Rigid PVC Specifications and Caliper Comparison

Unlike paper card stocks—which are specified by grammage (gsm) and distinguished in North America between US Text LB (based on a 25 x 38 in basis sheet) and US Cover LB (based on a 20 x 26 in basis sheet)—rigid PVC is a non-fibrous synthetic sheet specified by thickness (caliper). Standard offset card runs with specialist manufacturing partners start at 200 decks, with typical volume tiers at 200, 300, 500, and 1,000+ decks.

Stock Type Nominal Caliper (mm) Nominal Caliper (in) Core / Material Construction Key Production Constraint
Rigid PVC 0.30 mm 0.012 in Solid waterproof synthetic PVC UV-curable inks, static control, < 55 C (131 F), rounded corners
300 gsm Art / Blue Core 0.28–0.31 mm 0.011–0.012 in Coated paper with blue adhesive core Fiber-based; absorbs moisture without lamination
310 gsm Black-Core Linen 0.30–0.32 mm 0.012–0.013 in Textured paper with opaque black core Embossed linen texture; paper edge wear
330 gsm Black Core 0.32–0.34 mm 0.013 in Smooth paper with opaque black core Standard opaque paper snap; requires coating
350 gsm Art Stock 0.34–0.38 mm 0.013–0.015 in Heavyweight coated art paper Higher stiffness; less flexible for riffling
400 gsm Art Stock 0.40–0.44 mm 0.016–0.017 in Extra-heavyweight coated art paper Thickest standard paper tier; rigid handling

Note: Adding double-sided protective film lamination adds 0.03–0.05 mm (0.001–0.002 in) per card to total caliper.

Prepress and Edge Specifications

  • File formats and color: Supply print-ready AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 with outlined or embedded fonts, >= 300 DPI raster resolution, and CMYK color with separate spot layers where needed.
  • Black and ink limits: Use 100% K for fine text, rich black (C40–60 M30–40 Y30–40 K100) for large dark solids, and keep Total Area Coverage (TAC) at <= 280%–300%.
  • Bleed, safety, and corners: Include 3 mm (0.118 in) bleed per side, >= 3 mm (0.118 in) safety margin (>= 4–5 mm / 0.157–0.197 in for bordered card backs), and R3–R3.5 mm (0.118–0.138 in) corner radii.
  • Deck format sizing: Apply the exact assigned trim dimensions for the project rather than a generic default; non-standard deck proportions follow custom die-line geometry while keeping the same bleed, safety, and corner-radius rules.

Production Steps for Rigid PVC Cards

  1. Prepress Separation and Ink Limiting: Verify PDF/X-1a or PDF/X-4 compliance, confirm TAC <= 280%–300%, and separate any spot varnish or anti-scuff matte layers from the CMYK artwork.
  2. Sheet De-Ionization and Static Control: Condition PVC sheets with active static control prior to press feeding so smooth, non-conductive plastic surfaces separate cleanly without double-feeding or sheet cling.
  3. UV-Curable Ink Printing and Surface Coating: Print with UV-curable inks that polymerize immediately under UV lamps on non-absorbent plastic. Apply anti-scuff matte coating for dark artwork to reduce visible surface scratching; avoid thick film lamination if gilded edges are specified, as thick film conflicts with edge gilding adhesion.
  4. Thermal Control and Die-Cutting: Maintain press, curing, and post-press stacking temperatures strictly below 55 C (131 F) to prevent plastic softening or permanent curl. Die-cut cards with R3–R3.5 mm (0.118–0.138 in) rounded corners to remove sharp square plastic points.

Sign-Off Criteria

  • Caliper and flatness: Finished cards measure 0.30 mm (0.012 in) nominal thickness (plus 0.03–0.05 mm / 0.001–0.002 in if double-sided film is applied) and lie flat without thermal warp from exceeding 55 C (131 F).
  • Ink cure and registration: UV-cured ink layers show full surface polymerization without smearing, and front-to-back registration holds within the 3 mm (0.118 in) bleed and >= 3 mm (0.118 in) safety zone (>= 4–5 mm / 0.157–0.197 in on bordered backs).
  • Edge and corner finish: Die-cut edges are smooth and free of plastic burrs, with uniform R3–R3.5 mm (0.118–0.138 in) rounded corners.
  • Regulatory documentation (when applicable): If the deck is intended as a children's product or toy in regulated markets, maintain applicable EN 71 assessment and testing records aligned with the EU Toy Safety framework prior to market placement.

Failure Modes and Prevention

Failure Mode Physical Cause Prevention Rule
Ink smearing or flaking Conventional oil-based offset inks cannot absorb into non-porous PVC Use UV-curable inks and cap TAC at <= 280%–300%
Double-feeding and misregistration Electrostatic charge builds up between smooth synthetic sheets Run active static control during sheet feeding and collation
Sheet warping or curl Press, UV lamp, or storage heat reaches or exceeds 55 C (131 F) Enforce < 55 C (131 F) thermal limits across curing and storage
Sharp corner snagging and splitting Square 90-degree cuts on rigid 0.30 mm (0.012 in) plastic leave hard tips Die-cut all rigid PVC decks with R3–R3.5 mm (0.118–0.138 in) corners
Dark-art scuffing or gilding failure Unprotected dark ink shows friction marks; thick film rejects gilding Specify anti-scuff matte on dark art; omit thick lamination on gilded edges