This specification governs individual pocket openings within a multi-layer board; for how pocket depth, layer-to-layer registration shift, and overall board flatness interact across the full assembly, see Recess Cutout and Layer Registration.
Clearance Specifications by Component Type
Different component manufacturing methods produce different dimensional tolerances and edge profiles. Set per-side clearance based on the physical behavior of the seated piece:
| Component Type | Clearance per Side | Total Oversize (W & L) | Primary Sizing Drivers |
|---|---|---|---|
| Wooden cubes & blocks | 0.8 to 1.5 mm (0.031 to 0.059 in) | 1.6 to 3.0 mm (0.063 to 0.118 in) | Wood grain swelling, tumbling/sanding variance, and painted or lacquered coating buildup |
| Cardboard tiles | 0.5 to 1.0 mm (0.020 to 0.039 in) | 1.0 to 2.0 mm (0.039 to 0.079 in) | Steel-rule die kerf, beveled edge flare on 1.5 to 3 mm (0.059 to 0.118 in) greyboard, and wrapped paper edges |
| Plastic tokens | 0.5 to 0.8 mm (0.020 to 0.031 in) | 1.0 to 1.6 mm (0.039 to 0.063 in) | Mold shrinkage stability, draft angles, and parting-line flash |
| Cards & card stacks | 1.0 to 1.5 mm (0.039 to 0.059 in) | 2.0 to 3.0 mm (0.079 to 0.118 in) | Stack bow, corner radius matching, and finger clearance for lifting cards flat |
Use the following plain-text formulas to size the die-cut vector path from measured nominal component dimensions:
Cutout Width = Nominal Component Width + (2 * Clearance per Side)
Cutout Length = Nominal Component Length + (2 * Clearance per Side)
- Card stack and lamination allowances: A single card's caliper varies by stock—for example,
300 gsmart or blue core runs0.28–0.31 mm(0.011–0.012 in),330 gsmblack core runs0.32–0.34 mm(0.013 in), and400 gsmart stock runs0.40–0.44 mm(0.016–0.017 in), with double-sided film adding0.03–0.05 mm(0.001–0.002 in) per card. While caliper primarily drives recess depth rather than lateral width, double-sided lamination and subtle deck bow make the 1.0 to 1.5 mm (0.039 to 0.059 in) per-side lateral clearance necessary so cards do not bind against the pocket walls. - Corner radius matching: Round-cornered cards typically use
R3–R3.5 mm(R0.118–R0.138 in) corners. Match or slightly exceed the component's corner radius on the pocket dieline (or include corner relief cutouts) so rounded corners do not wedge into tighter die corners. - Wrapped vs. bare-cut pocket walls: Raw-cut greyboard (
1.5 / 2 / 2.5 / 3 mm, or0.059 / 0.079 / 0.098 / 0.118 in) holds the exact die-cut opening. When the printed top sheet is wrapped down into the pocket walls, the folded paper thickness and adhesive squeeze reduce the finished opening, requiring an extra 0.3 to 0.5 mm (0.012 to 0.020 in) per side in the structural dieline.
Job-Specific Production Steps
- Measure physical production samples: Measure at least 10 pieces from the actual partner-manufactured cube, tile, token, or card lot across all axes before locking the board dieline. Use the largest measured dimension—not the CAD target—as the baseline for the clearance formula.
- Account for top-layer greyboard thickness and rib width: Check the spacing between adjacent component wells. Keep solid greyboard bridges wide enough to withstand steel-rule die cutting and lamination pressure without crushing or tearing, especially on
2.5 mm(0.098 in) or3 mm(0.118 in) top layers. - Add finger-access geometry where clearance stays tight: If a tile or card well uses the 0.5 to 0.75 mm (0.020 to 0.030 in) side clearance to prevent piece shifting, add a semicircular thumb notch along one edge of the cutout so players can lift the component without prying against the paper wrap.
- Dry-fit a white-sample board: Assemble an unprinted or digitally printed physical dummy of the layered board using the target greyboard thickness and test-fit the physical components before cutting the production steel-rule die.
Sign-Off Criteria
- Drop-in seating: Every sampled component from the batch drops flat to the backing layer under light finger pressure without forcing or bowing the top layer.
- Clean extraction: Each piece lifts out cleanly by finger (or via its thumb notch) without catching on the cut paper edge or scraping painted wood or laminated tile faces.
- Batch repeatability: At least 10 randomly selected pieces from the component run fit the same pocket cleanly without binding at the corners or edges.
- Controlled play: Seated cubes and tiles stay aligned within their grid without rotating visibly out of square or sliding excessively during normal table contact.
Concrete Failure Modes
- Undersized pocket jamming (
< 0.5 mm/0.020 inper side): Normal tumbling variance on wooden cubes or slight die-cut flare on thick cardboard tiles wedges pieces tightly into the well, tearing or delaminating the printed top sheet when players pry them out. - Corner-radius binding on card wells: Cutting a card well with tight or square die corners while sizing lateral clearance near
0.5 mm(0.020 in) per side pinchesR3–R3.5 mm(R0.118–R0.138 in) cards at the corners, leaving cards tilted above the board surface. - Uncompensated wrapped-wall pinch: Applying bare-cut clearance numbers to a wrapped-edge recess narrows the finished opening by two layers of wrap paper and glue, turning a nominal
0.5 mm(0.020 in) per-side allowance into an interference fit. - Excessive rattle and skew (
> 1.5 mm/0.059 inper side): Over-sizing wells for small wooden cubes or thin tokens lets components twist out of alignment, double-stack unintentionally, or slide out of position when the board is bumped. - Collapsed inter-well ribs: Packing multiple pockets too tightly together on a die-cut sheet leaves thin greyboard walls that crush under the cutting rule or tear during lamination and stripping.
Parent guide Recess Cutout and Layer Registration Tolerances