Choose 310 gsm black-core linen stock when frequent shuffling, fan handling, and opaque card backs are the priority on offset runs starting at 200 decks (usual production tiers: 200, 300, 500, and 1,000+ decks). Switch to smooth art or unembossed core grades in the card stock specifications when designs rely on ultra-fine typography, heavy film lamination, or gilded edges.

Weight, Caliper, and Stack Loft Specifications

Card stock weight is specified in grams per square meter (gsm) rather than US pound ratings because US pound weights vary by basis sheet size. US Cover LB measures 500 sheets at 20 x 26 in (508 x 660.4 mm), whereas US Text LB measures 500 sheets at 25 x 38 in (635 x 965.2 mm). In metric-imperial sheet mass terms, 310 gsm equals 0.310 kg (0.683 lb) per square meter, and 330 gsm equals 0.330 kg (0.728 lb) per square meter.

Stock Grade Nominal Weight Base Caliper (mm) Base Caliper (in) Surface & Core Profile
Black-core linen 310 gsm (0.310 kg/m² / 0.683 lb/m²) 0.30–0.32 mm 0.0118–0.0126 in Embossed air-cushion texture; opaque black center
Black-core smooth (reference) 330 gsm (0.330 kg/m² / 0.728 lb/m²) 0.32–0.34 mm 0.0126–0.0134 in Smooth surface; higher stiffness and rigidity
Art / blue core (reference) 300 gsm (0.300 kg/m² / 0.661 lb/m²) 0.28–0.31 mm 0.0110–0.0122 in Smooth surface; lighter snap and opacity
Double-sided film allowance Added finish layer +0.03–0.05 mm +0.0012–0.0020 in Added per card when film lamination is applied

Mechanical embossing displaces paper fibers into peaks and valleys, increasing effective deck height beyond the raw unembossed sheet caliper. Calculate total deck height before finalizing packaging dimensions:

Stack height (mm) = (Card count * Single-card caliper in mm) + Emboss loft allowance

Stack height (in) = Stack height (mm) / 25.4

For any deck format, confirm the finished deck stack height physically before cutting boxes, because uncompensated emboss loft can bind inside rigid or tuck packaging. Packaging requires 1.5–2.5 mm (0.059–0.098 in) clearance across card width and height and 1.5–3 mm (0.059–0.118 in) clearance for stack height.

Coating, Surface, and Prepress Compatibility

Embossed micro-valleys change how coatings, inks, and fine details behave on press:

  • Varnish vs. film lamination: Aqueous or UV card varnishes conform to the embossed valleys and preserve air-cushion shuffle glide. Double-sided film lamination adds 0.03–0.05 mm (0.0012–0.0020 in) per card and bridges across embossed valleys, reducing surface air pockets and risking delamination if embossed deeply after lamination.
  • Dark artwork and edge finishes: Anti-scuff matte finishes suit dark artwork by reducing rub marks during handling. Thick lamination conflicts with gilded edges and should be avoided when metallic edge gilding is specified.
  • Small-type legibility: Embossed valleys break up hairline strokes and reversed-out micro-text. Set fine text in 100% K rather than multi-plate builds so minor registration shifts do not blur characters across the texture.
  • Color and file setup: Supply print-ready AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 with outlined or embedded fonts, CMYK color at ≥300 DPI, and separate spot layers where required. Use rich black C40–60 M30–40 Y30–40 K100 for solid dark areas while keeping total area coverage (TAC) at ≤280%–300%.
  • Bleed, safety, and corners: Include 3 mm (0.118 in) bleed per side, ≥3 mm (0.118 in) safety margin (increased to ≥4–5 mm / 0.157–0.197 in for bordered backs), and R3–R3.5 mm (R0.118–R0.138 in) corner radii.

Job-Specific Production Steps and Sign-Off Criteria

Specialist offset manufacturing partners execute linen-textured decks in a fixed sequence so embossing does not distort ink laydown or die-cut registration:

  1. Prepress check: Verify PDF/X-1a or PDF/X-4 files, ≥300 DPI resolution, 3 mm (0.118 in) bleed, ≥3 mm (0.118 in) or ≥4–5 mm (0.157–0.197 in) safety margins, 100% K fine text, and TAC ≤280%–300%.
  2. Offset printing: Print sheet fronts and backs on 310 to 330 gsm black-core board.
  3. Surface coating: Apply protective varnish (or anti-scuff matte for dark solids) and cure fully before mechanical texturing.
  4. Linen embossing: Pass coated press sheets through matched steel embossing rollers to press uniform micro-valleys across both faces.
  5. Die-cutting and cornering: Slit sheets into strips, punch individual cards with R3–R3.5 mm (R0.118–R0.138 in) rounded corners, and collate decks.
  6. Stack and box fit check: Measure finished deck stack height against the 1.5–3 mm (0.059–0.118 in) height clearance before sealing packaging runs.

Production Sign-Off Criteria

  • Single-card caliper measures within 0.30–0.32 mm (0.0118–0.0126 in) for 310 gsm black-core linen or 0.32–0.34 mm (0.0126–0.0134 in) for 330 gsm black core.
  • Embossing depth is uniform across the sheet with no crushed borders or flat spots.
  • Fine 100% K text remains readable across the micro-valleys without broken hairlines.
  • Bordered backs stay centered within the ≥4–5 mm (0.157–0.197 in) safety zone.
  • Deck stack height clears the box interior within the 1.5–3 mm (0.059–0.118 in) allowance.

Concrete Failure Modes

Failure Mode Physical Cause Corrective Action
Film silvering or peeling Thick film lamination bridges over embossed micro-valleys instead of bonding into them Use card varnish over linen embossing, or switch to unembossed stock for heavy film lamination
Broken or fuzzy small text Hairline strokes and multi-ink text sit across embossed peaks and valleys Set fine text to 100% K and avoid ultra-thin serifs or reversed micro-type
Tight or bulging card box Box height uses raw unembossed caliper without accounting for emboss loft Measure pressed deck stack height and maintain 1.5–3 mm (0.059–0.118 in) stack clearance
Scuffing on dark card backs High-ink dark solids rub during embossing and collation Specify anti-scuff matte finish and keep TAC ≤280%–300%
Gilded-edge delamination Thick lamination resists metallic edge foil adhesion Omit thick film lamination when gilded edges are specified