Conditions that change this default configuration:
- Dark, full-bleed back artwork: Specify anti-scuff matte finish instead of standard gloss or satin varnish to prevent surface rubbing during shuffling.
- High-wear or moisture-exposed handling: Step up to 330 gsm black-core stock or add double-sided protective film (adding 0.03–0.05 mm / 0.0012–0.0020 in per card), and increase the shallow box depth accordingly.
- Gilded card edges: Omit thick lamination, as thick film can conflict with edge-gilding adhesion and cleanly cut bevels.
- Other European or standard card formats: Deck formats outside the 32-card 59 x 91 mm (2.32 x 3.58 in) Skat specification follow their own assigned trim dimensions, card counts, and sheet impositions; see custom playing cards for parent format options.
Bill of Materials & Dimensional Specifications
Basis weights distinguish US Cover LB (20 x 26 in / 508 x 660 mm basis sheet) from US Text LB (25 x 38 in / 635 x 965 mm basis sheet).
| Component | Default Specification | Dimensions & Caliper | Notes |
|---|---|---|---|
| Playing Cards (32 count) | 310 gsm German black-core linen (~115 lb Cover, 20 x 26 in) or 330 gsm black core (~122 lb Cover, 20 x 26 in) | Trim: 59 x 91 mm (2.32 x 3.58 in) Corners: R3–R3.5 mm (0.118–0.138 in) Caliper: 0.30–0.32 mm (0.0118–0.0126 in) for 310 gsm; 0.32–0.34 mm (0.0126–0.0134 in) for 330 gsm |
32-card unboxed weight is approximately 0.053–0.057 kg (0.117–0.126 lb). Double-sided film adds 0.03–0.05 mm (0.0012–0.0020 in) per card. |
| Scoring Sheet / Leaflet | 80–120 gsm uncoated or matte interior stock (~54–81 lb Text, 25 x 38 in) | 4-, 6-, or 8-panel folded leaflet Caliper: 0.08–0.13 mm (0.0031–0.0051 in) per sheet |
Folded flat size must sit within 59 x 91 mm (2.32 x 3.58 in) so it stacks cleanly inside the shallow case. |
| Shallow 32-Card Tuck Box or Clear Rigid Lid Case | 300–350 gsm folding carton (~111–129 lb Cover, 20 x 26 in) or molded clear rigid lid case | Inner width: 60.5–61.5 mm (2.38–2.42 in) Inner height: 92.5–93.5 mm (3.64–3.68 in) Inner depth: 11.1–13.9 mm (0.44–0.55 in) |
Sized specifically for a 32-card stack plus scoring sheet; a standard 54-card box leaves excess slack. |
Stack Height & Shallow Case Clearance
Calculate the required inner case depth in plain text before finalizing the box dieline:
stack height = (32 * single-card caliper) + folded scoring sheet thickness
inner case depth = stack height + 1.5 to 3.0 mm (0.059 to 0.118 in) clearance
- Unlaminated 310 gsm stack (32 cards):
32 * 0.30 to 0.32 mm = 9.60 to 10.24 mm (0.378 to 0.403 in). - Unlaminated 330 gsm stack (32 cards):
32 * 0.32 to 0.34 mm = 10.24 to 10.88 mm (0.403 to 0.428 in). - With double-sided film: Add
0.96 to 1.60 mm (0.038 to 0.063 in)to the 32-card stack height. - Width and height clearance: Add
1.5 to 2.5 mm (0.059 to 0.098 in)to the 59 x 91 mm (2.32 x 3.58 in) card trim for smooth insertion without corner catching. - Packaged deck weight: A complete 32-card deck with scoring sheet and shallow tuck box weighs roughly 0.065–0.080 kg (0.14–0.18 lb).
Prepress & Print Specifications
- File Formats: Supply print-ready AI, PDF, or PSD files exported to PDF/X-1a or PDF/X-4.
- Resolution & Color: Raster artwork at >=300 DPI in CMYK, with any metallic or specialty spot inks placed on separate spot layers.
- Bleed & Safety: Provide 3 mm (0.118 in) bleed per side, yielding a 65 x 97 mm (2.56 x 3.82 in) full-bleed artboard. Keep critical text and suit pips >=3 mm (0.118 in) inside the trim line; increase safety margin to >=4–5 mm (0.157–0.197 in) on bordered card backs.
- Type & Black Builds: Outline or embed all fonts. Set fine text and thin rules to 100% K only. Use rich black (
C40–60 M30–40 Y30–40 K100) for large solid areas, keeping Total Area Coverage (TAC) <=280%–300%.
Production Steps & Sign-Off Criteria
- Prepress & Shallow-Case Dieline Lock: Verify the 32-card sheet imposition, 65 x 97 mm (2.56 x 3.82 in) bleed geometry, and shallow tuck or rigid-lid dieline depth matched to the chosen stock caliper and scoring-sheet fold (4, 6, or 8 panels).
- Offset Sheet Printing & Coating: Print the 32-card sheet on 310 gsm black-core linen or 330 gsm black-core board, apply aqueous or anti-scuff matte coating (or double-sided film where specified), and print the 80–120 gsm scoring sheet separately.
- Die-Cutting & Corner Rounding: Punch cards to 59 x 91 mm (2.32 x 3.58 in) with R3–R3.5 mm (0.118–0.138 in) corners in controlled registration so suit indices and back borders stay centered.
- Collation & Shallow Case Assembly: Collate the 32-card sequence with the folded scoring sheet and pack into the shallow tuck box or clear rigid lid case.
Sign-off criteria before bulk release:
- Measured card trim holds 59 x 91 mm (2.32 x 3.58 in) with clean R3–R3.5 mm (0.118–0.138 in) corners and no visible white core along cut edges.
- 32-card stack plus scoring sheet slides into the shallow case with 1.5–2.5 mm (0.059–0.098 in) lateral clearance and 1.5–3 mm (0.059–0.118 in) depth clearance—no bowing or lid gap.
- Fine text prints sharp in 100% K, solid dark areas stay <=280%–300% TAC with no ink set-off, and bordered backs show even margins.
European Market & Packaging Compliance
Because Skat decks frequently ship into Germany and neighboring EU markets, verify applicable product and packaging obligations before distribution:
- Toy Safety Assessment (EN 71): If the deck is marketed or intended for play by children under 14, conduct conformity assessment and applicable EN 71 testing and maintain technical documentation per the European Commission Toy Safety framework.
- German Packaging Act (VerpackG): If retail-packaged decks are placed on the German market, register with the LUCID Packaging Register and report packaging volumes under Stiftung Zentrale Stelle Verpackungsregister (ZSVR).
- French Sorting Info (Triman): If distributed to consumers in France, apply the required Triman logo and sorting instructions on the packaging per the French Ministry of Ecological Transition Info-Tri guidance.
Failure Modes & Physical Fixes
| Failure Mode | Root Cause | Physical Fix |
|---|---|---|
| Rattling cards or crushed tuck box | Packing 32 cards into a standard 54-card tuck dieline leaves ~7–8 mm (0.28–0.31 in) of empty depth. | Tool a dedicated shallow 32-card tuck box or rigid case sized to 11.1–13.9 mm (0.44–0.55 in) inner depth. |
| Off-center back borders | Placing bordered artwork closer than 4 mm (0.157 in) to the 59 x 91 mm trim amplifies minor die-cut drift. | Keep bordered back designs >=4–5 mm (0.157–0.197 in) from trim, or switch to full-bleed borderless backs. |
| Scuffed dark card backs | Heavy ink coverage (>280% TAC) with standard gloss or uncoated varnish marks during shuffling. | Cap TAC at <=280%–300%, use rich black (C40–60 M30–40 Y30–40 K100), and apply anti-scuff matte coating. |
| Gilded edge peeling or cracking | Applying thick double-sided film before edge gilding prevents clean foil bonding on the card edges. | Omit thick lamination on gilded Skat runs and use a thin aqueous or satin seal instead. |
| Rigid lid fails to seat flush | Omitting the folded scoring-sheet thickness or 0.03–0.05 mm/card film allowance from the case depth. | Add both the folded 80–120 gsm scoring-sheet thickness and film caliper to the stack calculation before cutting tooling. |
Parent guide Custom Playing Card Printing