Specifications and Tolerances
Card Deck Press produces custom die-cut tokens and chits with specialist offset and tabletop manufacturing partners. Boxed game components and custom steel-rule tooling follow project and component minimums.
| Parameter | Specification | Notes |
|---|---|---|
| Greyboard Core | 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in) | Thicker cores increase rigidity for small chits and require cleaner rule joints |
| Face & Back Liners | Matched gsm on both sides; 15–20 mm (0.591–0.787 in) wrap margin for wrapped edges | Specify paper weight in gsm; distinguish US Text LB (25 × 38 in / 635 × 965 mm basis sheet) from US Cover LB (20 × 26 in / 508 × 660 mm basis sheet) |
| Punchboard Die Gap | 3–4 mm (0.118–0.157 in) | Minimum spacing between adjacent die-cut tokens to prevent bridge collapse |
| Bleed | 3 mm (0.118 in) per side | Extends artwork past the cut line into the 3–4 mm (0.118–0.157 in) die gutter |
| Safety Margin | ≥3 mm (0.118 in) standard; ≥4–5 mm (0.157–0.197 in) for bordered backs | Protects text, icons, and borders from mounting shift |
| File & Color Setup | AI, PDF, or PSD; PDF/X-1a or PDF/X-4; ≥300 DPI; CMYK + separate spot layers | Outlined or embedded fonts; 100% K for fine text; rich black C40–60 M30–40 Y30–40 K100; TAC ≤280%–300% |
| Surface Finish | Anti-scuff matte recommended for dark artwork | Applied symmetrically to front and back liners to maintain sheet balance |
Production Steps
- Prepress and Die-Line Nesting Prepare artwork in AI, PDF, or PSD and export to PDF/X-1a or PDF/X-4 at ≥300 DPI. Place die lines on a separate spot layer, maintain a 3–4 mm (0.118–0.157 in) die gap between parts, and extend 3 mm (0.118 in) bleed around every token perimeter.
- Offset Printing and Symmetric Coating Print the front and back liner sheets in CMYK, keeping total area coverage at ≤280%–300% and fine text at 100% K. Apply the same protective finish—such as anti-scuff matte for dark solids—to both sheets before mounting so moisture and tension remain balanced.
- Face-and-Back Mounting Mount the printed face and back sheets onto the selected greyboard core (1.5–3 mm / 0.059–0.118 in) with matched grain direction and uniform adhesive coverage, then stack under flat weight to cure without warping.
- Steel-Rule Die Fabrication and Nicking Construct the steel-rule die with tight mitered or butted joints so corners sever cleanly. File small perimeter nicks along straight or low-stress edges of each token to hold parts in the sheet during stripping and transit.
- Die-Cutting and Waste Stripping Die-cut the mounted boards against a flat counterplate so the steel rule penetrates completely through the back liner without crushing the core. Strip outer skeleton waste while leaving nicked tokens seated in the sheet.
Sign-Off Criteria
- Clean Punch-Out: Tokens separate from the sheet under light thumb pressure without delaminating or tearing the printed paper liner at nick points.
- Uniform Edge Profile: Greyboard edges cut square without flared fibers, stepped ridges, or crushed bevels at rule joints.
- Sheet Flatness: Mounted sheets lie flat without cupping or bowing prior to boxing.
- Front-to-Back Registration: Die cuts fall within the ≥3 mm (0.118 in) safety margin on standard artwork and ≥4–5 mm (0.157–0.197 in) on bordered backs, with zero unprinted gutter showing on the token face.
Regulatory Assessment Records
When die-cut tokens and chits are included in products intended for children or marketed in jurisdictions subject to toy safety rules, EN 71 assessment and testing (including small-parts evaluation and chemical/mechanical requirements) apply conditionally based on product age grading and market scope. Maintain supporting lab test reports and technical documentation in accordance with the European Commission Toy Safety framework.
Concrete Failure Modes
- Edge Tearing During Punch-Out: Oversized nicks, too many nicks per token, or nicks placed on sharp corners pull the printed liner away from the greyboard when punched. Correction: Reduce nick width and relocate nicks to straight perimeter segments.
- Sheet Warping (Cupping or Bowing): Mismatched paper gsm between face and back liners, or coating applied to one side only, creates uneven drying tension across the greyboard. Correction: Match front and back liner weights and apply identical finishes to both sides.
- Crushed Edges or Collapsed Bridges: Nesting tokens closer than the 3–4 mm (0.118–0.157 in) die gap or running dull steel rules compresses the greyboard rather than slicing it cleanly. Correction: Enforce the 3–4 mm (0.118–0.157 in) gutter and sharpen or replace worn rule segments.
- Off-Center Artwork or Exposed Bleed: Mounting registration drift exceeds tight safety margins, clipping borders or shifting icons toward the cut edge. Correction: Keep all critical elements inside the ≥3 mm (0.118 in) safety zone and expand bordered backs to ≥4–5 mm (0.157–0.197 in).