These checks sit inside the broader physical handling checks sign-off stage and shift whenever the substrate caliper, double-sided film thickness, or board wrap changes.
Specifications and Tolerance Baselines
Prototype proxies must match the target board or heavyweight cardstock stack-up, including surface film, because lamination alters both friction and slot fit.
| Component or Parameter | Production Specification | Inch / Pound Equivalent | Prototype Check Implication |
|---|---|---|---|
| Greyboard core calipers | 1.5 / 2 / 2.5 / 3 mm | 0.059 / 0.079 / 0.098 / 0.118 in | Match exact target caliper for slot widths and punch-out force |
| Heavyweight cardstock (slotted parts) | 350 gsm (0.34–0.38 mm) / 400 gsm (0.40–0.44 mm) | 0.013–0.015 in / 0.016–0.017 in | Exceeds standard 200–300 gsm Cover stock (74–111 lb US Cover, 20 × 26 in basis) |
| Wrap / liner paper | 80–120 gsm (0.08–0.13 mm per sheet) | 0.003–0.005 in (approx. 54–81 lb US Text, 25 × 38 in basis) | Wrap margin requires 15–20 mm (0.591–0.787 in) for clean edge adhesion |
| Double-sided film addition | +0.03–0.05 mm per piece | +0.001–0.002 in per piece | Include film in slot-width math: slot width = laminated caliper |
| Punchboard die gap | 3–4 mm between cuts | 0.118–0.157 in | Prevents liner tearing and bridge collapse during ejection |
| Bleed and safety margins | 3 mm bleed; >=3 mm safety (>=4–5 mm bordered) | 0.118 in bleed; >=0.118 in safety (>=0.157–0.197 in) | Protects dial window numerals and token edges from die shift |
| Boxed stack clearance | 1.5–2.5 mm W/H; 1.5–3 mm stack height | 0.059–0.098 in W/H; 0.059–0.118 in height | Verify punchboard sheet stacks (typically 0.5–2.0 kg / 1.10–4.41 lb per tray) fit without bowing |
For print files feeding the prototype and production run, prepare CMYK artwork with separate spot layers at >=300 DPI in AI, PDF, or PSD format, exported as PDF/X-1a or PDF/X-4 with outlined or embedded fonts. Set fine dial text and small token labels to 100% K, use rich black (C40–60 M30–40 Y30–40 K100) with total area coverage (TAC) <=280%–300% on dark fills, and pair dark artwork with anti-scuff matte lamination to reduce handling marks during repeated assembly.
Job-Specific Prototype Checks
Build proxy pieces from the same greyboard caliper (1.5–3 mm / 0.059–0.118 in) or 350–400 gsm cardstock with double-sided film applied, rather than unlaminated dummy sheets.
Token Pickup Ergonomics
- Test surface pickup on flat and textured tables: Pick up small and thin tokens (especially 1.5 mm / 0.059 in greyboard) ten times in sequence to verify finger and nail purchase without sliding tokens to a table edge.
- Verify punch-out nick resistance: Push tokens out of a proxy sheet spaced with a 3–4 mm (0.118–0.157 in) die gap. Nicks should hold tokens flat in transit without requiring excessive thumb force that bends corners or tears the 80–120 gsm (54–81 lb US Text) wrap paper.
- Check edge cleanliness: Inspect the punched perimeter for hanging paper fibers or compressed crush lines along tight curves.
Standee Balance and Tip Resistance
- Measure slot-to-base friction: Seat the laminated standee foot into its proxy base slot. The joint must hold upright when lifted by the top edge without splitting the base wrap or deforming the standee tab.
- Test lateral tip stability: Place the assembled standee on a flat surface and lightly nudge the upper third of the figure. Top-heavy silhouettes on narrow bases or warped 1.5 mm (0.059 in) board will tip under minimal lateral force; widen the base footprint or step up to 2–2.5 mm (0.079–0.098 in) greyboard if tipping occurs.
- Check grain orientation: Verify that tall standees have their board grain running vertically to resist bowing along the height.
Double-Layer Dial Rotation and Window Legibility
- Check concentricity and rivet clearance: Spin the top dial layer 360 degrees five times around the center eyelet or plastic rivet. Rotation should stay smooth with uniform drag and zero binding against the outer rim.
- Verify window alignment across all stops: Read every value through the cut viewing window. Keep >=3 mm (0.118 in) safety between window die lines and printed numerals, or >=4–5 mm (0.157–0.197 in) if the window has a printed border.
- Check text contrast under film: Confirm 100% K fine text remains sharp through the window under overhead lighting when coated with anti-scuff matte film.
3D Slotted Assembly Rigidity
- Verify full-thickness slot fit: Assemble all interlocking walls using proxies that include the +0.03–0.05 mm (+0.001–0.002 in) double-sided film allowance (
slot width = base caliper + film thickness). - Test structural load and lift: Lift the assembled 3D piece by one side wall and rest a representative component load (for example, a 0.25–0.50 kg / 0.55–1.10 lb stack of tokens or cards, if the structure holds components) on top. Walls must stay square without tabs backing out or notches widening.
- Inspect repeated disassembly: Assemble and disassemble the slotted joints three times to confirm the 350–400 gsm cardstock or wrapped greyboard edges do not mushroom or delaminate.
Sign-Off Criteria and Regulatory Evidence
Approve the die drawing and prepress files only when all proxy checks meet these conditions:
- Tokens: Clean punch-out with intact wrap paper across a 3–4 mm (0.118–0.157 in) die gap and reliable finger pickup from a flat surface.
- Standees: Upright balance without lean, and firm tab-to-base retention when lifted.
- Dials: Full 360-degree rotation without catching, and unobstructed numeral legibility inside >=3 mm (0.118 in) window safety margins.
- Slotted 3D parts: Rigid, square interlocking joints that hold form under repeated assembly without liner splitting.
- Box fit: Stacked punchboard sheets clear the inner box walls by 1.5–2.5 mm (0.059–0.098 in) in width/height and 1.5–3 mm (0.059–0.118 in) in stack height.
Where punch-out tokens, standee tabs, or small dial fasteners fall into markets with toy-safety age grading, record material specifications and physical dimension checks for EN 71 assessment and testing in line with the European Commission Toy Safety framework before finalizing production tooling.
Concrete Failure Modes
- Wrap paper tearing during token punch-out: Caused by die gaps narrower than 3 mm (0.118 in) or oversized nicks that pull the 80–120 gsm (54–81 lb US Text) top sheet across adjacent cuts.
- Standee tab crushing or loose wobble: Caused by designing base slots to the bare greyboard caliper (such as 2 mm / 0.079 in) without accounting for the +0.03–0.05 mm (+0.001–0.002 in) double-sided film thickness or wrap overlap.
- Clipped dial numbers: Caused by placing dial typography inside the 3 mm (0.118 in) safety zone around the cut window, where normal die registration variance shifts the aperture over the text.
- 3D slot delamination on first assembly: Caused by cutting notches too tight for 350–400 gsm (0.34–0.44 mm / 0.013–0.017 in) laminated cardstock or routing slots parallel to weak paper grain without a clean entry chamfer.
Parent guide Physical Handling and Assembly Checks for Prototypes
Related guides
- Booklet, Leaflet, and Scorepad Handling Checks on Prototypes
- Booster Pack Opening and Opacity Checks on Prototypes
- Card Handling, Shuffling, and Border Checks on Prototypes
- Board Folding, Seam, and Dual-Layer Checks on Prototypes
- Two-State Insert and Loose-Piece Storage Checks on Prototypes
- Puzzle Assembly and Paper-Extra Checks on Prototypes