboard at corners: Over-mitering cuts away too much corner tab material, leaving raw grayboard visible at the board tips once the flaps are folded.
  • Back-liner overhang or edge catching: A back-liner inset smaller than 1.5 mm (0.059 in) leaves no margin for registration tolerance, allowing the liner edge to overhang the board perimeter and fray during handling.
  • Border drift onto the edge wall: Borders placed closer than 4–5 mm (0.16–0.20 in) to the face trim line shift visibly onto the board's edge wall under normal mounting tolerances.