For broader playing card construction options, finishes, and core materials, see the Custom Playing Cards manufacturing guide.
Choice Conditions: 40 vs. 50 Cards and Stock Selection
- Card count (40 vs. 50 cards): A 40-card deck reduces raw stack height by 3.0–4.0 mm (0.118–0.157 in) compared to a 50-card deck, requiring a narrower tuck-box spine and lighter carton packing.
- 310 gsm black-core linen (~115 lb Cover, 20 x 26 in basis; ~209 lb Text, 25 x 38 in basis): Best for frequent shuffling and opaque light blocking; linen embossing reduces surface contact friction and masks minor handling wear.
- 330 gsm black core (~122 lb Cover, 20 x 26 in basis): Adds stiffness and snap over 310 gsm while maintaining full opacity for dark or high-contrast card backs.
- 350 gsm art stock (~129 lb Cover, 20 x 26 in basis): Suited for collector or display editions requiring maximum rigidity, though it lacks an internal black-core barrier layer and increases stack height.
- Surface film and edge treatment: Anti-scuff matte lamination protects dark solid artwork against rub marks. Avoid thick double-sided lamination if gilded edges are specified, as heavy film thickness interferes with foil adhesion along the trimmed edge.
Finished Bill of Materials and Specifications
Card Dimensions, Prepress, and Tolerances
| Parameter | Specification |
|---|---|
| Trim size | 61.5 x 95 mm (2.42 x 3.74 in) |
| Bleed size (3 mm / 0.118 in per side) | 67.5 x 101 mm (2.66 x 3.98 in) |
| Standard safety margin (faces) | >= 3 mm (0.118 in) inside trim -> 55.5 x 89 mm (2.19 x 3.50 in) |
| Bordered-back safety margin | >= 4–5 mm (0.157–0.197 in) inside trim -> 51.5–53.5 x 85–87 mm (2.03–2.11 x 3.35–3.43 in) |
| Corner radius | R3–R3.5 mm (0.118–0.138 in) |
| Color & resolution | CMYK with separate spot layers, >= 300 DPI |
| Black & ink limits | 100% K for fine text; rich black C40–60 M30–40 Y30–40 K100; TAC <= 280%–300% |
| File format | AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 with outlined or embedded fonts |
Interrupted-Border ("La Pinta") Registration Rules
Traditional Baraja Espanola faces feature an outer frame with suit-specific breaks (interruptions) along the top and bottom edges—continuous for coins, one break for cups, two for swords, and three for clubs. Because die-cutting and guillotining introduce natural sheet shift:
- Keep the outer border frame >= 3 mm (0.118 in) inside the 61.5 x 95 mm trim so die-cut variance does not clip the frame thickness unevenly.
- Use consistent stroke weights (>= 0.5 pt / 0.18 mm) on the interrupted border segments so gaps remain visually distinct after ink spread.
- Center-align face frames and back borders on the same imposition grid; asymmetric face margins combined with bordered backs amplify perceived off-center shift.
Caliper, Stack Height, and Weight by Stock
Card area per piece is 61.5 x 95 mm = 0.0058425 sq m. Double-sided film lamination adds 0.03–0.05 mm (0.0012–0.0020 in) per card.
| Card Stock | Single-Card Caliper | 40-Card Stack Height (Uncoated/Varnish) | 50-Card Stack Height (Uncoated/Varnish) | Approx. Card-Only Weight (40 / 50 Cards) |
|---|---|---|---|---|
| 310 gsm black-core linen | 0.30–0.32 mm (0.012–0.013 in) | 12.0–12.8 mm (0.47–0.50 in) | 15.0–16.0 mm (0.59–0.63 in) | 0.072 kg (0.16 lb) / 0.091 kg (0.20 lb) |
| 330 gsm black core | 0.32–0.34 mm (0.013 in) | 12.8–13.6 mm (0.50–0.54 in) | 16.0–17.0 mm (0.63–0.67 in) | 0.077 kg (0.17 lb) / 0.096 kg (0.21 lb) |
| 350 gsm art stock | 0.34–0.38 mm (0.013–0.015 in) | 13.6–15.2 mm (0.54–0.60 in) | 17.0–19.0 mm (0.67–0.75 in) | 0.082 kg (0.18 lb) / 0.102 kg (0.23 lb) |
Note: Adding double-sided film (+0.03–0.05 mm per card) increases a 40-card stack by 1.2–2.0 mm (0.047–0.079 in) and a 50-card stack by 1.5–2.5 mm (0.059–0.098 in).
Tailored Tuck Box Sizing
A custom tuck box for 61.5 x 95 mm cards requires 1.5–2.5 mm (0.059–0.098 in) clearance across width and height, and 1.5–3.0 mm (0.059–0.118 in) clearance on stack depth:
- Internal width:
61.5 + 1.5 to 2.5 mm = 63.0–64.0 mm(2.48–2.52 in) - Internal height:
95.0 + 1.5 to 2.5 mm = 96.5–97.5 mm(3.80–3.84 in) - Internal depth (spine):
Stack height (including film) + 1.5 to 3.0 mm- Example (40 cards, 310 gsm, no film):
12.0–12.8 + 1.5 to 3.0 = 13.5–15.8 mm(0.53–0.62 in) - Example (50 cards, 350 gsm, no film):
17.0–19.0 + 1.5 to 3.0 = 18.5–22.0 mm(0.73–0.87 in)
- Example (40 cards, 310 gsm, no film):
- Tuck stock: 300–350 gsm art board (0.34–0.38 mm / 0.013–0.015 in at 350 gsm) with matte or gloss film lamination, adding roughly 0.010–0.015 kg (0.02–0.03 lb) to finished deck weight.
Job-Specific Production Steps
- Prepress and imposition: Verify 67.5 x 101 mm (2.66 x 3.98 in) bleed boxes, >= 3 mm face safety, >= 4–5 mm back border safety, and TAC <= 280%–300%. Convert fine black text to 100% K and isolate spot varnish or foil on separate vector layers.
- Dieline generation from final stock caliper: Measure actual sheet caliper (including any double-sided film) before locking the tuck-box dieline spine width.
- Offset sheet printing and coating: Print front and back sheets, apply aqueous varnish, UV coating, or anti-scuff matte film, and allow ink/coating cure before cutting.
- Slitting, corner rounding, and collation: Guillotine sheets into strips, punch cards to 61.5 x 95 mm with R3–R3.5 mm corners, and collate in exact 40- or 50-card order.
- Box die-cutting, gluing, and packing: Die-cut and side-glue tuck boxes, insert collated decks, and apply cellophane overwrap if specified.
Sign-Off Criteria
- Registration and border balance: Interrupted-border marks on all four suits sit completely inside the 55.5 x 89 mm (2.19 x 3.50 in) safe zone with no clipped outer lines; bordered backs show even visual margins across sample pulls.
- Stack and tuck fit: Finished 40- or 50-card deck slides into the glued tuck box without bowed side panels or forced thumb-notch resistance, maintaining 1.5–3.0 mm depth clearance.
- Color and TAC: Rich black areas dry without set-off or blocking; spot-color and foil layers align with CMYK keylines within standard offset tolerance.
- Conditional regulatory records (when applicable): If the deck is marketed for children's play in the EU, EN 71 toy safety assessment and testing procedures apply (European Commission Toy Safety). Retail packaging placed on the German or French market may require producer registration and sorting-label procedures under VerpackG (Zentrale Stelle Verpackungsregister) and Triman Info-tri (French Ministry of Ecological Transition).
Concrete Failure Modes
- Clipped or uneven suit-edge marks: Placing the interrupted border frame closer than 3 mm (0.118 in) to the 61.5 x 95 mm trim causes die-cut shift to slice away part of the gap pattern, obscuring suit identification.
- Tight or bulging tuck boxes: Ordering a fixed-depth tuck box before accounting for 350 gsm caliper variance or +0.03–0.05 mm per card from double-sided film adds up to 2.5 mm (0.098 in) to a 50-card stack, splitting box glue seams or jamming insertion.
- Ink set-off and scuffing on dark backs: Exceeding 300% TAC or omitting anti-scuff matte lamination on heavy dark-ink card backs causes ink transfer during guillotining and visible edge whitening during shuffling.
- Gilded-edge flaking: Specifying thick double-sided film lamination alongside metallic edge gilding prevents foil from bonding cleanly to the card edge, leading to peeling along the R3–R3.5 mm corners.
Parent guide Custom Playing Card Printing