Two conditions change this default build immediately:

  • Adding a tear-off score pad: A 13–15 mm (0.51–0.59 in) tuck box fits only the 36-card deck. Including a pad requires either increasing the tuck depth to match the combined stack height plus clearance, moving to a two-piece rigid box, or packing the pad outside the card tuck inside an outer sleeve.
  • Replacing varnish with double-sided film lamination: Double-sided film adds 0.03–0.05 mm (0.0012–0.0020 in) per card, pushing a 36-card stack upward by 1.08–1.80 mm (0.04–0.07 in) and requiring the upper end of the 15 mm (0.59 in) tuck depth or a custom dieline adjustment.

Bill of Materials and Core Specifications

Standard offset card runs with specialist manufacturing partners start at 200 decks (common production tiers: 200, 300, 500, and 1,000+ decks). Boxed configurations with rigid cartons or custom pad tooling follow project and component minimums.

When specifying paper weights, distinguish US Cover LB (measured on a 20 x 26 in basis sheet, used for cards and tuck boxes) from US Text LB (measured on a 25 x 38 in basis sheet, used for tear-off score-pad sheets and inserts).

Component Default Specification Dimensions / Caliper Material & Basis Weight
Card Deck 36 cards, rounded corners 57 x 89 mm (2.24 x 3.50 in); R3–R3.5 mm (0.12–0.14 in) corners 310 gsm black-core linen (approx. 115 lb Cover, 20 x 26 in basis), 0.30–0.32 mm (0.0118–0.0126 in) per card; or 330 gsm black core (approx. 122 lb Cover), 0.32–0.34 mm (0.0126–0.0134 in) per card
Card Coating Card varnish (gloss or matte) Negligible thickness addition Aqueous or UV card varnish; anti-scuff matte varnish or matte film for dark-ground backs
Bare Deck Weight 36-card stack mass — 0.057–0.060 kg (0.125–0.133 lb) bare deck (36 x 0.057 m x 0.089 m x 310–330 gsm)
Tuck Box (Bare Deck) Single-deck folding carton Internal: 58.5–59.5 x 90.5–91.5 x 13–15 mm (2.30–2.34 x 3.56–3.60 x 0.51–0.59 in) 300 gsm art/blue-core board (approx. 111 lb Cover, 0.28–0.31 mm / 0.011–0.012 in) or 350 gsm art stock (approx. 129 lb Cover, 0.34–0.38 mm / 0.013–0.015 in)
Tear-Off Score Pad Optional pad (separate allowance) Sized to fit outer box or 57 x 89 mm (2.24 x 3.50 in) footprint 80–120 gsm uncoated paper (approx. 54–81 lb Text, 25 x 38 in basis), 0.08–0.13 mm (0.003–0.005 in) per sheet, padded with chipboard backer
Rigid Box (Optional Set) Two-piece box for deck + score pad Custom cavity with 1.5–2.5 mm (0.06–0.10 in) X/Y clearance and 1.5–3 mm (0.06–0.12 in) Z clearance 1.5, 2, 2.5, or 3 mm (0.06, 0.08, 0.10, or 0.12 in) greyboard wrapped with 15–20 mm (0.59–0.79 in) turn-in margin

Tuck Depth and Clearance Calculation

Calculate internal tuck dimensions directly from the actual card caliper and finish rather than nominal stock names:

  • Bare 36-card stack height: 36 cards x 0.30 mm = 10.80 mm (0.43 in) on 310 gsm stock, up to 36 cards x 0.34 mm = 12.24 mm (0.48 in) on 330 gsm stock.
  • Stack-height clearance: Add 1.5–3.0 mm (0.06–0.12 in) to the bare stack height. This yields 12.30–15.24 mm (0.48–0.60 in), establishing the 13–15 mm (0.51–0.59 in) internal tuck depth for a bare 36-card Jass deck.
  • Width and height clearance: Add 1.5–2.5 mm (0.06–0.10 in) to the 57 x 89 mm (2.24 x 3.50 in) trim, giving 58.5–59.5 mm (2.30–2.34 in) internal width and 90.5–91.5 mm (3.56–3.60 in) internal height.
  • Score-pad depth allowance: A 50-sheet pad on 80–120 gsm paper adds 50 x 0.08 to 0.13 mm = 4.0–6.5 mm (0.16–0.26 in) plus glue-head and backing-board thickness (typically 1.0–1.5 mm / 0.04–0.06 in). Packing both inside one box requires increasing the internal Z-axis depth to 18–23 mm (0.71–0.91 in) or splitting the deck and pad into a rigid two-piece box.

Prepress and Artwork Requirements

  • File formats and color: Supply print-ready AI, PDF (PDF/X-1a or PDF/X-4), or PSD files in CMYK at >= 300 DPI, with separate spot-color layers for any metallic, foil, or spot-UV masks.
  • Bleed and safety margins: Include 3 mm (0.118 in) bleed on all four sides (63 x 95 mm / 2.48 x 3.74 in full-bleed artboard for a 57 x 89 mm trim). Keep critical indices, pips, and typography at least 3 mm (0.118 in) inside the trim line; increase the safety margin to 4–5 mm (0.16–0.20 in) on card backs with printed borders.
  • Fonts and black ink: Outline or embed all fonts. Set fine text and thin rules to 100% K only. Use rich black (C40–60 M30–40 Y30–40 K100) only on large solid fills, and keep Total Area Coverage (TAC) at <= 280%–300%.
  • Edge treatments: Avoid thick film lamination if the specification includes gilded edges; film overhang interferes with foil adhesion along the card edge.

Production Steps and Sign-Off Criteria

  1. Prepress and Dieline Lock
    • Verify the 36-card imposition (typically one 36-card sheet or paired press forms) and confirm the tuck box dieline matches the chosen stock caliper (310 vs. 330 gsm) and coating.
    • Sign-off criterion: Digital proof approval confirming 3 mm (0.118 in) bleed, >= 4–5 mm (0.16–0.20 in) bordered-back safety, 100% K fine text, and TAC <= 280%–300%.
  2. Offset Press Run and Coating
    • Print 36-card faces and backs on black-core linen or smooth board; apply aqueous/card varnish (or anti-scuff matte finish for dark-ink designs). Print the tuck box flat on 300–350 gsm art board and score-pad sheets on 80–120 gsm uncoated stock.
    • Sign-off criterion: Press-sheet color check against CMYK/spot targets and opaque black-core light-block verification (no face-to-back show-through).
  3. Die-Cutting, Cornering, and Pad Assembly
    • Slit and die-cut cards to 57 x 89 mm (2.24 x 3.50 in) with R3–R3.5 mm (0.12–0.14 in) corners. Die-cut, crease, and glue the tuck box; collate and top-glue the tear-off score pad onto its chipboard backer.
    • Sign-off criterion: Caliper check on a 36-card stack (10.80–12.24 mm / 0.43–0.48 in unlaminated), clean corner radius free of burrs, and smooth sheet tear-off without detaching the pad spine.
  4. Collation and Pack-Out
    • Collate all 36 cards in sequence, insert into the 13–15 mm (0.51–0.59 in) tuck box (or pair with the score pad in the designated outer box/sleeve), and shrink-wrap or seal as specified.
    • Sign-off criterion: Tuck flap closes flat without bowing, and the deck slides in and out without binding against the side walls.

Concrete Failure Modes

  • Visible off-center borders on 57 x 89 mm backs: The narrow 57 mm (2.24 in) width amplifies normal press and die-cutting registration tolerance (+/- 0.5–1.0 mm / 0.02–0.04 in). Borders placed closer than 4–5 mm (0.16–0.20 in) from the trim edge make minor registration shifts immediately obvious.
  • Tuck box bowing or split seams: Packing a 330 gsm deck with double-sided film lamination (total stack 13.3–14.0 mm / 0.52–0.55 in) or forcing a tear-off score pad into a 13 mm (0.51 in) tuck box eliminates the 1.5–3 mm (0.06–0.12 in) stack clearance, causing the tuck flap to pop open and the glued side seam to fail.
  • Ink scuffing on dark card backs: Heavy CMYK dark grounds printed with standard gloss varnish instead of anti-scuff matte varnish or matte film show edge whitening and rub marks after the first few shuffles.
  • Blurry fine indices and slow drying: Setting small suit pips or corner text in 4-color rich black instead of 100% K, or exceeding 280%–300% TAC on smooth coated stock, causes registration haloing and ink set-off on the press stack.
  • Delaminated gilded edges: Combining thick double-sided film lamination (0.03–0.05 mm / 0.0012–0.0020 in per card) with edge gilding causes foil flaking along the card perimeter during cutting and shuffling.

Conditional Compliance and Market Documentation

Distribution into European markets triggers specific regulatory assessment and packaging-registration procedures depending on target age grading and destination country:

  • Toy Safety (EN 71): Custom Jass decks marketed or intended for play by children under 14 years of age require conformity assessment and laboratory testing under the EU Toy Safety framework before placing on the market; maintain test reports and technical documentation per the European Commission Toy Safety guidance.
  • German Packaging Act (VerpackG): Shipping packaged decks into Germany requires producer registration and packaging-volume reporting in the LUCID register for all retail and shipping cartons; retain registration records per Stiftung Zentrale Stelle Verpackungsregister (VerpackG).
  • French Sorting Label (Triman): Selling packaged decks to consumers in France requires displaying the Triman logo and sorting instructions on the tuck box or outer packaging in accordance with Ministère de la Transition écologique (Info-Tri).