Specifications and Physical Conditions
Edge behavior depends on core thickness, surface finish, and the spacing between adjacent cuts:
| Parameter | Specification | Impact on Edge Bevel and Burr |
|---|---|---|
| Greyboard core thickness | 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), 3 mm (0.118 in) | Thicker cores require deeper rule penetration, increasing compression on the entry bevel and accelerating blade dulling. |
| Punchboard die gap | 3–4 mm (0.118–0.157 in) | Minimum bridge width between adjacent token cuts to prevent core crushing or tearing under dulling blades. |
| Wrap margin (mounted boards) | 15–20 mm (0.591–0.787 in) | Allowance for wrapping printed liners cleanly around sheet edges before die cutting. |
| Artwork bleed and safety | 3 mm (0.118 in) bleed; >= 3 mm (0.118 in) safety | Keeps critical graphics away from the rolled entry bevel and minor shear shift. |
| Surface lamination (when used) | 0.03–0.05 mm (0.001–0.002 in) total for double-sided film | Film-laminated liners (such as anti-scuff matte for dark artwork) resist fiber tearing on entry, though a dull rule will stretch or fray the film edge. |
Die-Strike Direction and Blade Maintenance Steps
- Set face-entry strike orientation. Mount the sheet so the steel rule contacts the primary printed face first. As the beveled blade enters the liner and compresses the greyboard core, the top edge forms a smooth, rounded bevel while the exit rim on the underside remains slightly sharper.
- Match rule bevel and makeready to board caliper. Calibrate cutting pressure against the steel cutting plate so the rule severs the bottom liner cleanly across 1.5–3 mm (0.059–0.118 in) greyboard without bottoming out hard enough to flatten the blade edge.
- Place ejection rubber and holding nicks. Position resilient ejection foam along both sides of the rule to strip the waste matrix cleanly without dragging fibers, and keep holding nicks minimal so punched tokens separate without tearing core layers.
- Inspect and re-knife on schedule. Monitor exit edges throughout the run and replace or re-knife worn steel rules as soon as fiber fuzzing or crushed edges appear, especially on dense 2.5–3 mm (0.098–0.118 in) boards and high-volume runs.
Sign-Off Criteria
- Entry face: Uniformly rolled bevel along the token perimeter with no cracked ink, peeled liner, or stretched lamination film.
- Exit rim: Cleanly severed bottom liner with a slightly sharper rim and no loose greyboard fuzz or hanging fiber burrs.
- Die-gap bridges: All 3–4 mm (0.118–0.157 in) bridges between tokens remain flat, intact, and uncrushed across the full sheet.
- Token release: Tokens push out smoothly with light thumb pressure and leave clean, uniform edges without delaminating the backing sheet.
Concrete Failure Modes
- Dull or nicked steel rule: Instead of shearing the board, a worn blade crushes the greyboard core and tears fibers at the exit rim, producing visible paperboard fuzz and ragged token edges.
- Reversed strike direction (back-entry): Striking from the underside places the rounded bevel on the back and leaves the sharper, higher-burr exit rim on the primary printed face, exposing raw core fibers around dark or full-bleed artwork.
- Excessive cutting pressure: Over-impressing the die to compensate for a dull blade flattens the steel-rule tip prematurely, widens the entry crush zone, and scores the cutting plate.
- Worn ejection rubber or undersized die gaps: Weak stripping pressure or gaps narrower than 3–4 mm (0.118–0.157 in) cause sheets to drag on the blade during retraction, fraying liner edges and snapping bridges between tokens.
Parent guide Punchboard Die-Cut Tolerances