For projects that need mirror-like specular reflection rather than satin sheen, hot foil stamping is the better fit; see the metallic inks overview for how coated-stock spot inks compare with other metallic decoration methods.
Flake Leafing, Satin Reflectance, and Topcoat Compatibility
Coated papers and cardboards seal surface fibers with a smooth clay or polymer layer. When metallic spot ink is printed on these substrates, the metal flakes remain suspended near the top of the ink film instead of sinking into paper pores.
- Satin reflectance: Because the smooth coating lets flakes settle relatively flat, light reflects evenly across solids and accents, producing a soft satin luster rather than a sharp mirror finish.
- Texture interaction: Smooth art stocks give the most uniform reflectance, whereas embossed linen finishes break up flake alignment across the grain peaks and valleys.
- Protective topcoats: Uncoated metallic ink oxidizes from hand oils and abrades quickly during shuffling. Sealing the sheet with an aqueous varnish or film lamination prevents tarnishing and flake rub-off, though heavy matte coatings slightly mute the metallic sheen.
- Finish compatibility: Anti-scuff matte lamination pairs well with dark artwork and metallic spot accents. Double-sided film lamination adds 0.03–0.05 mm (0.0012–0.0020 in) per card, and thick lamination can conflict with gilded edges if both are specified on the same deck.
Card Stock, Box Wrap, and Prepress Specifications
Standard offset card runs start at 200 decks (usual tiers: 200, 300, 500, and 1,000+ decks), while boxed games and custom tooling follow project and component minimums. When converting paper weights between metric gsm and US pounds (lb), distinguish US Text LB (25 × 38 in basis sheet) from US Cover LB (20 × 26 in basis sheet), as the same lb rating represents different thicknesses across basis sizes.
| Component or Parameter | Specification (Metric / Imperial) | Notes for Metallic Spot Ink |
|---|---|---|
| 300 gsm art / blue-core stock | 0.28–0.31 mm (0.011–0.012 in) | Smooth coated surface supports even flake leafing |
| 310 gsm black-core linen | 0.30–0.32 mm (0.012–0.013 in) | Linen texture scatters reflectance slightly compared with smooth art stock |
| 330 gsm black-core stock | 0.32–0.34 mm (0.0126–0.0134 in) | Standard gaming card core; requires topcoat for shuffle durability |
| 350 gsm art stock | 0.34–0.38 mm (0.013–0.015 in) | Rigid coated surface suitable for cards or tuck/insert components |
| 400 gsm art stock | 0.40–0.44 mm (0.016–0.017 in) | Heavy card/board stock; verify creasing and wrap clearances |
| Double-sided film lamination | +0.03–0.05 mm (0.0012–0.0020 in) per card | Protects metallic ink from tarnish; factor into total deck stack height |
| Rigid box greyboard & wrap | 1.5 / 2 / 2.5 / 3 mm (0.059 / 0.079 / 0.098 / 0.118 in) board; 15–20 mm (0.591–0.787 in) wrap margin | Laminate coated wrap sheets before folding to prevent ink cracking on edges |
| Box clearances | 1.5–2.5 mm (0.059–0.098 in) width/height; 1.5–3 mm (0.059–0.118 in) stack height | Accounts for laminated card caliper and smooth insertion |
| Bleed & safety margins | 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) safety; ≥4–5 mm (0.157–0.197 in) for bordered backs | Keep metallic borders inside safety margins; round corners R3–R3.5 mm (0.118–0.138 in) |
| File & color setup | AI, PDF, or PSD (PDF/X-1a or PDF/X-4); ≥300 DPI | Separate spot layer for metallic ink; outlined or embedded fonts |
| Black & ink limits | 100% K for fine text; rich black C40–60 M30–40 Y30–40 K100; TAC ≤280%–300% | Knock out CMYK beneath solid metallic spot fills |
Production Steps and Sign-Off Criteria
- Prepress separation: Place all metallic elements on a dedicated spot color layer/channel rather than building metallic simulates in CMYK. Knock out underlying process inks behind solid metallic areas to stay within the 280%–300% TAC limit, and keep fine text in 100% K instead of small metallic reverses.
- Offset printing and curing: Print CMYK layers first, then lay down the metallic spot ink on the smooth coated surface so flakes remain near the top of the film. Allow full curing before stacking or feeding into coating units, as non-absorbent coated stocks slow solvent/vehicle evaporation.
- Topcoat and converting: Apply aqueous varnish or film lamination (such as anti-scuff matte for dark designs) after the metallic ink sets. For cards, die-cut and round corners to R3–R3.5 mm (0.118–0.138 in); for packaging, laminate the coated wrap sheet before turning the 15–20 mm (0.591–0.787 in) wrap margin over 1.5–3 mm (0.059–0.118 in) greyboard.
Sign-Off Criteria
- Uniform satin luster: Solid metallic areas show even reflectance without streaking, mottling, or visible paper grain breakthrough.
- Spot registration: Metallic spot layers align cleanly with CMYK artwork and stay clear of the 3 mm (0.118 in) bleed and ≥3 mm (0.118 in) safety zone (≥4–5 mm / 0.157–0.197 in on bordered backs).
- Rub resistance: Cured and topcoated sheets show no metallic flake transfer onto adjacent cards, box interiors, or hands.
- Fit and finish clearance: Laminated deck stacks fit within the 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) stack-height box clearances, and any edge gilding is verified against the chosen film thickness.
Failure Modes and Remedies
- Tarnishing and shuffle scuffing: Exposed metallic ink reacts with skin moisture and wears down along card edges during handling. Seal the printed surface with an aqueous coating or double-sided film lamination; use anti-scuff matte film on dark card backs.
- Muddied or dull reflectance: Overprinting metallic ink on top of dense CMYK ink or burying it under an overly thick matte coating disrupts flake leafing. Knock out CMYK underneath the spot channel and match the topcoat weight to the desired sheen.
- Ink set-off in press piles: Slow-drying metallic ink vehicles transfer flakes onto the reverse of the next sheet when stacked too soon on smooth coated stock. Extend drying time and lower pile heights before topcoating or converting.
- Cracking along box-wrap folds: Heavy metallic ink coverage across 90-degree rigid box corners fractures when wrapped over greyboard. Lamination over the coated wrap sheet reinforces the ink film across the 15–20 mm (0.591–0.787 in) wrap fold.
- Edge-gilding adhesion conflict: Thick protective film applied to shield metallic face ink can interfere with gilded edges. Confirm film thickness and edge-finishing compatibility before locking the deck specification.
Parent guide Metallic Spot Inks