These checks sit within physical handling checks and depend on the board's structural format. Single-fold and quad-fold game boards require flat seating and crease alignment across wide spans, standing GM screens depend on panel balance and hinge stiffness at open angles, and dual-layer boards add die-cut registration and finger-access checks for recessed wells.
Specifications and Physical Allowances
Prototype boards built with Card Deck Press manufacturing partners use the following core, wrap, and prepress tolerances:
| Parameter | Specification |
|---|---|
| Greyboard core thickness | 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), 3 mm (0.118 in) |
| Wrap margin | 15–20 mm (0.591–0.787 in) |
| Bleed per side | 3 mm (0.118 in) |
| Safety margin (text and icons from edges/seams) | >= 3 mm (0.118 in) |
| Folded board box clearance (width and height) | 1.5–2.5 mm (0.059–0.098 in) |
| Folded board box clearance (stack height) | 1.5–3 mm (0.059–0.118 in) |
| Prepress files and resolution | AI/PDF/PSD exported as PDF/X-1a or PDF/X-4, >= 300 DPI, fonts outlined or embedded |
| Ink and black density | CMYK with separate spot layers, 100% K fine text, rich black C40–60 M30–40 Y30–40 K100, TAC <= 280%–300% |
| Surface protection for dark artwork | Anti-scuff matte lamination |
Prototype Check Steps and Sign-Off Criteria
Run these four checks on a full-scale, laminated physical mockup before approving production tooling or print runs:
- Verify folding sequence and box-fit clearance. Fold and unfold the board through its intended sequence (bi-fold, tri-fold, quad-fold, or accordion Z-fold) to confirm each hinge bends in the correct direction without forcing adjacent panels. Place the folded board into the prototype box with all other components to confirm 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) stack-height clearance.
- Inspect seam gutter clearance and crease visibility. Open the board under normal table lighting and examine every hinge seam. Confirm that track numbers, icons, and 100% K fine text sit outside the >= 3 mm (0.118 in) safety zone from fold gaps so characters do not split or sink into the crease. Check that wrapped edges (15–20 mm / 0.591–0.787 in wrap margin) and dark-ink creases with anti-scuff matte lamination remain intact after repeated folding without whitening or cracking.
- Test flat table seating and GM screen stability. For game boards, lay the opened board on a level surface and check that all panels rest flat without tenting at the center hinge or curling at the outer corners. For standing GM screens, open the panels to typical table angles and verify that the screen stands upright on its own without tipping backward, sliding, or bowing across outer wings.
- Check dual-layer pocket lift and die registration. Insert actual prototype tokens, tiles, or cards into every recessed pocket on a dual-layer board. Confirm that fingers or a die-cut thumb notch can lift each piece cleanly without prying against the top layer. Inspect the alignment of the top die-cut openings against printed borders and verify that narrow bridges between adjacent pockets stay firmly bonded to the base board.
Concrete Failure Modes
| Failure Mode | Physical Cause | Prototype Correction |
|---|---|---|
| Binding fold or bulging box lid | Hinges wrapped on the wrong face or folded stack exceeds 1.5–3 mm (0.059–0.118 in) box stack clearance | Re-specify inward/outward hinge order or step down greyboard thickness (e.g., from 3 mm / 0.118 in to 2 mm / 0.079 in) |
| Split icons or illegible text at seams | Artwork placed inside the fold gutter without >= 3 mm (0.118 in) seam clearance | Shift labels and grid markers clear of the hinge line or adjust panel breaks |
| Center tenting or tipping GM screen | Excess hinge tension, uneven wrap pull, or narrow wing proportions on standing screens | Balance inner/outer paper wrap tension, widen standing wing angles, or adjust board thickness |
| Trapped components in dual-layer pockets | Pocket walls cut tight to component size without a finger-lift notch | Add semicircular finger cutouts or widen pocket clearance so pieces lift without prying |
| Peeling bridges or cracked dark creases | Narrow top-layer bridges between cutouts delaminate, or > 280%–300% TAC ink cracks on the fold | Widen bridges between recessed wells, enforce TAC <= 280%–300%, and apply anti-scuff matte lamination |
Parent guide Physical Handling and Assembly Checks for Prototypes
Related guides
- Booklet, Leaflet, and Scorepad Handling Checks on Prototypes
- Booster Pack Opening and Opacity Checks on Prototypes
- Card Handling, Shuffling, and Border Checks on Prototypes
- Two-State Insert and Loose-Piece Storage Checks on Prototypes
- Punch-Out Token, Standee, and Dial Checks on Prototypes
- Puzzle Assembly and Paper-Extra Checks on Prototypes