The concrete choice comes down to matching the interlocking slot width and fold score profile to the finished board stack rather than the raw core:
- Core stiffness vs. slot depth: Thicker greyboard—2.5 mm (0.098 in) or 3 mm (0.118 in)—provides rigid vertical walls for tall structures, while 1.5 mm (0.059 in) or 2 mm (0.079 in) suits smaller stands and angled tabs.
- One-time assembly vs. repeated teardown: Tighter slot tolerances hold permanent displays rigid, whereas components assembled and packed flat between uses require slightly more clearance to prevent edge crushing and liner peeling.
- Liner and finish buildup: Mounted facing paper, adhesive, and protective film add measurable thickness to the core, changing the required slot width in the cutting die.
Specifications and Caliper Sizing
Slot-together parts are die-cut from greyboard laminated on both sides with printed paper sheets. Always calculate slot widths from the finished, laminated caliper:
Finished Caliper = Greyboard Core + Front Facing + Back Facing + Adhesive + Film
| Parameter | Specification | Notes |
|---|---|---|
| Greyboard core options | 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), 3 mm (0.118 in) | Selected for structural span and load |
| Facing paper weight | Measured in gsm; distinguish US Text LB (25 × 38 in basis sheet) from Cover LB (20 × 26 in basis sheet) | Lighter text-weight liners (e.g., 80–120 gsm) wrap and score with less cracking |
| Film lamination | Double-sided film adds 0.03–0.05 mm (0.001–0.002 in) | Anti-scuff matte suits dark artwork |
| Punchboard die gap | 3–4 mm (0.118–0.157 in) | Minimum clearance between adjacent parts on the sheet |
| Bleed and safety | 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) safety | Safety applies to outer edges and internal slot cutouts |
| Prepress files | AI, PDF, or PSD; PDF/X-1a or PDF/X-4 | Fonts outlined or embedded; ≥300 DPI |
| Color and ink | CMYK with separate spot layers for cut/crease/slot rules | 100% K for fine text; rich black C40–60 M30–40 Y30–40 K100; TAC ≤280%–300% |
Production Steps
- Measure the laminated board stack: Confirm the actual caliper of the chosen greyboard core combined with the printed facing sheets, mounting adhesive, and film finish before locking the cutting die CAD.
- Engineer the die-line and spot layers: Place cut lines, half-lap notch cutouts, and crease/score rules on separate spot color layers. Maintain a 3–4 mm (0.118–0.157 in) die gap between parts on the punchboard sheet, and include small nicks (bridges) so pieces remain held in the frame until punch-out.
- Prepare and print facing sheets: Export print-ready PDF/X-1a or PDF/X-4 files at ≥300 DPI with 3 mm (0.118 in) bleed per side and ≥3 mm (0.118 in) safety around every edge and internal notch. Apply surface lamination (such as anti-scuff matte on dark artwork) and mount the sheets to the greyboard core.
- Die-cut and crease: Run the mounted boards through the steel-rule die to cut outer profiles, punch out half-lap slots, and impress crease lines along any folded tabs or angled joints.
Sign-Off Criteria
- Dry-fit assembly on laminated stock: Test-assemble a physical prototype cut from the exact laminated board combination. Half-lap notches must slide together by hand with firm friction and no forced bending.
- Crease and fold integrity: Folded tabs must bend cleanly along scored lines without cracking the printed paper fibers or lifting the film lamination.
- Alignment and clearance: Verify that all artwork stays ≥3 mm (0.118 in) clear of slot cutouts and outer cut lines, and that the 3–4 mm (0.118–0.157 in) die gap holds cleanly across the sheet.
- Compliance documentation (when applicable): Where the finished 3D assembly falls under toy safety or national packaging rules, maintain EN 71 assessment and testing records per the EU Toy Safety framework, alongside applicable packaging registration or sorting marks such as VerpackG and Triman.
Failure Modes
- Crushed slot edges and delamination: Cutting slots to the nominal greyboard thickness (such as 2 mm / 0.079 in) without accounting for facing paper, glue, and 0.03–0.05 mm (0.001–0.002 in) of film makes the joint too tight, causing the facing liner to peel or mushroom when forced together.
- Wobbly or collapsing joints: Oversized slot tolerances or compressed board edges from repeated disassembly leave half-lap intersections loose under load.
- Cracking along folded tabs: Shallow, missing, or misaligned crease rules—or heavy ink coverage exceeding TAC 280%–300% across a fold—fracture the printed liner along the bend.
- Torn edges during punch-out: Spacing parts closer than the 3–4 mm (0.118–0.157 in) die gap or placing oversized nicks near delicate slot corners tears the surface paper when parts are removed from the sheet.
- Clipped graphics inside notches: Placing text or key visual elements within the 3 mm (0.118 in) safety zone around internal slots results in cropped artwork once the notches are punched out.
Guides in this section
Parent guide Punchboard Component Structures