Standard offset production starts at 200 decks (usual tiers: 200, 300, 500, and 1,000+ decks) through specialist offset and tabletop manufacturing partners. Choose 59 x 91 mm (2.32 x 3.58 in) for traditional European-style handling or 57 x 89 mm (2.24 x 3.50 in) when matching standard bridge-width trays and sleeves; step up from a bare-deck tuck to a deeper tuck or two-piece box whenever you include a score pad or folded rule leaflet. For broader playing card stock options and general deck construction, see the playing cards printing guide.

Bill of Materials and Card Specifications

A complete doppelkopf deck consists of 48 playing cards (24 distinct face designs, each duplicated once), a shared card-back layout, a printed paperboard tuck box, and optional paper extras such as a folded rule leaflet or score pad.

Component Primary Specification Metric Dimensions / Caliper US Customary Equivalent Notes
Card trim (Option A) 48 cards (24 faces x 2) 59 x 91 mm 2.32 x 3.58 in Traditional European format
Card trim (Option B) 48 cards (24 faces x 2) 57 x 89 mm 2.24 x 3.50 in Narrower bridge-width format
Corner radius Die-cut round corners R3–R3.5 mm R0.118–R0.138 in Consistent across all 48 cards
Card stock (Standard) 310 gsm black-core linen 0.30–0.32 mm per card ~115 lb Cover (20 x 26 in basis); 0.0118–0.0126 in Opaque black-core layer prevents show-through
Card stock (Heavy) 330 gsm black core 0.32–0.34 mm per card ~122 lb Cover (20 x 26 in basis); 0.0126–0.0134 in Firmer snap; increases stack height
Surface finish Linen emboss + varnish or anti-scuff matte +0.03–0.05 mm if double-sided film +0.0012–0.0020 in per card Anti-scuff matte suits dark card backs
Tuck box stock 300–350 gsm SBS or art board 0.34–0.38 mm (350 gsm) ~111–129 lb Cover (20 x 26 in basis) Matched to deck width, height, and stack depth
Optional leaflet 4/6/8-panel folded insert on 80–120 gsm 0.08–0.13 mm per sheet ~54–81 lb Text (25 x 38 in basis) Folds flat against top of deck

Basis weight distinction: US paper weights depend on basis sheet size. Card and tuck box stocks use Cover weight (20 x 26 in basis sheet, roughly gsm / 2.704), whereas score pad sheets and rule leaflets use Text weight (25 x 38 in basis sheet, roughly gsm / 1.480). Specify gsm alongside Cover LB or Text LB so mills and converters do not substitute the wrong caliper.

Bare-deck weight estimate: Using Weight (kg) = (Width_mm / 1000) x (Height_mm / 1000) x Cards x (gsm / 1000):

  • 48 cards at 59 x 91 mm on 310 gsm: 0.059 x 0.091 x 48 x 0.310 = 0.080 kg (0.176 lb) for the cards alone, or roughly 0.095–0.105 kg (0.21–0.23 lb) packed in a tuck box.
  • A 200-deck minimum offset run weighs roughly 19–21 kg (41.9–46.3 lb) net before master cartons.

Tuck Box Clearances and Optional Score Pad Allowance

Tuck box internal dimensions must absorb both card caliper tolerance and die-cut clearance without crushing corners or leaving excessive rattle.

  1. Width and height clearance: Add 1.5–2.5 mm (0.059–0.098 in) to the card trim width and height.
    • For 59 x 91 mm cards: target 60.5–61.5 mm (2.38–2.42 in) internal width by 92.5–93.5 mm (3.64–3.68 in) internal height.
    • For 57 x 89 mm cards: target 58.5–59.5 mm (2.30–2.34 in) internal width by 90.5–91.5 mm (3.56–3.60 in) internal height.
  2. Bare-deck internal depth: Multiply single-card caliper by 48 cards, then add 1.5–3.0 mm (0.059–0.118 in) stack clearance.
    • 310 gsm black-core linen (0.30–0.32 mm): 48 x 0.30 = 14.40 mm to 48 x 0.32 = 15.36 mm bare stack; adding 1.5–3.0 mm yields 15.9–18.4 mm (0.63–0.72 in) internal depth.
    • 330 gsm black core (0.32–0.34 mm): 48 x 0.32 = 15.36 mm to 48 x 0.34 = 16.32 mm bare stack; adding 1.5–3.0 mm yields 16.9–19.3 mm (0.67–0.76 in) internal depth.
    • Double-sided film lamination adds 0.03–0.05 mm per card (1.44–2.40 mm across 48 cards), pushing the required internal depth to the upper end of the 16.5–19 mm (0.65–0.75 in) range or slightly beyond if paired with 330 gsm stock.
  3. Score pad and leaflet allowance: Measure the finished thickness of any score pad (sheet count x 0.08–0.13 mm for 80–120 gsm Text stock, plus any 0.30–0.38 mm backing board) and any 4/6/8-panel leaflet, then add that exact stack height to the tuck depth rather than forcing extras into a bare-deck dieline.

Prepress, Doubled-Rank Collation, and Production Steps

  1. File setup and color separation: Supply print-ready PDF/X-1a or PDF/X-4 files (exported from Adobe Illustrator, InDesign, or Photoshop) in CMYK at >=300 DPI with all fonts outlined or embedded. Keep fine black text at 100% K, use rich black (C40–60 M30–40 Y30–40 K100) only for large solid fills, limit total area coverage (TAC <= 280%–300%), and place any metallic or spot varnishes on separate named spot layers.
  2. Bleed and safety margins: Build 3 mm (0.118 in) bleed on all four sides of every card and tuck panel. Keep all text, corner indices, and pips at least 3 mm (0.118 in) inside the trim line, and increase the safety margin to 4–5 mm (0.157–0.197 in) on bordered card backs so die-cut drift does not create uneven borders.
  3. Sheet imposition and doubled-rank collation: Impose the 48-card deck as two identical 24-card sets (or a 48-slot sheet) so every rank and suit appears exactly twice per finished deck. Verify the imposition map before plate output so duplicated faces align with the shared back orientation.
  4. Printing, coating, and die-cutting: Offset print faces and backs, apply linen embossing and protective varnish (or anti-scuff matte for dark artwork; note that thick lamination can conflict with gilded edges if edge gilding is specified), slit into strips, punch to final trim with R3–R3.5 mm (R0.118–R0.138 in) corners, and collate in sequence before tucking and shrink-wrapping.

Sign-Off Criteria and Regulatory Records

Approve production only after verifying the following job-specific gates:

  • Prepress proof: Confirm CMYK separations, TAC <= 280%–300%, 3 mm (0.118 in) bleed, >=4–5 mm border safety on backs, and 48-card imposition showing every rank duplicated once.
  • Physical dummy: Measure a 48-card sample stack in the actual stock and finish inside the unglued tuck dieline to confirm 1.5–2.5 mm width/height play and 1.5–3.0 mm depth clearance (including any score pad).
  • Collation check: Pull random decks from the first collated batch and count 48 cards consisting of 24 exact pairs with zero missing or tripled ranks.
  • Market compliance records: Maintain documentation appropriate to the target sales channel and age grading without assuming blanket exemption:

Failure Modes and Prevention

Failure Mode Physical Cause Prevention / Fix
Missing or tripled card rank Imposition error on 24-card duplicated layout or mis-fed collator pocket Lock a 48-slot imposition proof and run a pair-count check on first-off sheets
Split tuck seams or bowed flaps Bare-deck 16.5–19 mm tuck reused after adding double-sided film, 330 gsm stock, or a score pad Recalculate 48 x card caliper + 1.5–3 mm + pad thickness and cut a revised tuck dieline
Uneven card-back borders Bordered back placed within 3 mm safety margin during strip slitting Enforce >=4–5 mm (0.157–0.197 in) safety on bordered backs or switch to full-bleed backs
Scuffing or ink transfer on dark backs High TAC (>300%) or standard gloss varnish on heavy dark solids Cap TAC at 280%–300% and specify anti-scuff matte finish
Card show-through under bright light Standard non-opaque art board substituted for black-core stock Specify 310–330 gsm black-core stock explicitly on the purchase order