Standard offset metallic inks rely on light passing through a semi-translucent binder, reflecting off metallic flakes, and bouncing back from a bright white paper surface. On dark or non-paper substrates, that optical and mechanical system breaks down in two ways: dark materials absorb incident light before it can reflect, and non-porous or unevenly porous surfaces prevent standard ink vehicles from anchoring. For standard offset metallic printing on coated white paperboard, see the metallic inks guide.
Substrate and Ink Specifications
| Substrate | Optical & Surface Behavior | Required Ink & Underbase Setup | Finishing & Compatibility Notes |
|---|---|---|---|
| Black-dyed board | Absorbs light through thin offset ink; dulls metallic reflectance | High-pigment screen-printed metallic ink or opaque white underbase | Pair surrounding dark artwork with anti-scuff matte coating; thick lamination can conflict with gilded edges |
| Wood tokens | Porous grain wicks ink binder unevenly, leaving loose flakes | Sealed wood surface + screen or pad-printed metallic ink with high pigment load | Requires a protective topcoat to prevent rub-off during handling |
| Acrylic pieces | Non-porous, low surface energy; standard inks sit on top and peel | UV-cured screen or pad-printed metallic ink (or opaque backing on reverse prints) | Requires surface cleaning and adhesion-promoting ink chemistry |
| Dark fabric pouches | Textured weave and dark dye swallow thin ink deposits | Heavy-deposit screen printing with opaque underbase or high-opacity metallic paste | Heat-cure fully so the deposit flexes with the weave without cracking |
Prepress and Artwork Specifications
- File formats and color setup: Supply print-ready AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 with outlined or embedded fonts.
- Spot layers and resolution: Place the metallic ink and any opaque white underbase on separate named spot layers rather than merging them into CMYK. Keep raster artwork at >=300 DPI.
- Bleed and safety: Include 3 mm (0.118 in) bleed per side on full-bleed layouts, with >=3 mm (0.118 in) safety margin from trim or piece edges (>=4–5 mm / 0.157–0.197 in for bordered layouts).
- Surrounding blacks and ink limits: Set fine dark text to 100% K. Build rich black backgrounds around metallic accents at C40–60 M30–40 Y30–40 K100, keeping total area coverage (TAC) at <=280%–300%.
- Board thickness reference: When black-dyed wrap or board mounts onto rigid greyboard cores (1.5 mm / 0.059 in, 2 mm / 0.079 in, 2.5 mm / 0.098 in, or 3 mm / 0.118 in), maintain a 15–20 mm (0.591–0.787 in) wrap margin so metallic graphics near folds do not crack over edges.
Production Steps
- Separate and choke the underbase: Put the metallic layer and the opaque white underbase on distinct spot channels. Choke the underbase slightly inward relative to the metallic top layer so press registration variance does not expose a white edge.
- Prepare the substrate: Verify dye consistency on black-dyed board, sand and seal porous wood tokens, clean non-porous acrylic to remove mold-release residue, and tension fabric pouches flat on the print platen.
- Deposit the underbase or high-load base: Print and flash-dry or cure the opaque underbase where needed to block dark substrate absorption.
- Apply and cure the metallic ink: Screen-print, pad-print, or UV-cure the metallic layer according to the substrate. Allow full thermal or UV cross-linking before stacking pieces.
- Apply protective topcoats and verify compliance: Add a compatible varnish or anti-scuff matte coating over dark boards and handled tokens to lock flakes in place. When metallic-decorated wood, acrylic, or board pieces are produced for children's products in the EU market, retain supplier material declarations and complete EN 71 toy safety assessment and testing records for the finished ink-and-substrate combination.
Sign-Off Criteria
- Substrate-matched drawdown: Approve color brightness and flake coverage on a physical drawdown using the actual black-dyed board, wood, acrylic, or pouch fabric rather than white proof paper.
- Registration check: Inspect edges under magnification to confirm no white underbase halo peeks out around the metallic ink.
- Cure and rub check: Perform a dry rub and tape-pull check after full curing to confirm metallic pigment does not transfer to adjacent pieces or crack when fabric flexes.
Concrete Failure Modes
- Greyed-out, flat metallic appearance: Running standard translucent offset metallic ink directly over black-dyed board or dark fabric without an opaque underbase or high-pigment screen deposit.
- White haloing around graphics: Exporting the opaque white underbase at exact 1:1 dimensions with the metallic layer instead of choking it slightly inward.
- Flaking and peeling on acrylic: Using air-dry offset or unprimed ink on non-porous acrylic rather than UV-cured or adhesion-promoted screen/pad ink.
- Patchy coverage and rub-off on wood: Printing directly onto unsealed wood grain, allowing the ink vehicle to wick into fibers while dry metallic flakes rub off on hands.
- Cracking on fabric pouches: Applying an under-cured or overly brittle metallic ink deposit that fractures when the woven fabric bends.
- Bridged fine details: Placing fine strokes or small text in heavy screen-printed metallic deposits, where coarse pigment flakes clog the mesh and fill in tight negative space.
Parent guide Metallic Spot Inks