For general playing-card stock options and standard deck configurations, see the playing cards manufacturing guide.
When Conditions Change the Specification
- Thicker stock or double-sided film: Moving from 310 gsm black-core linen (0.30–0.32 mm / 0.0118–0.0126 in) to 330 gsm black core (0.32–0.34 mm / 0.0126–0.0134 in) or adding double-sided film (+0.03–0.05 mm / 0.0012–0.0020 in per card) increases each 54-card stack height and requires deepening the compartment or tuck.
- Alternative card stocks: 300 gsm art/blue core (0.28–0.31 mm / 0.0110–0.0122 in) reduces snap slightly; 350 gsm art stock (0.34–0.38 mm / 0.0134–0.0150 in) and 400 gsm (0.40–0.44 mm / 0.0157–0.0173 in) add stiffness and bulk; 0.30 mm (0.0118 in) PVC alters ink adhesion and heat-sealing handling.
- Order tiers and box tooling: Standard offset card printing starts at 200 decks (usual tiers: 200, 300, 500, 1,000+), while twin-compartment rigid boxes, custom inserts, and dedicated die tooling follow project and component minimums.
- Dark backs and edge finishes: High-coverage dark artwork benefits from anti-scuff matte coating; thick lamination conflicts with gilded edges and prevents clean edge-foil adhesion.
Complete Bill of Materials and Specifications
Specify all paper and board weights in gsm alongside caliper in mm/in. When referencing US pound weights, distinguish US Text LB (25 x 38 in basis sheet) from US Cover LB (20 x 26 in basis sheet), as equal pound ratings represent different sheet thicknesses and densities.
| Component | Default Specification | Dimensions / Caliper | Notes |
|---|---|---|---|
| Playing cards (108 total) | Two 54-card stacks on 310 gsm black-core linen | 57 x 89 mm (2.24 x 3.50 in); 0.30–0.32 mm (0.0118–0.0126 in) per card; R3–R3.5 mm (0.118–0.138 in) corners | Bare 108-card weight: 108 x 0.057 m x 0.089 m x 310 gsm = 170 g (0.17 kg / 0.37 lb) |
| Single 54-card bare stack | 54 cards, linen finish + aqueous varnish | Stack height: 16.2–17.3 mm (0.64–0.68 in) | Add +0.03–0.05 mm (0.0012–0.0020 in) per card if double-sided film is applied |
| Split-cavity tuck or compartment (x2) | Twin tuck boxes in sleeve, or twin-well rigid box | Internal W x H: 58.5–59.5 x 90.5–91.5 mm (2.30–2.34 x 3.56–3.60 in); Internal depth: 18–20 mm (0.71–0.79 in) | Includes 1.5–2.5 mm (0.059–0.098 in) W/H clearance and 1.5–3 mm (0.059–0.118 in) stack height clearance |
| Rigid outer box (optional) | Wrapped greyboard two-piece or hinged box | Greyboard: 1.5, 2, 2.5, or 3 mm (0.059, 0.079, 0.098, or 0.118 in); Wrap margin: 15–20 mm (0.59–0.79 in) | Accommodates two side-by-side 54-card wells plus optional leaflet space |
| Rules / scoring leaflet (optional) | 4-, 6-, or 8-panel folded sheet | 80–120 gsm interior stock (Text LB scale), 0.08–0.13 mm (0.003–0.005 in) per sheet | Bound booklets use multiples of 4: saddle stitch 12–40 pages with 200–300 gsm cover (Cover LB scale) |
Point-Value Corner Pip and Prepress Specifications
- Corner pip placement: Canasta decks require corner pips showing rank, suit, and point value so fanned hands remain readable. Place all pips, indices, and point numerals inside the safety zone: ≥3 mm (0.118 in) from the 57 x 89 mm (2.24 x 3.50 in) trim edge, and ≥4–5 mm (0.157–0.197 in) for bordered card backs.
- Bleed and file format: Supply AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 at ≥300 DPI with 3 mm (0.118 in) bleed per side (63 x 95 mm / 2.48 x 3.74 in untrimmed artboard).
- Color and typography: Outline or embed all fonts. Use CMYK with separate spot layers for metallic inks or spot varnishes. Set fine text and small point-value numerals to 100% K; use rich black (C40–60 M30–40 Y30–40 K100) for solid dark backgrounds while keeping total area coverage (TAC) at ≤280%–300%.
Production Steps and Sign-Off Criteria
- Prepress and imposition: Lay out 108 distinct card faces (two 54-card press forms or a combined 108-card imposition) and verify corner-pip safety clearance against the R3–R3.5 mm (0.118–0.138 in) corner die path. Confirm PDF/X-1a or PDF/X-4 compliance, 3 mm (0.118 in) bleed, and TAC ≤280%–300%.
- Offset printing and coating: Print CMYK + spot layers on 310 gsm black-core linen. Inspect registration on 100% K point-value pips and apply aqueous or anti-scuff matte coating.
- Die-cutting, cornering, and collation: Slit and round corners to 57 x 89 mm (2.24 x 3.50 in) with R3–R3.5 mm (0.118–0.138 in) radii. Collate strictly into two separate 54-card stacks so duplicate ranks and jokers remain balanced across both halves.
- Cavity loading and packing: Insert each 54-card stack into its 18–20 mm (0.71–0.79 in) compartment or tuck, add any 4/6/8-panel leaflet, and pack into master cartons.
- Sign-off criteria:
- Card caliper measures 0.30–0.32 mm (0.0118–0.0126 in) and bare 54-card stack height measures 16.2–17.3 mm (0.64–0.68 in).
- Cavity clearance holds 1.5–2.5 mm (0.059–0.098 in) on width and height and 1.5–3 mm (0.059–0.118 in) on stack depth without pinching or excessive rattle.
- All point-value corner pips sit clear of R3–R3.5 mm (0.118–0.138 in) rounded corners, and carton gross weights are recorded in both kg and lb.
Regulatory and Packaging Compliance
- EN 71 (Toy Safety): If the canasta set is marketed or intended for children under 14, perform EN 71 safety assessment and laboratory testing in line with EU Toy Safety requirements and maintain technical documentation.
- Germany (VerpackG): For finished sets placed on the German market, register the brand and report packaging weights under VerpackG LUCID.
- France (Triman): For consumer-facing decks sold in France, apply sorting marks on the packaging per Triman Info-Tri.
Concrete Failure Modes
- Clipped point-value pips: Placing point numerals closer than 3 mm (0.118 in) to the trim line causes R3–R3.5 mm (0.118–0.138 in) corner-rounding dies to slice through the numbers.
- Overstuffed single cavity or tight tuck: Packing all 108 cards into one cavity (32.4–34.6 mm / 1.28–1.36 in bare stack height) or omitting the 1.5–3 mm (0.059–0.118 in) depth clearance in a 54-card tuck—especially after adding double-sided film (+0.03–0.05 mm per card)—causes bowed lids and crushed card edges.
- Blurred point numerals: Using 4-color rich black instead of 100% K on small corner-pip text creates cyan/magenta/yellow fringing under normal press registration tolerances.
- Off-center bordered backs: Keeping safety margins below 4–5 mm (0.157–0.197 in) on bordered backs makes minor die-cut drift immediately visible when fanning a 108-card hand.
- Gilding and scuff defects: Applying thick lamination prevents gilded edge foil from bonding cleanly, while omitting anti-scuff matte on dark, high-TAC backs leads to visible rubbing after initial shuffles.
Parent guide Custom Playing Card Printing