For broader board-level dimensional rules and shared caliper references, see the game board tolerances overview.

Core Specifications and Stack Build-Up

Parameter Standard Specification Tolerance Drivers and Physical Impact
Greyboard core caliper 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), 3 mm (0.118 in) Sets panel rigidity and base folded stack height per panel
Wrap turn-in margin 15–20 mm (0.591–0.787 in) per edge Overlaps board edges; adds double wrap thickness along the perimeter
Lamination film allowance 0.03–0.05 mm (0.001–0.002 in) for double-sided film Compounds across 3 to 4 folded panels
Box width/height clearance 1.5–2.5 mm (0.059–0.098 in) Prevents side-wall binding when inserting the folded screen
Box stack height clearance 1.5–3 mm (0.059–0.118 in) Absorbs hinge crown, pocket layers, and film build-up
Prepress bleed and safety 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) safety Prevents wrap-edge color shift or clipped borders along bottom edges

Folded Stack Thickness Formula

Calculate total folded thickness before sizing outer rigid boxes or slipcases:

Folded Stack Thickness = (Panel Count × Greyboard Caliper)
                       + (Panel Count × Wrap and Liner Thickness)
                       + (Panel Count × Film Thickness)
                       + Pocket or Sleeve Build-Up
                       + Hinge Crown Allowance
  • Wrap and liner contribution: Printed wrap sheets (such as 80–120 gsm text-weight paper, about 0.08–0.13 mm / 0.003–0.005 in per sheet; US Text LB is measured on a 25 × 38 in / 635 × 965 mm basis sheet, whereas Cover LB uses 20 × 26 in / 508 × 660 mm) add thickness on both the outer face and inner liner, plus an extra layer where the 15–20 mm (0.591–0.787 in) turn-in overlaps at the perimeter.
  • Pocket and sleeve build-up: Clear vinyl or paper pockets glued to the interior panels add material thickness on every panel that carries them and push the hinge gap wider so the screen still closes flat.
  • Box sizing: Add 1.5–2.5 mm (0.059–0.098 in) to the folded screen's width and height and 1.5–3 mm (0.059–0.118 in) to the measured folded stack thickness (not the bare greyboard sum) when specifying box cavities.

Bottom-Edge Coplanarity and Panel Squareness

Coplanarity means the bottom edges of all panels sit in the same horizontal plane when the screen is opened to its standing angle.

  • Board squareness: Each greyboard panel is cut with 90-degree corners so opposite edges are parallel and the two diagonals of each panel match. Out-of-square panels tilt the hinge axis, lifting adjacent bottom corners off the table.
  • Hinge gutter alignment: The cloth, paper, or wrap hinge bridging two boards must keep both bottom edges flush along a straight reference bar during casing-in. Even a small vertical offset at the hinge compounds across a 3-panel or 4-panel span.
  • Grain direction: Align greyboard and wrap paper grain vertically (parallel to the hinges) on standing screens so seasonal humidity changes do not curl the bottom edge into a rocker curve.

Job-Specific Production Steps

  1. Board cutting: Guillotine or die-cut all greyboard panels from the same caliper batch (1.5, 2, 2.5, or 3 mm / 0.059, 0.079, 0.098, or 0.118 in) to lock height uniformity across the set.
  2. Prepress and lamination: Prepare wrap artwork in CMYK with separate spot layers at ≥300 DPI, 3 mm (0.118 in) bleed per side, and ≥3 mm (0.118 in) safety, using PDF/X-1a or PDF/X-4 with outlined or embedded fonts, 100% K for fine text, rich black (C40–60 M30–40 Y30–40 K100), and TAC ≤280%–300%. Apply anti-scuff matte lamination on dark artwork to resist rubbing along folded edges.
  3. Jigged casing-in: Position panels against a bottom straightedge jig with calibrated hinge gaps sized to at least twice the board caliper plus wrap and pocket thickness, then wrap the 15–20 mm (0.591–0.787 in) turn-ins cleanly around corners.
  4. Inner lining and pocket mounting: Mount the inner liner sheet and any interior pockets, keeping adhesive coverage even to balance moisture pull on both faces of the greyboard.
  5. Pressing and folding: Press flat under controlled weight until adhesive cures, then score and pre-fold hinges to verify flat closure without spring-back.

Sign-Off Criteria

  • Flat-surface standing check: Open the finished screen to a natural 90-to-120-degree standing angle on a verified flat surface; all bottom corners and panel edges contact the table without rocking when tapped lightly at the top corners.
  • Panel squareness check: Measure both diagonals on each individual panel and verify parallel hinge seams when folded; panels stack flush at the top, bottom, and fore-edge without stepped overhang.
  • Folded stack and box-fit check: Measure the closed screen at the center and near the spine/hinges under light hand pressure; confirm the total folded stack fits the packaging cavity with 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) stack height clearance.

Concrete Failure Modes

  • Rocking or seesawing panels: Caused by mismatched panel heights, out-of-square board cuts, or vertical drift during casing-in; the screen pivots on one high corner when opened.
  • Hinge binding and spring-back: Caused by hinge gaps set too narrow for the chosen greyboard caliper (for example, 2.5 mm / 0.098 in or 3 mm / 0.118 in board) plus double-sided film (0.03–0.05 mm / 0.001–0.002 in) and interior pockets; the folded stack wedges open like a fan and cracks the wrap paper along the spine.
  • Warp-induced bottom lift: Caused by cross-grain greyboard or unbalanced moisture between outer wrap and inner liner; the center of the panel bows away from the table even when corners touch.
  • Box-lid crush or tight insertion: Caused by sizing the outer box from bare greyboard thickness (Panel Count × Greyboard Caliper) without adding wrap overlap, film, pocket layers, and hinge crown, leaving less than the 1.5–3 mm (0.059–0.118 in) stack clearance.