Why Text lb and Cover lb Differ for the Same GSM
Metric gsm (grams per square meter) measures the mass of a 1 x 1 m (39.37 x 39.37 in) sheet regardless of paper grade. US basis weight (lb) measures the mass of one 500-sheet ream cut to that paper grade's standard uncut parent sheet size:
- US Text (Book) basis sheet: 25 x 38 in (635 x 965.2 mm), or 950 sq in per sheet.
- US Cover basis sheet: 20 x 26 in (508 x 660.4 mm), or 520 sq in per sheet.
Because a Text parent sheet has 1.827 times the surface area of a Cover parent sheet, the same 300 gsm paper weighs roughly 203 lb (92.1 kg) per 500-sheet Text ream versus 111 lb (50.3 kg) per 500-sheet Cover ream.
Plain-Text Conversion Formulas
Use these direct formulas to convert between metric gsm, US basis weight (lb), and ream mass (kg):
US Text lb = gsm * 0.6756
gsm = US Text lb * 1.4801
US Cover lb = gsm * 0.3698
gsm = US Cover lb * 2.7041
General 500-sheet ream formula (any basis sheet size):
lb = gsm * (width_in * height_in * 0.0007112)
kg = lb * 0.4536
GSM, US Basis Weight, and Card Caliper Reference
Standard offset card runs start at 200 decks (usual tiers 200, 300, 500, and 1,000+ decks). Use the table below to map metric gsm to the matching US grade, 500-sheet ream weight, and typical uncoated/coated base caliper before surface film is applied:
| Stock Application | Metric GSM | US Grade & Basis Weight | 500-Sheet Ream Mass | Typical Base Caliper (mm / in) |
|---|---|---|---|---|
| Booklet interior | 80 gsm | 54 lb Text | 54 lb / 24.5 kg | 0.08–0.13 mm (0.0031–0.0051 in) |
| Booklet interior | 100 gsm | 68 lb Text | 68 lb / 30.8 kg | 0.08–0.13 mm (0.0031–0.0051 in) |
| Booklet interior | 120 gsm | 81 lb Text | 81 lb / 36.7 kg | 0.08–0.13 mm (0.0031–0.0051 in) |
| Booklet cover | 200 gsm | 74 lb Cover | 74 lb / 33.6 kg | — |
| Card / booklet cover (art or blue core) | 300 gsm | 111 lb Cover | 111 lb / 50.3 kg | 0.28–0.31 mm (0.0110–0.0122 in) |
| Card stock (black-core linen) | 310 gsm | 115 lb Cover | 115 lb / 52.2 kg | 0.30–0.32 mm (0.0118–0.0126 in) |
| Card stock (black core) | 330 gsm | 122 lb Cover | 122 lb / 55.3 kg | 0.32–0.34 mm (0.0126–0.0134 in) |
| Card stock (art stock) | 350 gsm | 129 lb Cover | 129 lb / 58.5 kg | 0.34–0.38 mm (0.0134–0.0150 in) |
| Heavy card stock | 400 gsm | 148 lb Cover | 148 lb / 67.1 kg | 0.40–0.44 mm (0.0157–0.0173 in) |
| Plastic card stock (PVC) | — | — | — | 0.30 mm (0.0118 in) |
Note on surface film: Double-sided lamination adds 0.03–0.05 mm (0.0012–0.0020 in) per card to the finished caliper without changing the base paper's gsm rating.
Job-Specific Calculation and Specifying Steps
- Match the grade to the component: Use Text lb (25 x 38 in / 635 x 965.2 mm) only for 80–120 gsm booklet interiors; use Cover lb (20 x 26 in / 508 x 660.4 mm) for 200–300 gsm booklet covers and 300–400 gsm card stocks.
- Convert US pound specs to gsm: Multiply Cover lb by 2.7041 (or Text lb by 1.4801) so mill and offset print specifications use an unambiguous metric weight.
- Calculate finished card caliper: Take the base stock caliper in mm (in) and add 0.03–0.05 mm (0.0012–0.0020 in) if the card receives double-sided film lamination.
- Size the box cavity from stacked caliper: Multiply the finished single-card caliper by the deck card count, then add 1.5–3 mm (0.059–0.118 in) of box clearance for stack height (alongside 1.5–2.5 mm / 0.059–0.098 in clearance across card width and height).
Sign-Off Criteria
- Production spec lists both metric gsm and the explicit US grade and basis size (e.g., 300 gsm / 111 lb Cover), never an unlabeled pound number.
- Target finished card caliper is stated in mm and in, accounting for core type, coating, and any 0.03–0.05 mm (0.0012–0.0020 in) double-sided film.
- Box internal depth matches
(finished card caliper x card count) + 1.5–3 mm (0.059–0.118 in)clearance.
Concrete Failure Modes
- Omitting the Text or Cover grade label: Specifying "110 lb" without "Cover" can be interpreted as 110 lb Text (~163 gsm), producing a thin, translucent sheet instead of ~298–300 gsm card stock.
- Sizing boxes from gsm instead of caliper: Two 300–350 gsm stocks with different pulp density, core layers, or coatings can differ by 0.03–0.04 mm (0.0012–0.0016 in) per card, shifting a 100-card deck by 3–4 mm (0.118–0.157 in) and exceeding the 1.5–3 mm (0.059–0.118 in) box stack-height clearance.
- Ignoring lamination thickness in stack height: Double-sided film adds 0.03–0.05 mm (0.0012–0.0020 in) per card; across a 100-card deck, that adds 3–5 mm (0.118–0.197 in) to stack height and causes tight or bulging tuck boxes if omitted from the cavity calculation.
Parent guide Card Stocks and Paper Core Construction