| Component Structure | Mechanical Job | Typical Greyboard Caliper | Key Structural Requirement | Primary Fit or Tolerance Risk |
|---|---|---|---|---|
| Flat tokens | Pick-up counters, coins, chits | 1.5–2 mm (0.059–0.079 in) | Clean punch-out nicks with 3–4 mm (0.118–0.157 in) die gap | Face-paper tearing at nicks or tight bridges |
| Modular map tiles | Flat, repeatable table layouts | 2–3 mm (0.079–0.118 in) | Balanced top/bottom wrap tension and square or radiused joints | Board warping, rocking, or uneven border registration |
| Slotted standees | Vertical figure seated in a base | 1.5–2.5 mm (0.059–0.098 in) | Slot width matched to finished laminated board caliper | Crushed slot edges (too tight) or leaning figures (too loose) |
| Riveted dials | Multi-layer rotating value tracker | 1.5–2 mm (0.059–0.079 in) per layer | Rivet post length matched to total stacked caliper | Bound rotation (too tight) or window misalignment (too loose) |
| 3D slot-together assemblies | Load-bearing trays, towers, stands | 2–3 mm (0.079–0.118 in) | Tab-and-slot friction fit with chamfered lead-ins and grain alignment | Wrap delamination during assembly or flexing under load |
Specifications by Structure
Core Board, Wraps, and Finish Stack
- Greyboard calipers: Standard structural cores run 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), and 3 mm (0.118 in).
- Printed wraps: Specify top and bottom wrap sheets in gsm rather than US pound weights alone, because US Text LB is measured on a 25 x 38 in (635 x 965 mm) basis sheet while US Cover LB is measured on a 20 x 26 in (508 x 660 mm) basis sheet.
- Lamination thickness: Double-sided film adds 0.03–0.05 mm (0.001–0.002 in) to the finished sheet caliper. Anti-scuff matte film suits dark artwork and high-touch dials or tiles by reducing visible rub marks.
- Die-cut spacing: Maintain a 3–4 mm (0.118–0.157 in) gap between adjacent components on the punch sheet so steel rules and ejection rubber have room to cut cleanly without crushing nearby edges. Where wrapped/turned edges are used on rigid assemblies, allow a 15–20 mm (0.591–0.787 in) wrap margin.
Flat Tokens and Modular Map Tiles
- Flat tokens: Small chits and coins perform best on 1.5 mm (0.059 in) or 2 mm (0.079 in) greyboard. Keep minimum token widths wide enough to maintain the 3–4 mm (0.118–0.157 in) die gap without leaving fragile waste bridges.
- Modular map tiles: Larger tiles typically use 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in) greyboard to resist dishing. Butt-jointed tiles require clean, square perimeter cuts; interlocking puzzle-tab tiles require smooth corner radii so tabs do not catch or delaminate during repeated assembly.
Slotted Standees
- Base pairing: Vertical standees seat into either a die-cut punchboard base of the same sheet caliper or a separate molded plastic base.
- Slot sizing: Set slot width to the finished laminated board caliper (core greyboard + top/bottom printed wraps + film), not the raw greyboard thickness alone:
Finished slot width = Core caliper + Top wrap & film + Bottom wrap & film - Stress relief: Add a small rounded relief at the base of the slot and slight lead-in chamfers on the mating edge so the printed face paper does not split when pushed into the base.
Riveted Dials
- Layer stack: A standard dial consists of a base wheel, one or more rotating indicator wheels, and a top cover plate with a die-cut viewing window, joined through a central hole by a two-part plastic or metal rivet.
- Clearance and post length: The center hole must clear the rivet barrel so the wheel turns freely, while the rivet post length must match the combined thickness of every stacked layer (for example, two 1.5 mm / 0.059 in layers plus wraps and film versus two 2 mm / 0.079 in layers).
- Window safety: Keep printed numbers, icons, and borders at least 3 mm (0.118 in) clear of viewing window cut lines so normal die registration shift does not clip values.
3D Slot-Together Assemblies
- Structural caliper: Multi-plane builds (trays, risers, towers, and terrain) typically require 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in) greyboard so interlocking walls stay rigid without bowing.
- Tab-and-slot geometry: Size slots to the finished laminated caliper for a firm friction fit, and taper or chamfer tab corners slightly so the wrap paper slides in without peeling. Orient long load-bearing walls parallel to the board grain to minimize flex.
Prepress and Production Steps
- Artwork and file setup: Supply files in AI, PDF, or PSD format, exported as PDF/X-1a or PDF/X-4 with all fonts outlined or embedded and raster imagery at >=300 DPI.
- Color and ink limits: Build artwork in CMYK with separate spot layers for die-cut lines, kiss-cuts, nicks, and rivet holes. Use 100% K for fine text, rich black (C40–60 M30–40 Y30–40 K100) for solid dark areas, and keep total area coverage (TAC) at <=280%–300%.
- Bleed and safety margins: Extend artwork 3 mm (0.118 in) bleed per side past every cut line (including internal slots and dial viewing windows). Keep critical graphics >=3 mm (0.118 in) inside cut lines, and >=4–5 mm (0.157–0.197 in) on bordered tiles or tokens.
- Printing, mounting, and pressing: Specialist tabletop manufacturing partners print top and bottom sheets via offset CMYK, apply lamination or varnish, mount both wraps onto the selected greyboard caliper, and press the sheets flat while adhesive cures.
- Die cutting and secondary assembly: Steel-rule dies punch the nested components, leaving calibrated nicks to hold parts in the sheet during transit. Riveted dials proceed to secondary rivet insertion; slot-together builds and standees are collated flat in the sheet or pre-punched according to pack-out requirements.
- Regulatory assessment and testing: When components include small punch-out tokens, detachable rivets, or accessible edges intended for children's products, plan EN 71 assessment and testing early and maintain supporting lab test records and material documentation; see the European Commission Toy Safety overview for applicable procedures.
Sign-Off Criteria
- Registration and margins: Cut lines, viewing windows, and center rivet holes align cleanly with printed graphics; 3 mm (0.118 in) bleed and >=3 mm (0.118 in) (or >=4–5 mm / 0.157–0.197 in for bordered backs/faces) safety zones are preserved.
- Hand punch-out test: Tokens, tiles, and slot-together parts release cleanly from the frame by hand without tearing face paper at the nicks.
- Mechanical fit on laminated dummy: Standees seat firmly without crushing slot edges; riveted dials rotate smoothly without binding or drifting off the window; 3D slot-together joints lock securely without peeling the wrap.
- Flatness and surface integrity: Mounted boards lie flat on a level surface with no visible curl, and lamination shows no bubbling or edge lift around tight radii or slots.
Concrete Failure Modes
- Slot too tight or too loose: Sizing standee or 3D slots to raw greyboard caliper (such as 2 mm / 0.079 in) without adding wrap and double-sided film thickness (+0.03–0.05 mm / 0.001–0.002 in) causes crushed edges and delaminated paper on assembly, or loose, leaning parts.
- Face-paper tear on punch-out: Nesting parts closer than the 3–4 mm (0.118–0.157 in) die-gap minimum, placing oversized nicks on delicate corners, or cutting across narrow bridges rips the printed wrap off the core when players punch components out.
- Rivet binding or gapping: Using a rivet post that is too short for the stacked caliper pinches the rotating wheel so it cannot turn; a post that is too long leaves play between layers and lets dial values drift out of the window.
- Tile warping and rocking: Unbalanced moisture absorption between top and bottom wraps, mismatched paper grain direction, or insufficient pressing time causes modular map tiles to dish and rock on the table.
- Clipped dial numbers or uneven borders: Ignoring the >=3 mm (0.118 in) safety margin around viewing windows or the >=4–5 mm (0.157–0.197 in) margin on bordered tiles makes normal die-cut registration tolerance immediately visible.
- Scuffing on dark artwork: Leaving dark rich-black tiles or high-friction dial faces with standard unprotected finishes results in visible rub marks during shipping and repeated rotation; specifying anti-scuff matte film prevents this.