These checks sit within Physical Handling Checks and establish whether the pack opens cleanly without damaging enclosed cards and hides card faces or backs from external light. The exact test emphasis shifts with the wrapper construction: metallized or white-backed film wrappers prioritize crimp-zone tear initiation and light-blocking ink coverage, whereas paper sleeves or belly-band wraps prioritize fold-line cracking, friction fit, and slip resistance.
Specifications and Prepress Clearances
Prototype mockups must match the actual production stack thickness and surface finish of the enclosed cards before wrapper or band dimensions are finalized:
- Card stack caliper: Build mockups using the target card stock rather than substitute paper. Approximate single-card calipers are 0.28–0.31 mm (0.011–0.012 in) for 300 gsm art/blue core, 0.30–0.32 mm (0.012–0.013 in) for 310 gsm black-core linen, 0.32–0.34 mm (0.013–0.0134 in) for 330 gsm black core, 0.34–0.38 mm (0.013–0.015 in) for 350 gsm art stock, 0.40–0.44 mm (0.016–0.017 in) for 400 gsm, and 0.30 mm (0.012 in) for PVC. Double-sided film lamination adds 0.03–0.05 mm (0.001–0.002 in) per card.
- Total stack height formula:
Stack height (mm) = Card count x (Single-card caliper + Lamination allowance). Multiply the total in mm by1 / 25.4for inches. - Belly-band and paper-wrap stock: Specify paper weight in gsm and distinguish US Text LB (25 x 38 in basis sheet) from Cover LB (20 x 26 in basis sheet). Lighter interior-grade sheets at 80–120 gsm (about 0.08–0.13 mm / 0.003–0.005 in per sheet, Text LB basis) conform around small card stacks with minimal spring-back, while 200–300 gsm cover stocks (Cover LB basis) hold shape for rigid bands and require scored creases to fold cleanly.
- Prepress and artwork zones: Supply artwork in AI, PDF, or PSD using PDF/X-1a or PDF/X-4 with outlined or embedded fonts, CMYK plus separate spot layers (such as opaque white underprint for film opacity or varnish/seal-zone knockouts), and >=300 DPI raster resolution. Include 3 mm (0.118 in) bleed per side and keep critical text, barcodes, and tear-line graphics at least 3 mm (0.118 in) inside trim and heat-seal edges (>=4–5 mm / 0.157–0.197 in for bordered backs). Use 100% K for fine text, rich black (C40–60 M30–40 Y30–40 K100) for dark solids, TAC <=280%–300%, and anti-scuff matte finishes on dark artwork.
- Conditional regulatory records: For packs distributed into regulated markets, keep material composition records for packaging participation under VerpackG, verify sorting-symbol placement against Triman / Info-tri rules where applicable, and coordinate EN 71 assessment and testing on the final film or paper packaging and enclosed game components when the product falls within toy-safety scope.
Prototype Checking Steps
- Assemble hand-sealed mockups at production stack height: Insert the exact card count using the production stock and finish so the wrapper tension, fin-seal slack, and belly-band circumference reflect real compression.
- Test tear-notch position and tamper-seal initiation: Pinch and tear at the notch using normal finger pressure without tools. Confirm the notch sits outside the welded heat-seal crimp and clear of the card corners.
- Trace pull-strip direction and opening ergonomics: Pull the tear strip across its full path. Observe whether the film or paper tracks straight across the top or back seam without veering into the card stack, catching on card edges, or requiring excessive force that bends the enclosed cards.
- Measure belly-band slip and retention: If the pack uses a paper belly band or inner wrap, shake and tilt the mockup and slide it in and out of a shipping carton or display tray. Verify that friction against the card finish holds the band centered without tearing the seam or letting cards slide free.
- Inspect wrapper opacity against bright light: Hold the sealed mockup directly in front of a bright inspection lamp or daylight window, rotating it across flat and angled views. Check the front, back, and side gussets to confirm card-back borders, dark ink blocks, foil stamps, or high-contrast faces do not show through the film or paper.
Sign-Off Criteria
Approve the prototype dimensions and artwork layout only when every mockup meets these conditions:
- Tear initiation: The tear notch opens on the first pull without stretching the film or delaminating the seal.
- Card protection: Opening the pack leaves zero nicks, creases, or corner bends on the outermost cards.
- Band retention: Any belly band or paper sleeve stays in position under normal handling and slides off only when pulled intentionally.
- Light blocking: Zero card-back graphics, text, or foil outlines are legible through the sealed wrapper under direct bright backlighting.
- Clearance integrity: Barcodes, legal marks, and critical typography remain readable and outside all heat-seal crimps and fold scores.
Failure Modes and Corrective Actions
| Failure Mode | Physical Cause | Corrective Action |
|---|---|---|
| Tear notch stretches instead of ripping | Notch cut inside the heat-seal weld or through thick laminated film without a score | Move the tear notch clear of the crimp line and align it with the film's tear direction |
| Pull strip veers into the card stack | Film orientation or paper grain runs perpendicular to the intended tear path | Reorient the wrapper grain/machine direction or add a perforated tear guide |
| Belly band slips off or binds tightly | Band circumference sized without lamination allowance, or wrong Text LB vs. Cover LB stiffness | Recalculate circumference from actual laminated stack height and adjust gsm/score lines |
| Card backs show through under bright light | Missing or thin opaque white spot layer on film, or low-opacity paper stock | Add or double-hit the opaque white spot underprint layer, or switch to metallized/higher-opacity stock |
| Ink cracks or scuffs along crimps and folds | TAC above 280%–300% or gloss dark solids rubbing during sealing and transit | Reduce TAC to <=280%–300%, apply anti-scuff matte finish, and keep ink out of heavy crimp zones |
Parent guide Physical Handling and Assembly Checks for Prototypes
Related guides
- Prototype Box Opening, Display, and Pack-Up Checks
- Booklet, Leaflet, and Scorepad Handling Checks on Prototypes
- Card Handling, Shuffling, and Border Checks on Prototypes