For general UV coating selection, curing behavior, and artwork setup across all printed components, see the flat and raised spot UV overview.
When to Keep Flat Spot UV vs. Knock It Out
Flat spot UV works best as a localized contrast layer over matte or anti-scuff matte film lamination on flat, non-flexing panels. Change the spot-varnish mask under any of these conditions:
- Artwork crosses a fold or score line: Knock out the spot UV channel across the entire crease channel and hinge zone on tuck boxes, folding boards, and GM screens.
- Artwork extends to a rigid box edge: Stop the spot UV mask on the face or side panel before the board edge rather than carrying it into the 15–20 mm (0.591–0.787 in) turn-in wrap margin.
- Dark or solid-ink backgrounds: Pair flat spot UV with anti-scuff matte lamination beneath the varnish so unvarnished background areas resist burnishing and the UV contrast stays distinct.
- Thin rules or small text: Avoid placing spot UV on fine hairlines or small body type where minor sheet-to-screen registration shift exposes an offset gloss halo.
Artwork and Structural Specifications
Flat spot UV on boxes and boards requires a dedicated spot-mask separation aligned to the structural dieline, plus adequate base-film compatibility and board tolerances.
| Parameter | Specification / Requirement | Production Purpose |
|---|---|---|
| Artwork Files | AI, PDF, or PSD; PDF/X-1a or PDF/X-4; outlined or embedded fonts | Ensures clean vector edges on the spot UV plate |
| Color & Spot Separation | CMYK print layers with a separate 100% vector spot UV layer | Isolates the UV mask from four-color process plates |
| Resolution & Bleed | ≥300 DPI for raster elements; 3 mm (0.118 in) bleed per side on CMYK | Prevents white edges after die-cutting or wrapping |
| Safety Margin | ≥3 mm (0.118 in) from trim and crease lines | Keeps key elements and UV edges clear of cut/fold stress |
| Black & Ink Limits | 100% K for fine text; rich black C40–60 M30–40 Y30–40 K100; TAC ≤280%–300% | Prevents ink set-off and improves UV adhesion over dark solids |
| Rigid Board Thickness | Greyboard 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in) | Determines corner turn-in radius and wrap tension |
| Rigid Wrap Margin | 15–20 mm (0.591–0.787 in) turn-in around greyboard edges | Secures the printed wrap inside the box without lifting |
| Minimum Order | Project and component minimums apply for boxed games and custom tooling | Tooling, dies, and wrap setups govern run economics |
Note on paper weights: When specifying wrap sheets or folding carton board, distinguish US Text LB (based on a 25 × 38 in basis sheet) from Cover LB (based on a 20 × 26 in basis sheet) alongside metric gsm so sheet stiffness and wrap foldability match the selected greyboard caliper.
Registration, Score-Line, and Wrap-Edge Rules by Component
Each structural format stresses the cured UV layer differently during finishing and use:
- Tuck Boxes (Folding Cartons): Tuck flaps, dust flaps, and side-seam glue flaps flex during assembly and every time the box opens. Keep flat spot UV strictly inside flat face and spine panels, pulled back from every crease score and perforation, and completely absent from glue flaps so adhesive bonds directly to paper or primed lamination.
- Rigid Box Wraps: Printed wraps are glued over 1.5–3 mm (0.059–0.118 in) greyboard and folded around 90-degree corners into the 15–20 mm (0.591–0.787 in) turn-in margin. Stop the spot UV mask short of the board fold lines on lids and bases; cured varnish folded over a sharp greyboard edge cracks along the corner seam and weakens wrap adhesion inside the rim.
- Folding Game Boards and GM Screens: Multi-panel boards and screens rely on wrapped paper hinges (often reinforced with cloth or heavy wrap stock) that flex repeatedly in play. Hold flat spot UV back from every panel gutter and wrap-edge turn-in, treating each panel face as an independent flat zone separated by the hinge clearance.
Production Steps and Sign-Off Criteria
- Dieline & Mask Alignment: Overlay the separate spot UV vector layer onto the approved structural dieline and verify clearances against all cut, score, crease, hinge, and wrap-turn lines.
- Prepress Trap & Registration Check: Confirm bold shapes rather than hairline strokes carry the UV mask so normal press-to-UV registration tolerance does not create visible misregistration.
- CMYK Printing & Base Lamination: Print CMYK sheets (with anti-scuff matte lamination applied where dark artwork requires rub protection) and allow ink and adhesive to stabilize before UV application.
- Spot UV Application & Curing: Apply the flat UV varnish through the dedicated screen or plate and cure under UV lamps.
- Die-Cutting, Creasing, or Wrapping: Cut and crease tuck boxes, or wrap and turn-in rigid boxes and folding boards.
- Physical Sign-Off Criteria: Inspect a folded, wrapped, or creased proof under angled light. Sign-off requires clean registration on focal graphics, zero cracking or white stress lines along any score or hinge after multiple flex cycles, and intact wrap adhesion along all 15–20 mm (0.591–0.787 in) turn-ins.
Concrete Failure Modes
- Varnish Flaking Along Creases and Hinges: Occurs when the spot UV mask crosses a score line or board gutter. As the board folds, the brittle cured film fractures and sheds flakes. Fix by knocking out the spot UV layer across the full crease channel and safety zone.
- Edge Lifting on Rigid Box Corners: Occurs when spot UV extends into the wrap turn-in zone over 1.5–3 mm (0.059–0.118 in) greyboard. The rigid varnish resists the 90-degree bend and pulls the paper wrap away from the board edge. Fix by stopping UV inside the flat panel face.
- Visible Registration Halo: Occurs when spot UV is assigned to thin rules, small type, or tight-fitting borders. Minor mechanical shift between the offset press sheet and the UV screen makes one edge look glossy while the opposite edge sits bare. Fix by restricting flat spot UV to bold shapes, logos, and background patterns with forgiving edge tolerances.
- Scuffing Around Unvarnished Matte Areas: Occurs on dark rich-black artwork when spot UV is applied over uncoated stock or standard soft matte film. Handling marks appear on the matte surround, reducing contrast. Fix by specifying anti-scuff matte lamination beneath the flat spot UV layer.
Parent guide Flat Spot UV Coating