Registration sits near ±0.5 mm (±0.020 in) on compact sheets with rigid greyboard plies and balanced grain direction, and widens toward ±1.0 mm (±0.039 in) on larger sheet formats, wrapped top plies with heavy 15–20 mm (0.591–0.787 in) wrap tension, or thin card-stock plies that expand slightly from adhesive moisture. This tolerance governs how closely recessed wells, cutouts, and printed base graphics align within recess cutout and layer registration.

Specifications

Parameter Specification Notes
Sheet-fed layer registration ±0.5 to ±1.0 mm (±0.020 to ±0.039 in) Measured from top-ply well edge to base-ply artwork
Base-well internal bleed ≥3 mm (0.118 in) Extends base-well color/art past the die-cut opening
Safety margin (base & top) ≥3 mm (0.118 in) Keep critical text, numbers, and borders clear of cut walls
Greyboard ply thickness 1.5 / 2.0 / 2.5 / 3.0 mm (0.059 / 0.079 / 0.098 / 0.118 in) Selected per ply for structural rigidity and well depth
Cardstock ply option 350–400 gsm (0.34–0.44 mm / 0.013–0.017 in) ~129–148 lb US Cover (20 × 26 in basis sheet; distinct from 25 × 38 in US Text)
Wrap margin (wrapped plies) 15–20 mm (0.591–0.787 in) Required around outer edges when wrapping greyboard
Minimum die gap / web width 3–4 mm (0.118–0.157 in) Minimum bridge between adjacent wells to prevent flex
Prepress artwork setup PDF/X-1a or PDF/X-4 (AI/PDF/PSD), ≥300 DPI CMYK with separate spot/die layers; TAC ≤280%–300%; 100% K fine text; rich black C40–60 M30–40 Y30–40 K100

Production Steps

  1. Prepress & Shared Coordinate Setup: Build the top-ply die-line and base-ply print file on a single shared origin in PDF/X-1a or PDF/X-4. Extend base-well background fills at least 3 mm (0.118 in) beyond every cutout edge, and keep all base-well icons or labels at least 3 mm (0.118 in) inside the opening.
  2. Printing & Surface Lamination: Print top and base sheets in CMYK at ≥300 DPI with TAC capped at 280%–300%. Apply protective film (such as anti-scuff matte for dark artwork) before mounting to stabilize sheet surface tension.
  3. Top-Ply Die-Cutting & Stripping: Die-cut the recessed openings into the upper ply while preserving at least 3–4 mm (0.118–0.157 in) webs between adjacent wells so the top sheet stays flat during feeding.
  4. Sheet-Fed Mounting & Pressing: Align the die-cut top ply to the printed base ply using mechanical side-lay and lead-edge guides on a sheet-fed laminator. Apply controlled adhesive coat weight and press flat through curing.
  5. Final Perimeter Trim: Trim the laminated two-ply board to finished size once the adhesive bond sets, using the outer 3 mm (0.118 in) bleed.

Sign-Off Criteria

  • Registration Check: Across first-off mounted sheets, measure well-to-base graphic offset at all four corners; offset stays within ±0.5 to ±1.0 mm (±0.020 to ±0.039 in).
  • Zero Unprinted Edge Exposure: No white stock or unprinted base border is visible inside any recessed well at maximum tolerance shift.
  • Clean Well Interiors: No adhesive squeeze-out along internal cut walls and no crushed or delaminated 3–4 mm (0.118–0.157 in) webs.
  • Board Flatness: Cured dual-layer boards lie flat without edge lift or ply separation.

Concrete Failure Modes

  • White Halo Inside Wells: Omitting the 3 mm (0.118 in) internal bleed on the base ply exposes unprinted board or white paper whenever the top ply shifts by 0.5–1.0 mm (0.020–0.039 in). Extend all well backgrounds ≥3 mm (0.118 in) past the die path.
  • Clipped Base Graphics or Borders: Thin keylines or numbers placed within 1–2 mm (0.039–0.079 in) of a well wall get partially covered by the top ply. Maintain a ≥3 mm (0.118 in) safety zone inside every opening, and avoid tight concentric borders around individual wells.
  • Lead-to-Tail Misregistration on Large Sheets: Moisture from water-based mounting adhesive expands the base liner across the sheet width, pushing tail-edge wells past ±1.0 mm (±0.039 in). Match paper grain direction across both plies and condition sheets in the pressroom before mounting.
  • Web Skew or Tear During Feeding: Bridges narrower than 3–4 mm (0.118–0.157 in) flex under laminator roller pressure, distorting well geometry. Keep die gaps at ≥3–4 mm (0.118–0.157 in) and keep outer frame borders continuous until final trim.
  • Adhesive Squeeze-Out in Wells: Excess glue near cutout perimeters oozes onto the printed base well under pressing pressure. Control adhesive film thickness and keep glue application clear of the immediate die-cut lip.