Use 3 mm (0.118 in) as the floor on lighter 1.5 mm (0.059 in) or 2 mm (0.079 in) greyboard with simple straight or gently curved tokens. Step up to 4 mm (0.157 in) when cutting thicker 2.5 mm (0.098 in) or 3 mm (0.118 in) greyboard, nesting small or intricate shapes, or running long parallel cut lines where platen pressure concentrates along a narrow strip. For broader dimensional allowances across mounted sheets, see the punchboard tolerances overview.
Specifications and Spacing Parameters
| Parameter | Specification | Notes |
|---|---|---|
| Minimum die-to-die gap | 3–4 mm (0.118–0.157 in) | Keeps steel-rule base rigid and prevents crushed waste bridges |
| Supported greyboard cores | 1.5 / 2 / 2.5 / 3 mm (0.059 / 0.079 / 0.098 / 0.118 in) | Thicker cores require the 4 mm (0.157 in) end of the gap range |
| Bleed per cut edge | 3 mm (0.118 in) | Extends artwork into the waste bridge or outer margin |
| Interior safety margin | ≥3 mm (0.118 in) | ≥4–5 mm (0.157–0.197 in) for tokens with printed borders |
| Wrap margin (wrapped boards) | 15–20 mm (0.591–0.787 in) | Applied where outer board edges wrap rather than flush-trim |
| Corner radius (rounded parts) | R3–R3.5 mm (0.118–0.138 in) | Reduces corner nicking and rule stress on rounded shapes |
| Prepress artwork & die file | AI / PDF / PSD (PDF/X-1a or PDF/X-4) | CMYK ≥300 DPI, TAC ≤280%–300%, separate spot layer for die lines |
A 3–4 mm (0.118–0.157 in) waste bridge between tokens also accommodates standard 3 mm (0.118 in) bleed per side without adjacent token artwork colliding in the live area. Keep fine text in 100% K and use rich black (C40–60 M30–40 Y30–40 K100) for solid dark fills so minor die-registration variance stays visually clean along cut edges.
Production Steps
- Select core thickness and nest parts with bridge clearance. Match the token layout to the chosen greyboard thickness (1.5 mm, 2 mm, 2.5 mm, or 3 mm; 0.059 in, 0.079 in, 0.098 in, or 0.118 in) and maintain at least 3–4 mm (0.118–0.157 in) between every pair of adjacent cut paths as well as from outer sheet edges.
- Isolate the die layer and build bleed/safety zones. Place all cut paths on a dedicated spot-color layer in AI, PDF, or PSD (exported as PDF/X-1a or PDF/X-4) with outlined or embedded fonts. Extend token artwork 3 mm (0.118 in) past each cut line into the waste bridge, and keep critical elements ≥3 mm (0.118 in) inside the cut (≥4–5 mm / 0.157–0.197 in for bordered tokens).
- Build the steel-rule die base. Partner die-makers rout the die board with solid base material between neighboring steel rules; the 3–4 mm (0.118–0.157 in) gap provides enough supporting wood/base width so rules do not lean or pinch under cutting pressure.
- Mount, die-cut, and verify sheet integrity. After laminating the printed face sheet to the greyboard core, the sheet is struck on the platen press. Waste rails and inter-part bridges remain intact for packing while allowing clean token punch-out.
Sign-Off Criteria
- Every adjacent cut-to-cut distance measures ≥3 mm (0.118 in) on 1.5–2 mm (0.059–0.079 in) board, or ≥4 mm (0.157 in) on 2.5–3 mm (0.098–0.118 in) board and dense layouts.
- Sheet-edge margins keep outer waste rails intact and clear any 15–20 mm (0.591–0.787 in) wrap allowance on wrapped boards.
- All die lines sit on a separate non-printing spot layer over ≥300 DPI CMYK artwork with 3 mm (0.118 in) bleed and ≥3 mm (0.118 in) safety (≥4–5 mm / 0.157–0.197 in for bordered graphics).
Failure Modes
- Crushed waste bridges: Spacing below 3 mm (0.118 in) leaves too little board fiber between steel rules, causing the waste strip to collapse into the cut channel during the press strike.
- Chipped or delaminated token edges: Narrow, weakened bridges tear unevenly when stripped or punched, pulling the printed face paper away from the greyboard core.
- Steel-rule deflection: Insufficient base width between adjacent rules on 2.5–3 mm (0.098–0.118 in) greyboard lets rules flex laterally, producing slanted cuts or wedged tokens.
- Exposed core or uneven borders: Omitting the 3 mm (0.118 in) bleed or using less than 4–5 mm (0.157–0.197 in) border safety leaves unprinted paperboard or visibly off-center frames along the cut edge.
Parent guide Punchboard Die-Cut Tolerances