Specialty metallic and painted-edge finishes introduce post-trim heat, pressure, and adhesive transfer that standard print-only checks miss. This guide covers lot inspection checkpoints for gilded, painted-edge, and hot or cold foil-stamped decks; for baseline sampling plans and general print/cut tolerances, see card deck inspection.
Conditions That Change the Inspection
- Gilded edges vs. painted edges: Metallic gilding uses heat-activated foil applied under clamp pressure to the trimmed deck block, which risks edge-block sticking and foil flaking at the corners. Solid painted edges use liquid pigment, which risks bridging between cards if stacked before full cure.
- Hot foil stamping vs. cold foil transfer: Hot foil presses a heated die onto the sheet, creating a slight deboss and risking foil bridging on fine lines or pinholing on broad fills. Cold foil transfers inline over adhesive before or under varnish, which avoids deboss distortion but requires close checks for registration and edge lift.
- Lamination thickness and surface finish: Thick double-sided lamination can conflict with gilded edges by resisting edge-foil adhesion or lifting under heat. Anti-scuff matte film suits dark artwork where surface scratches and foil contrast are immediately visible.
- Card stock caliper and deck count: Thicker stocks (350–400 gsm) and double-sided film increase total stack height and edge stiffness, changing how tightly the deck sits inside its box and how much stress bends put on edge coatings.
Relevant Specifications and Tolerances
Card stocks are specified in gsm and US Cover LB (based on a 20 × 26 in basis sheet, distinct from US Text LB based on a 25 × 38 in basis sheet). Standard offset card runs start at 200 decks (usual tiers: 200, 300, 500, and 1,000+ decks).
| Parameter | Specification | Inspection Relevance |
|---|---|---|
| 300 gsm art / blue core | 0.28–0.31 mm (0.011–0.012 in) | Baseline stiffness; lower edge-cracking risk |
| 310 gsm black-core linen | 0.30–0.32 mm (0.012–0.013 in) | Textured surface; check foil fill on linen valleys |
| 330 gsm black core | 0.32–0.34 mm (0.013–0.013 in) | Standard heavy gaming stock; verify clean edge shear |
| 350 gsm art stock | 0.34–0.38 mm (0.013–0.015 in) | Rigid deck; higher flaking risk on thick edge coats |
| 400 gsm stock | 0.40–0.44 mm (0.016–0.017 in) | Maximum rigid edge area; inspect corner bend resistance |
| PVC stock | 0.30 mm (0.012 in) | Non-porous; verify foil and edge-coating adhesion |
| Double-sided film | +0.03–0.05 mm (0.001–0.002 in) per card | Adds stack height; thick film conflicts with gilding |
| Bleed and safety | 3 mm (0.118 in) bleed; >= 3 mm (0.118 in) safety | >= 4–5 mm (0.157–0.197 in) safety for bordered backs |
| Corner radius | R3–R3.5 mm (0.118–0.138 in) | Rounded corners must show continuous edge coverage |
| Box clearance | 1.5–2.5 mm (0.059–0.098 in) W/H; 1.5–3 mm (0.059–0.118 in) stack | Verify deck slides cleanly after film and edge coating |
Lot Inspection Steps
- Check deck fit and outer wrap first: Confirm the finished deck slides into its box within the 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) stack-height clearance without scuffing the gilded or painted edges.
- Inspect edges under raking light before separating: Look across all four sides of the clamped deck block for dull patches, uneven pigment, or exposed white paper core at the R3–R3.5 mm (0.118–0.138 in) corners.
- Fan and riffle every sampled deck: Fan the deck in both directions and separate every card individually. Listen and feel for resistance where gilding adhesive or uncured edge paint has fused adjacent cards.
- Examine hot or cold foil artwork on faces and backs: Check separate spot-layer foil elements for crisp edges on fine lines, full coverage on solid fills, and alignment against the >= 3 mm (0.118 in) safety margin (or >= 4–5 mm / 0.157–0.197 in on bordered backs).
- Flex corners and check lamination edges: Gently flex a corner of several sampled cards and inspect the cut edge under angled light for lamination edge lift or metallic flaking.
- Verify dark-artwork scuff resistance: On dark backgrounds with anti-scuff matte film, inspect card faces and backs after fanning to confirm the finish resists marking from adjacent foil-stamped faces.
Sign-Off Criteria
- Edge separation: Every card in every sampled deck separates cleanly during fanning with zero fused pairs or torn paper fibers along the trimmed edge.
- Edge coverage: Gilded or painted edges show uniform sheen and color across all four sides and around the R3–R3.5 mm (0.118–0.138 in) corners without exposed core.
- Foil transfer quality: Fine lines remain sharp without bridging across negative space, solid foil areas show no pinholes or flaking, and foil registration sits cleanly inside the safety margin.
- Lamination integrity: Film adheres flush to the trimmed edge and corners with no peeling, bubbling, or white edge lift after flexing.
- Box clearance: The completed deck, including double-sided film (+0.03–0.05 mm / 0.001–0.002 in per card), fits the box without binding against the inner walls.
Failure Modes and Root Causes
| Failure Mode | Observable Defect | Root Cause |
|---|---|---|
| Edge-block sticking | Cards cling together or tear fibers when fanned | Residual gilding heat/adhesive or uncured edge paint bridging adjacent cards under clamp pressure |
| Metallic flaking | Shiny flakes shed onto fingers or card faces during fanning | Excessive foil build-up, brittle edge coating on thick 350–400 gsm stock, or poor adhesion over thick lamination |
| Foil bridging | Fine serif type, thin rules, or tight gaps fill in with solid foil | Excess die pressure or temperature in hot foil stamping, or insufficient gap spacing in the spot foil layer |
| Lamination edge lift | Film peels back slightly at trimmed edges or R3–R3.5 mm (0.118–0.138 in) corners | Thick double-sided film delaminating under corner-rounding shear or reacting with gilding heat |
| Foil registration drift | Foil shifts noticeably relative to CMYK print or borders | Sheet stretch or die misalignment, most visible when foil sits close to the 3 mm (0.118 in) safety zone |
| Box binding | Gilded edges scrape against the tuck or rigid box walls | Stack height growth from double-sided film (+0.03–0.05 mm / 0.001–0.002 in per card) exceeding the 1.5–3 mm (0.059–0.118 in) stack clearance |
Parent guide Card Deck Lot Inspection Checkpoints