Standard offset production with specialist playing-card and tabletop manufacturing partners starts at 200 decks (usual tiers: 200, 300, 500, and 1,000+). Rigid club cases and custom tooling follow project and component minimums. For the broader custom playing cards baseline covering standard 54-card formats and general finishing options, see the parent specification.
Concrete Choice and What Changes It
- Trim size (
56 x 87 mmvs.59 x 92 mm): Select 56 x 87 mm (2.20 x 3.43 in) for traditional compact French belote handling and tight pocket carry. Select 59 x 92 mm (2.32 x 3.62 in) when larger suit indices, corner pips, or club-table legibility take priority. - Card stock (
310 gsmlinen vs.330 gsmsmooth black core): Select 310 gsm black-core linen (0.30–0.32 mm / 0.0118–0.0126 in) for frequent shuffling, reduced air-pocket friction, and club play. Select 330 gsm smooth black core (0.32–0.34 mm / 0.0126–0.0134 in) when maximum stiffness, snap, and high-resolution solid-ink smoothness matter more than embossed texture. - Alternative stocks: Use 300 gsm art or blue-core stock (0.28–0.31 mm / 0.0110–0.0122 in) only for light promotional decks where cost and lower deck weight outweigh extended shuffle life. Use 0.30 mm (0.0118 in) PVC only for waterproof outdoor or café decks.
- Packaging (
tuck boxvs.rigid club case): Use a shallow tuck box sized to the 32-card stack for retail and standard club distribution. Use a rigid two-piece club case (1.5–3 mm / 0.059–0.118 in greyboard) for tournament, commemorative, or twin-deck gift sets. - Surface finish and edge gilding: Apply anti-scuff matte lamination or varnish on dark card backs to prevent rub marks. Avoid thick double-sided film lamination when specifying gilded edges, as thick film edges conflict with foil adhesion and cleanly sheared edges.
Default Bill of Materials and Specifications
All paper weights are specified in gsm; US paper designations distinguish Cover LB (20 x 26 in basis sheet) used for card and tuck stock from Text LB (25 x 38 in basis sheet) used for interior leaflets.
| Component | Default Specification | Dimensions / Caliper | Notes & Alternatives |
|---|---|---|---|
| Card set | 32 French-suited cards | 56 x 87 mm (2.20 x 3.43 in) or 59 x 92 mm (2.32 x 3.62 in) | R3–R3.5 mm (R0.118–R0.138 in) rounded corners |
| Card stock | 310 gsm black-core linen or 330 gsm black core | 0.30–0.32 mm (0.0118–0.0126 in) or 0.32–0.34 mm (0.0126–0.0134 in) | 300 gsm art/blue core (0.28–0.31 mm / 0.0110–0.0122 in); PVC 0.30 mm (0.0118 in) |
| Surface film | Playing-card varnish or matte/gloss film | +0.03–0.05 mm (0.0012–0.0020 in) per card if double-sided film | Anti-scuff matte for dark backs; omit thick film on gilded decks |
| Deck weight (cards only) | 32-card unlaminated stack | 56 x 87 mm: 0.048–0.051 kg (0.107–0.113 lb); 59 x 92 mm: 0.054–0.057 kg (0.119–0.126 lb) | 200-deck card weight: 9.67–11.46 kg (21.3–25.3 lb) depending on trim and gsm |
| Shallow tuck box | Printed paperboard tuck sized to 32 cards | Clearance: +1.5–2.5 mm (0.059–0.098 in) W/H; +1.5–3 mm (0.059–0.118 in) depth | Must use a 32-card dieline, not a 54-card dieline |
| Rigid club case (optional) | Wrapped greyboard two-piece box | 1.5, 2, 2.5, or 3 mm (0.059, 0.079, 0.098, or 0.118 in) greyboard | 15–20 mm (0.59–0.79 in) wrap margin on all turned edges |
| Rules leaflet (optional) | 4, 6, or 8 panels, folded | 80–120 gsm interior stock (0.08–0.13 mm / 0.0031–0.0051 in per sheet; US Text LB basis 25 x 38 in) | Bound booklets use multiples of 4 pages (12–40 pp saddle stitch; 200–300 gsm Cover LB basis 20 x 26 in) |
Shallow-Box Sizing Math
Calculate internal box dimensions directly from the finished 32-card stack height plus clearance:
- 32-card stack height (varnished, no film):
32 x 0.30–0.34 mm = 9.60–10.88 mm(0.378–0.428 in). - 32-card stack height (with double-sided film): add
32 x 0.03–0.05 mm = 0.96–1.60 mm(0.038–0.063 in), yielding10.56–12.48 mm(0.416–0.491 in). - Internal box depth (stack +
1.5–3 mm/0.059–0.118 inclearance):- Unlaminated 32-card deck:
11.10–13.88 mm(0.437–0.546 in). - Laminated 32-card deck:
12.06–15.48 mm(0.475–0.609 in). - Add folded leaflet thickness (
panels x 0.08–0.13 mm) if a rules insert ships inside the tuck.
- Unlaminated 32-card deck:
- Internal box width and height (trim +
1.5–2.5 mm/0.059–0.098 inclearance):56 x 87 mmdeck:57.5–58.5 x 88.5–89.5 mm(2.26–2.30 x 3.48–3.52 in).59 x 92 mmdeck:60.5–61.5 x 93.5–94.5 mm(2.38–2.42 x 3.68–3.72 in).
Prepress File Specifications
- File formats: AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 with fonts outlined or embedded.
- Color and ink limits: CMYK with separate spot layers (for Pantone inks, foil, or edge gilding), >=300 DPI raster assets, 100% K for fine text and suit pips, rich black
C40–60 M30–40 Y30–40 K100, and Total Area Coverage (TAC)<= 280%–300%. - Bleed and safety:
3 mm(0.118 in) bleed per side;>= 3 mm(0.118 in) safety margin for full-bleed artwork and>= 4–5 mm(0.157–0.197 in) safety margin for bordered card backs.
Job-Specific Production Steps and Sign-Off Criteria
- Prepress and 32-Card Imposition Check
- Verify all 32 card fronts, shared or sequential backs, bleed (
3 mm/0.118 in), and bordered-back safety (>= 4–5 mm/0.157–0.197 in). - Confirm separate spot-color or foil layers are set to overprint where required and that fine suit pips and indices use 100% K rather than four-color rich black.
- Verify all 32 card fronts, shared or sequential backs, bleed (
- Shallow-Box Dieline and Stack Calibration
- Lock the tuck box or rigid club case dieline only after confirming final card stock caliper, film choice (
+0.03–0.05 mmper card if laminated), and leaflet panel count. - Sign off on a physical white dummy holding 32 cards of the target stock to verify thumb-notch clearance and snug stack retention.
- Lock the tuck box or rigid club case dieline only after confirming final card stock caliper, film choice (
- Press Proof and Color Sign-Off
- Approve CMYK density, TAC (
<= 280%–300%), and dark-back scuff resistance on the target board before full press run.
- Approve CMYK density, TAC (
- Die-Cutting, Corner Rounding, and Pack-Out
- Verify consistent
R3–R3.5 mm(R0.118–R0.138 in) corner radii, clean sheet-to-sheet registration across all 32 cards, and intact tuck/wrap edges with15–20 mm(0.59–0.79 in) wrap margins on rigid cases.
- Verify consistent
Regulatory and Market-Entry Procedures
When placing custom belote decks on European markets, maintain the applicable assessment, registration, and packaging-marking records:
- Toy Safety (EN 71): If the deck is marketed or intended for use by children under 14 rather than adult club play, follow the European Commission EU Toy Safety assessment and EN 71 testing procedures for the finished product and inks.
- France Packaging Sorting (Triman / Info-Tri): For packaged decks distributed in France, apply the required sorting instructions and maintain producer-responsibility records per Info-Tri / Triman.
- Germany Packaging Act (VerpackG): For packaged decks placed on the German market, complete LUCID registration, system participation, and data reporting per ZSVR Verpackungsregister.
Concrete Failure Modes
- Oversized 54-Card Tuck Box: Using a standard 54-card box depth (~18–20 mm / 0.71–0.79 in) for a 32-card belote stack (~9.60–12.48 mm / 0.378–0.491 in) leaves 6–10 mm (0.24–0.39 in) of empty slack, causing cards to rattle, corner-ding in transit, and crush the tuck panel.
- Uneven Borders on Card Backs: Setting bordered-back safety margins below
4–5 mm(0.157–0.197 in) exposes slight die-cut registration shifts as visibly lopsided frames during fanning and dealing. - Scuffed Dark Backs or Peeling Gilded Edges: Running heavy dark solids without anti-scuff matte protection leads to visible rub tracks after initial shuffling; combining thick double-sided film lamination with edge gilding causes foil flaking or edge separation.
- Blurred Pips and Ink Set-Off: Exceeding
280%–300%TAC or building small suit pips out of four-color rich black instead of100% Kcauses ink set-off on press sheets and misregistered edges on small corner indices. - Lifting Wrap on Rigid Club Cases: Reducing greyboard wrap margins below
15–20 mm(0.59–0.79 in) on1.5–3 mm(0.059–0.118 in) board causes cover paper to pull back and delaminate along inner box walls.