Set every punchboard token with a 3 mm (0.118 in) bleed per side, a minimum 3 mm (0.118 in) inner safe zone for borderless art, and a 4–5 mm (0.157–0.197 in) safe zone when using bordered backs or tight concentric frames. Borderless, full-bleed designs absorb cumulative mounting and die-strike drift cleanly across the cut line, while thin perimeter borders or small centered icons make minor front-to-back offsets immediately visible. For broader structural and dimensional specs across punchboard components, see punchboard tolerances.

Specifications and Registration Margins

Parameter Specification Physical Role in Registration
Greyboard core thickness 1.5 / 2 / 2.5 / 3 mm (0.059 / 0.079 / 0.098 / 0.118 in) Sets board rigidity and blade travel depth during die strike
Bleed per side 3 mm (0.118 in) Prevents unprinted white slivers when liner mounting or die strike shifts
Inner safe zone (standard) >= 3 mm (>= 0.118 in) Keeps live text and icons clear of die-cut bevels and registration drift
Inner safe zone (bordered backs) >= 4–5 mm (>= 0.157–0.197 in) Protects visual symmetry on framed backs against front-to-back offset
Punchboard die gap (gutter) 3–4 mm (0.118–0.157 in) Separates adjacent cut paths so board bridges do not crush or tear
Outer wrap margin (wrapped sheets) 15–20 mm (0.591–0.787 in) Anchors sheet edges around the board perimeter without pulling face art
Prepress file format PDF/X-1a or PDF/X-4 (AI/PDF/PSD) Locks front, back, and spot die-line layers to a single coordinate grid
Color & resolution CMYK + spot die layer, >= 300 DPI, TAC <= 280%–300% Keeps fine text sharp (100% K) and avoids ink-saturation stretch on liners

Production Steps

  1. Lock front, back, and die-line coordinates in prepress: Build the front face, back face, and die-cut path in the same AI, PDF, or PSD layout at >= 300 DPI, exporting as PDF/X-1a or PDF/X-4 with fonts outlined or embedded. Place the die-cut vector on a dedicated spot layer and extend token artwork 3 mm (0.118 in) past every cut line into the 3–4 mm (0.118–0.157 in) die gap.
  2. Mount the front printed liner to the greyboard: Laminate the front printed sheet onto the 1.5–3 mm (0.059–0.118 in) greyboard core using the sheet's lead-edge and side-guide references. Any sheet skew or stretch during lamination establishes the baseline offset between the front artwork and the physical board edge.
  3. Mount the back printed liner to the reverse face: Laminate the back sheet onto the opposite side of the same greyboard core. Because the back liner is registered independently to the board guides rather than directly to the front ink, front-to-back variance combines the mounting tolerances of both passes.
  4. Register and strike the steel-rule die: Align the mounted board in the die-cutting press against the primary sheet guides and strike through the front liner, greyboard core, and back liner. Deeper cuts through 2.5 mm (0.098 in) or 3 mm (0.118 in) greyboard exert higher lateral force on the steel rules, making the full 3–4 mm (0.118–0.157 in) gutter necessary to keep adjacent tokens cleanly separated.

Sign-Off Criteria

  • Full bleed coverage: Token background colors and textures extend 3 mm (0.118 in) past the die line on both faces with no white paper showing along any cut edge.
  • Safe-zone clearance: All critical typography, numbers, and icons sit at least 3 mm (0.118 in) inside the cut line on borderless tokens, and at least 4–5 mm (0.157–0.197 in) inside the cut line on bordered backs.
  • Front-to-back correspondence: Opposing front and back faces land within the same token footprint without cropping into neighboring token artwork or distorting symmetrical backs.
  • Clean gutter separation: The die severs all three layers cleanly around each token while leaving intact 3–4 mm (0.118–0.157 in) waste gutters and holding nicks.

Concrete Failure Modes

  • Exposed white edges along token perimeters: Insufficient bleed (< 3 mm / 0.118 in) fails to cover normal sheet-mounting or die-strike drift, leaving unprinted liner stock visible on one side of a token. Extend full-bleed background artwork 3 mm (0.118 in) beyond every cut path.
  • Uneven or clipped borders on two-sided tokens: Thin perimeter frames placed closer than 4–5 mm (0.157–0.197 in) to the die line exaggerate minor front-to-back mounting shifts, making one border look noticeably wider than the opposite side. Replace tight frames with full-bleed backgrounds or move borders >= 4–5 mm (>= 0.157–0.197 in) inward.
  • Clipped icons or edge text: Live elements positioned inside the 3 mm (0.118 in) safe zone get nicked by the steel rule or crowd the bevel when die-strike registration shifts. Hold all essential graphics and text >= 3 mm (>= 0.118 in) inside the cut line.
  • Crushed gutters and torn liner bridges: Spacing adjacent tokens closer than 3–4 mm (0.118–0.157 in) leaves too little greyboard between parallel steel rules, causing the waste strip to collapse or tear the printed liner during punching. Maintain a 3–4 mm (0.118–0.157 in) die gap between all neighboring cut paths.