Thicker greyboard cores—2.5 mm or 3 mm (0.098 in or 0.118 in) compared to 1.5 mm or 2 mm (0.059 in or 0.079 in)—displace more material under blade pressure, requiring the wider 4 mm (0.157 in) die gap and adjusted slot widths. Tightly nested small tokens, acute corners, and heavy-ink or dark-art finishes with anti-scuff matte lamination also require stricter margin and nick placement to prevent crushed waste bridges and face-liner tearing during punch-out.
Clearances, Die-Line, and Prepress Specifications
| Parameter | Specification | Governing Condition |
|---|---|---|
| Adjacent die-to-die gap | 3–4 mm (0.118–0.157 in) min | 3 mm (0.118 in) for straight edges on 1.5–2 mm (0.059–0.079 in) board; 4 mm (0.157 in) for 2.5–3 mm (0.098–0.118 in) board or acute shapes |
| Greyboard core thickness | 1.5 / 2 / 2.5 / 3 mm (0.059 / 0.079 / 0.098 / 0.118 in) | Selected for token rigidity, slot strength, and overall stack height |
| Print bleed | 3 mm (0.118 in) per side | Extends continuously past every cut and slot line |
| Inner safety margin | ≥3 mm (0.118 in) standard; ≥4–5 mm (0.157–0.197 in) bordered | Keeps text, icons, and borders clear of die-registration shift |
| Rounded corner radius | R3–R3.5 mm (0.118–0.138 in) | Applied to rounded tiles or board perimeters |
| Boxed stack clearance | 1.5–2.5 mm (0.059–0.098 in) W/H; 1.5–3 mm (0.059–0.118 in) height | Prevents edge binding or lid lift when packed with other components |
| Artwork & color limits | ≥300 DPI, CMYK + spot die layer, TAC ≤280%–300% | AI, PDF, or PSD (PDF/X-1a or PDF/X-4); 100% K fine text; rich black C40–60 M30–40 Y30–40 K100 |
Nick Geometry
Nicks are small, intentional gaps ground into the steel-rule blade that leave tiny uncut paper bridges between a token and the surrounding waste matrix. They hold pieces flat during die-cutting, stripping, collating, and transit, then break cleanly when pushed out by hand.
- Placement: Position nicks symmetrically on straight edges or near sturdy corners rather than on sharp tips, narrow necks, or tight concave curves.
- Balance: Large tiles need evenly distributed nicks on opposing sides to stop warping or sagging, while small tokens need minimal, shallow nicks so the face liner does not peel away on release.
Registration Tolerances and Prepress Setup
Mechanical die-cutting introduces slight positional variance between the printed sheet and the steel-rule die. Supplying vector die-lines on a dedicated spot-color layer—separate from CMYK artwork, with outlined or embedded fonts—keeps cut paths crisp. Extending artwork 3 mm (0.118 in) past every cut line and holding critical elements at least 3 mm (0.118 in) inside the cut (or 4–5 mm / 0.157–0.197 in for bordered backs) ensures normal press-to-die shift never exposes unprinted white edges or clips borders.
Edge Profiles and Slot-Fit Allowances
Steel-rule blades have a beveled profile that compresses the top liner slightly inward as it shears through the greyboard core and bottom liner. Thicker cores (2.5–3 mm / 0.098–0.118 in) exhibit a more pronounced bevel than thinner cores (1.5–2 mm / 0.059–0.079 in). For interlocking standees or slotted dividers, size the slot width to the actual laminated caliper (greyboard plus both printed liners and any surface film) rather than the raw core thickness alone, allowing a firm friction fit without splitting the slot walls.
Job-Specific Production Steps
- Prepress and die-line separation: Place all cut, crease, and slot paths on a distinct non-printing spot layer in PDF/X-1a or PDF/X-4. Verify 3 mm (0.118 in) bleed around every token and ≥3 mm (0.118 in) safety (≥4–5 mm / 0.157–0.197 in for bordered designs).
- Sheet printing and lamination: Print face and back liners at ≥300 DPI within a 280%–300% total area coverage limit, using anti-scuff matte lamination on dark artwork to resist rubbing during die-cutting and packing.
- Board mounting and curing: Laminate printed sheets onto 1.5, 2, 2.5, or 3 mm (0.059, 0.079, 0.098, or 0.118 in) greyboard and stack under weight to cure flat.
- Steel-rule die fabrication: Bend rule blades to maintain a 3–4 mm (0.118–0.157 in) minimum waste bridge between adjacent pieces and grind balanced nicks along straight edges.
- Die-cutting and waste stripping: Cut mounted boards, strip outer perimeter trim while leaving tokens intact on their nicks, and pack sheets within box clearances of 1.5–2.5 mm (0.059–0.098 in) across width/height and 1.5–3 mm (0.059–0.118 in) for stack height.
Sign-Off Criteria
- Prepress proof: Spot die layer aligns over CMYK art, all tokens carry 3 mm (0.118 in) bleed, bordered designs keep ≥4–5 mm (0.157–0.197 in) inner clearance, and no adjacent die lines sit closer than 3 mm (0.118 in) (or 4 mm / 0.157 in on 2.5–3 mm / 0.098–0.118 in board).
- Physical sample check: Tokens remain secure when the sheet is flexed or handled, punch out cleanly without delaminating the printed face, and any slotted components assemble snugly without tearing.
- Regulatory records (when applicable): For products within toy-safety scope, EN 71 assessment and testing records are scoped to the specific board materials, inks, coatings, and small-part token dimensions per the European Commission toy safety framework.
Failure Modes
- Crushed or delaminated waste bridges: Adjacent die lines spaced under 3 mm (0.118 in)—especially on 2.5–3 mm (0.098–0.118 in) greyboard—cause opposing blade bevels to pinch and shred the narrow strip between tokens. Increase spacing to 3–4 mm (0.118–0.157 in).
- Face-paper tearing during punch-out: Nicks placed on acute corners, tight curves, or ground too wide pull the printed liner off the greyboard core when pushed out. Move nicks to straight edges and reduce nick width.
- Premature token drop-out in transit: Too few nicks or nicks placed on only one side allow heavy or large tokens to shake loose during shipping. Distribute nicks symmetrically on opposite sides.
- White edge slivers or uneven borders: Omitting the 3 mm (0.118 in) bleed or placing frames closer than 4–5 mm (0.157–0.197 in) from the cut line exposes registration variance. Extend background fills 3 mm (0.118 in) past the die line and widen inner border margins.
- Loose or splitting slot-fit joints: Cutting slots to nominal greyboard thickness without accounting for paper liners, film thickness, and blade bevel leads to wobbly tabs or split slot walls. Calibrate slot width against the laminated board caliper.