When the board thickness changes:

  • 1.5 mm (0.059 in) greyboard: Suits compact, single-sided tiles or high-count sets where lower stack height and weight matter most, though thinner cores cup more easily if front and back surface tension are not balanced.
  • 2.0 mm (0.079 in) greyboard: Standard choice for most modular terrain and double-sided map grids, balancing rigidity, clean steel-rule cuts, and box stack height.
  • 2.5 mm (0.098 in) greyboard: Better for large-format map sections or heavily handled tiles that need extra mass and stiffness to stay flat when pushed together on the table.
  • 3.0 mm (0.118 in) greyboard: Increases edge compression and blade-entry bevels during die cutting, which can leave wider visible seams between adjacent tiles unless die geometry and press depth are tightly controlled.

For broader board-core and die-cut sheet options across punchboard components, see punchboard structures.

Structural and Prepress Specifications

Parameter Specification Notes
Greyboard core 2.0 mm (0.079 in) or 2.5 mm (0.098 in) 1.5 mm (0.059 in) for compact sets; 3.0 mm (0.118 in) for maximum rigidity
Punchboard die gap 3–4 mm (0.118–0.157 in) Minimum waste bridge between adjacent tiles on the sheet
Wrap margin (wrapped boards) 15–20 mm (0.591–0.787 in) Applies when edges are wrapped rather than flush die-cut
Bleed 3 mm (0.118 in) per side Extends map artwork past the die line
Safety margin ≥3 mm (0.118 in) Keeps grid markers, walls, and borders clear of cut edges
Box / tray clearance 1.5–2.5 mm (0.059–0.098 in) width/height; 1.5–3 mm (0.059–0.118 in) stack height Prevents tight stacks from binding or bowing corners
Prepress files AI / PDF / PSD (PDF/X-1a or PDF/X-4) Fonts outlined or embedded; CMYK with separate spot layers; ≥300 DPI
Ink and black density 100% K fine text; rich black C40–60 M30–40 Y30–40 K100 Total area coverage (TAC) ≤280%–300%
Surface finish Anti-scuff matte lamination Reduces table glare and protects dark map artwork from abrasion

Printed facing and backing sheets are specified in gsm; if US basis weights are referenced, distinguish Text LB (25 × 38 in basis sheet) from Cover LB (20 × 26 in basis sheet) so liner thickness stays matched on both faces. Custom die tooling and boxed-game runs follow project and component minimums with specialist tabletop manufacturing partners.

Production Steps

  1. Impose sheets with consistent grain and die gaps: Arrange tiles across the punchboard sheet with a 3–4 mm (0.118–0.157 in) die gap between pieces. Align greyboard and liner grain in the same direction across all sheets so any ambient moisture movement acts uniformly rather than twisting individual tiles out of square.
  2. Print and balance both faces: Print facing and backing sheets at ≥300 DPI in CMYK (with separate spot layers where needed) and 3 mm (0.118 in) bleed. Apply matching lamination—such as anti-scuff matte on dark map art—to both sides before mounting so surface tension pulls equally on front and back.
  3. Mount and cure flat under load: Laminate the printed liners to the greyboard core with even adhesive coverage, then stack and press the mounted sheets under flat weight while moisture dissipates.
  4. Die-cut with bevel control: Cut sheets with calibrated steel-rule dies from the primary face side. Sharp rules, firm ejection rubber, and controlled press depth keep the blade-entry compression bevel narrow so tiles meet cleanly along straight seams.
  5. Place minimal nicks away from key seams: Position small, evenly spaced nicks along non-critical edges—or avoid straight butt-joint edges where possible—so tiles stay retained in the punchboard frame during transit without leaving proud burrs after punching.

Sign-Off Criteria

  • Flatness: Every tile rests flat on a level surface on both faces with no corner lift or rocking.
  • Dimensional consistency: Outer tile dimensions and corner angles match across all punchboard frames so multi-tile grids align without cumulative drift.
  • Clean butt edges: Cut edges show minimal die-entry bevel, no crushed greyboard fibers, no liner delamination, and no proud nick burrs holding tiles apart.
  • Artwork registration: Cut lines fall cleanly inside the 3 mm (0.118 in) bleed with no white paper slivers or clipped ≥3 mm (0.118 in) safety elements.
  • Box fit: Stacked tiles clear the box or insert walls by 1.5–2.5 mm (0.059–0.098 in) in width/height and 1.5–3 mm (0.059–0.118 in) in stack height.

Failure Modes

  • Cupping and edge lift: Lamination on only one side, mismatched liner weights, or opposing grain directions pull the greyboard toward the tighter face and prevent adjacent tiles from sitting flush.
  • V-shaped gaps between tiles: Dull steel-rule knives, overly soft cutting pads, or 3.0 mm (0.118 in) board cut without adjusted press depth crush the entry edge inward, creating visible seams where tiles meet.
  • Proud burrs holding seams open: Heavy or poorly placed nicks along straight butt-joint edges tear the greyboard core when punched, leaving nubs that push neighboring tiles out of line.
  • Cumulative grid drift: Slight variations in die wear, sheet distortion, or press pressure across different punchboard frames compound into noticeable alignment offsets across multi-tile layouts.
  • Crushed tile walls: Narrowing the punchboard die gap below 3–4 mm (0.118–0.157 in) compresses the waste bridge during cutting, deforming tile edges or tearing the surface wrap.