This choice changes with sheet weight, binding style, and cut geometry:
- Booklet covers (200–300 gsm): Rigid enough to carry bold flat spot UV accents on the front and back panels, provided the mask stops short of the spine fold or hinge score.
- Leaflets (80–120 gsm, 4/6/8 panels): Too thin and flexible for large solid UV coverage across folds or unlaminated lightweight stock; restrict spot UV to small, flat panel accents away from every crease.
- Postcards and dividers: Heavy cover or board stock holds flat spot UV well on the main face, while protruding divider tabs, die-cut edges, and writable postcard backs should stay free of UV.
- Stickers: Keep spot UV inside the kiss-cut perimeter so the die blade does not chip the cured gloss and peeling does not craze the surface.
Specifications and Clearance Limits
Stock Weight and Basis Size
Distinguish US Text LB from US Cover LB when specifying paper extras with manufacturing partners, because the two grades are weighed on different basis sheet sizes:
- US Text LB uses a 25 × 38 in (635 × 965 mm) basis sheet. Typical 80–120 gsm leaflet and booklet interior stocks sit in this range, measuring roughly 0.08–0.13 mm (0.003–0.005 in) per sheet.
- US Cover LB uses a 20 × 26 in (508 × 660 mm) basis sheet. Booklet covers (200–300 gsm), postcards, and heavy dividers sit in this range; for reference, 300 gsm art stock measures about 0.28–0.31 mm (0.011–0.012 in) before film lamination, and double-sided film adds 0.03–0.05 mm (0.001–0.002 in).
A heavier-sounding Text LB number is often much thinner than a lower Cover LB number, so always confirm both the gsm and target caliper before approving spot UV on paper extras.
Placement and Prepress Rules
| Component | Typical Stock | Binding / Cut Structure | Spot UV Placement Rule |
|---|---|---|---|
| Booklet covers | 200–300 gsm Cover | Saddle stitch (12–40 pp), perfect bind (28+ pp), or sewn (80–100+ pp) | Keep UV clear of the spine fold and hinge score; apply over matte or anti-scuff matte film. |
| Leaflets | 80–120 gsm Text | 4-, 6-, or 8-panel folded sheets | Restrict to small, flat panel elements; stop UV short of all fold lines to prevent cracking and spring-back. |
| Postcards | 300–400 gsm Cover | Guillotine trim or rounded corners | Apply to the laminated display side inside a 3 mm (0.118 in) trim safety margin; leave writable/address backs uncoated. |
| Dividers | 300–400 gsm Cover | Die-cut with protruding index tabs | Keep UV off the tab neck, flex points, and outer die-cut edge to prevent edge chipping during handling. |
| Stickers | Face stock + liner | Kiss-cut or die-cut on release liner | Inset UV inside the kiss-cut line so the cutting blade does not fracture or lift the gloss layer. |
Artwork and Prepress Setup
- File format: Supply press-ready AI, PDF, or PSD files exported to PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
- Spot UV layer: Place the flat spot UV mask on a dedicated, top-level spot color layer (100% solid vector shapes) knocked out or overprinted per the partner's prepress spec, never merged into the CMYK plates.
- Resolution and bleed: Keep raster artwork at ≥300 DPI with 3 mm (0.118 in) bleed per side on printed graphics, while pulling the spot UV mask back to respect at least a 3 mm (0.118 in) safety zone—or 4–5 mm (0.157–0.197 in) on bordered layouts where registration shift is more noticeable.
- Ink density and blacks: Set fine text to 100% K. For dark backgrounds under spot UV, use rich black (C40–60 M30–40 Y30–40 K100) with total area coverage (TAC) at ≤280%–300%, paired with anti-scuff matte lamination so dark areas do not scuff before or after UV curing.
Production Steps and Sign-Off Criteria
Specialist offset and tabletop manufacturing partners run flat spot UV as a post-press coating pass after ink drying and lamination:
- Offset CMYK printing: Print the flat press sheets for covers, postcards, dividers, leaflets, or sticker face stock and allow full ink drying so residual solvents do not interfere with film or UV adhesion.
- Base lamination (recommended for covers and dark artwork): Apply matte or anti-scuff matte BOPP/film lamination. Matte film creates high gloss-versus-matte contrast and stabilizes the sheet surface for uniform UV wetting.
- Spot UV application and curing: Apply the clear UV polymer via screen or digital UV head using the separate spot layer, then cure immediately under UV lamps.
- Scoring, folding, binding, or die-cutting:
- Score and fold booklet covers before binding (saddle stitch, perfect bind, or sewn).
- Score and fold 4/6/8-panel leaflets along the UV-free panel gaps.
- Guillotine-trim postcards or die-cut dividers and kiss-cut stickers after the UV layer is fully cured.
Sign-Off Criteria
Before approving a production run from press proofs or wet/digital samples:
- Registration check: Confirm the cured gloss aligns cleanly with underlying graphics and does not create visible haloing around fine 100% K text or thin rules.
- Flex and fold check: Open and close bound booklet covers and fold leaflets flat several times; the hinge and crease zones must show zero crazing, whitening, or flaking.
- Edge and kiss-cut check: Inspect trimmed postcard edges, divider tabs, and peeled stickers under angled light to verify the cutting blade has not chipped or lifted the UV edge.
- Surface integrity: Confirm dark rich-black areas under anti-scuff matte film show no rub marks or uneven gloss mottling.
Concrete Failure Modes
- Spine-hinge and fold cracking: Extending flat spot UV across a saddle-stitched spine, perfect-bound hinge score, or leaflet fold causes the rigid cured varnish to fracture into white craze lines and flake off after repeated opening.
- Trim-edge chipping and sticker edge lift: Running spot UV flush to a guillotine trim, divider die-cut, or sticker kiss-cut forces the steel blade through brittle cured polymer, leaving jagged, chipped edges or causing the UV layer to peel when a sticker is lifted from its liner.
- Registration haloing on fine details: Applying flat spot UV to hairline rules or small type magnifies normal mechanical sheet shift (0.5–1.0 mm / 0.020–0.039 in), making the gloss appear misaligned against the printed ink.
- Sheet curl and show-through on lightweight leaflets: Heavy flood or large solid spot UV blocks on unlaminated 80–120 gsm text stock cure with slight shrinkage, warping thin panels and causing uneven folding.
- Dark-artwork scuffing: Pairing high-TAC rich black with standard uncoated matte or unlaminated press varnish shows rub marks from sheet feeding and stacking around the glossy UV regions; use anti-scuff matte lamination underneath when dark backgrounds dominate.
Parent guide Flat Spot UV Coating