Specifications & Material Grades
Single-ply C2S art stock is manufactured from bleached chemical pulp with clay/mineral coatings applied to both faces and no internal black or blue adhesive barrier. Because the sheet is a single continuous ply, it delivers higher bending stiffness per gram than multi-ply cored boards of the same nominal gsm, while keeping surface smoothness high for four-color offset reproduction.
Caliper, Basis Weight, and Lamination Add-On
When specifying weight in North American units, distinguish US Cover LB (20 × 26 in / 508 × 660 mm basis sheet) from US Text LB (25 × 38 in / 635 × 965 mm basis sheet). Card stocks are always specified in Cover LB rather than Text LB, because a 200 lb Text sheet is roughly equivalent to a 110 lb Cover sheet (approx. 300 gsm).
| Grade (gsm) | US Cover LB (20 × 26 in / 508 × 660 mm) | US Text LB Equivalent (25 × 38 in / 635 × 965 mm) | Unlaminated Caliper | Double-Sided Film Add-On | Finished Caliper Range | Primary Structural Profile |
|---|---|---|---|---|---|---|
| 300 gsm | ~111 lb Cover (50.3 kg / 111 lb per 500 basis sheets) | ~203 lb Text | 0.28–0.31 mm (0.011–0.012 in) | +0.03–0.05 mm (0.0012–0.0020 in) | 0.31–0.36 mm (0.012–0.014 in) | Flexible snap, standard light-duty decks |
| 350 gsm | ~129 lb Cover (58.5 kg / 129 lb per 500 basis sheets) | ~237 lb Text | 0.34–0.38 mm (0.013–0.015 in) | +0.03–0.05 mm (0.0012–0.0020 in) | 0.37–0.43 mm (0.015–0.017 in) | Firm hand feel, reduced flex, heavier stack |
| 400 gsm | ~148 lb Cover (67.1 kg / 148 lb per 500 basis sheets) | ~270 lb Text | 0.40–0.44 mm (0.016–0.017 in) | +0.03–0.05 mm (0.0012–0.0020 in) | 0.43–0.49 mm (0.017–0.019 in) | Semi-rigid board feel, minimal bend/shuffle flex |
Plain-text basis weight conversion:
gsm = (Cover LB × 453.592) / 167.74
gsm = (Text LB × 453.592) / 306.45
Stiffness, Opacity, and Surface Finishing
- Stiffness vs. Shuffleability: Solid C2S board resists bending more than black-core or blue-core boards at equal gsm because it has no soft internal glue line. At 350–400 gsm, cards resist riffle shuffling and are best suited for placement tiles, reference cards, or overhand-shuffled decks.
- Opacity Limits: Without an internal opaque core, light passes through solid bleached pulp. Under direct overhead or backlit conditions, heavy dark ink areas on one face can cast a faint silhouette visible from the opposite face.
- Lamination & Coating Selection:
- Varnish / Aqueous Coating: Adds negligible thickness (<0.01 mm / <0.0004 in) and preserves natural paper snap, but offers lower abrasion resistance on dark full-bleed artwork.
- Matte or Gloss Film Lamination: Adds 0.03–0.05 mm (0.0012–0.0020 in) per card across both sides, increases tear resistance, and protects dark solids. Use anti-scuff matte lamination when cards feature dark backgrounds or heavy rich black coverage.
- Edge Gilding Compatibility: Thick film lamination (0.03–0.05 mm / 0.0012–0.0020 in total) can conflict with gilded edges, as foil adhesion weakens along laminated film lips during trimming and rounding.
Production Steps & Sign-Off Criteria
Standard offset card runs start at 200 decks (typical production tiers: 200, 300, 500, 1,000+ decks) through specialist offset manufacturing partners.
1. Prepress & File Setup
- File Formats: Submit print-ready AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
- Color & Ink Density: Use CMYK with separate spot layers for foil or spot UV. Set fine text to 100% K (no four-color black) and large dark solids to rich black (C40–60 M30–40 Y30–40 K100), keeping Total Area Coverage (TAC) at ≤280%–300%.
- Bleed, Safety & Corners: Provide ≥300 DPI raster resolution, 3 mm (0.118 in) bleed per side, ≥3 mm (0.118 in) inner safety margin (increase to ≥4–5 mm / 0.157–0.197 in for bordered card backs), and R3–R3.5 mm (R0.118–R0.138 in) corner radius specifications where rounded corners are used.
2. Offset Printing & Surface Curing
- Sheet Conditioning & Press Run: Print CMYK and spot passes onto acclimated C2S press sheets. Because coated art stock is non-absorbent compared to uncoated board, allow full ink setting before stacking or coating to prevent set-off.
- Coating / Lamination Application: Apply aqueous varnish or double-sided BOPP film lamination (matte, anti-scuff matte, or gloss). Verify film bond before cutting; uncured adhesive causes edge delamination under the die.
3. Die-Cutting, Corner Rounding & Stack Verification
- Cutting & Rounding: Trim press sheets to the specified card format and round corners to R3–R3.5 mm (R0.118–R0.138 in) as specified.
- Stack Height & Box Fit: Calculate finished deck height using the laminated caliper (
Finished Caliper × Card Count). Verify box internals maintain 1.5–2.5 mm (0.059–0.098 in) clearance across card width and height, and 1.5–3 mm (0.059–0.118 in) clearance for total stack height.
Sign-Off Criteria
- Caliper Check: Micrometer readings across sampled cards fall within the target grade's laminated or unlaminated range (e.g., 0.31–0.36 mm / 0.012–0.014 in for laminated 300 gsm).
- Ink & Registration: Fine 100% K text shows no color haloing; bordered backs remain centered within tolerance inside the ≥4–5 mm (0.157–0.197 in) safety zone.
- Edge & Coating Integrity: Die-cut edges and R3–R3.5 mm (R0.118–R0.138 in) corners show no coating cracking, film peeling, or ink flaking.
- Packaging Fit: Completed deck slides into its box with 1.5–2.5 mm (0.059–0.098 in) lateral clearance and 1.5–3 mm (0.059–0.118 in) stack-height clearance without bowing the lid or crushing card edges.
Concrete Failure Modes
- Backlighting Show-Through: Using 300–350 gsm C2S solid board for hidden-role or competitive games played under strong overhead or window light allows high-contrast face art to ghost through the card back. Fix: Switch to a black-core or blue-core stock when opacity is critical.
- Edge Cracking on Thick Unlaminated Grades: Printing dark rich-black solids to the bleed edge on 350–400 gsm C2S without film lamination causes the brittle clay coating to chip along the cut line during die-cutting and play. Fix: Apply anti-scuff matte or gloss lamination to bridge and seal the cut edge.
- Gilded Edge Delamination: Combining thick double-sided film lamination (+0.03–0.05 mm / 0.0012–0.0020 in) with metallic edge gilding prevents uniform foil bonding along the card perimeter, causing flaking after minimal handling. Fix: Use unlaminated varnish or thin-profile finishing when edge gilding is specified.
- Scuffing on Dark Artwork: Standard matte varnish or standard matte film shows glossy burnish marks and white scuff lines quickly on dark solid C2S cards. Fix: Specify anti-scuff matte lamination and keep TAC ≤280%–300%.
- Box Crush from Lamination Stack Growth: Designing a rigid box or tuck box around unlaminated 350 gsm caliper (0.34–0.38 mm / 0.013–0.015 in) and later adding double-sided film (+0.03–0.05 mm / 0.0012–0.0020 in per card) adds 1.8–3.0 mm (0.071–0.118 in) to a 60-card deck, eliminating the required 1.5–3 mm (0.059–0.118 in) stack-height clearance. Fix: Lock lamination specs before finalizing box dielines.
Parent guide Card Stocks and Paper Core Construction